Polymer compositions and pressure-resistant pipes made therefrom
AssigneeBorealis AG
InventorsMats Bäckman, Carl-Gustaf Ek, Anneli Pakkanen, Magnus Palmlöf
Life of this patent
Estimating the term…
Loading patent…
AssigneeBorealis AG
InventorsMats Bäckman, Carl-Gustaf Ek, Anneli Pakkanen, Magnus Palmlöf
Estimating the term…
The present invention deals with polymer compositions suitable for making pipes. The compositions comprise a multimodal copolymer of ethylene and one or more alpha-olefins having from 4 to 10 carbon atoms wherein the multimodal ethylene copolymer has a density of from 924 to 935 kg/m3, a melt index MFR5 of from 0.5 to 6.0 g/10 min, a melt index MFR2 of from 0.1 to 2.0 g/10 min and a shear thinning index SHI2.7/210 of from 2 to 50. In addition the multimodal copolymer comprises: (A) from 30 to 70% by weight, based on the combined amount of components (A) and (B), of a low molecular weight ethylene polymer selected from ethylene homopolymer and a copolymer of ethylene and one or more alpha-olefins having from 4 to 10 carbon atoms and having a weight average molecular weight of from 5000 to 100000 g/mol and a density of from 945 to 975 kg/m3; and (B) from 30 to 70% by weight, based on the combined amount of components (A) and (B), of a high molecular weight copolymer of ethylene and one or more alpha-olefins having from 4 to 10 carbon atoms and having a weight average molecular weight of from 100000 to 1000000 g/mol and a density of from 890 to 929 kg/m3.
A polymer composition comprising a multimodal copolymer of ethylene and one or more alpha-olefins having from 4 to 10 carbon atoms wherein the multimodal ethylene copolymer has a density of from 927 to 933 kg/m3, a melt index MFR5 of from 0.5 to 6.0 g/10 min, a melt index MFR2 of from 0.1 to 2.0 g/10 min and a shear thinning index SHI2.7/210 of from 2 to 20.
Dependencies are inferred from the claim text.