Elastomeric paint with protective coating upon styrenic block copolymer articles
AssigneeApex Materials Corporation
InventorYuh-Jye Uang
Life of this patent
Estimating the term…
Abstract
A process for forming a protective sealant and coating onto a thermoplastic elastic substrate forming an article, including applying a paint coating composition to the surface of the elastomeric formed article, to provide a permanent printed coating thereon, and the step of applying a top coat treatment onto the paint coating composition as previously applied onto the thermoplastic elastomeric substrate forming the article.
Claims6
A process for forming an elastomeric paint and/or elastomeric protective coating upon a thermoplastic elastomeric substrate forming an article and having a surface structure receptive to receiving at least one selective elastomeric paint coating, said process including:
- said thermoplastic elastic substrate substantially comprising a styrenic block copolymer;
- permanently applying a paint coating composition to the surface structure of a thermoplastic elastomeric substrate article, said elastomeric paint coating composition comprising:
- (a) one or more copolymer resins selected from the group consisting of a tailback, radical block and multiblock copolymer, and optionally a diblock copolymer;
- (b) mineral oil;
- (c) solvents;
- (d) colorants;
- and,
- (e) additives;
- wherein each of said copolymers contains at least two thermodynamically incompatible segments, selected from the group consisting of:
- (a) styrene-butadiene-styrene polymers;
- (b) styrene-isoprene-styrene polymers;
- (c) styrene-ethylene-butadiene-styrene polymers;
- (d) styrene-ethylene-propylene-styrene polymers;
- (e) styrene-ethylene-butylene-styrene polymers;
- (f) styrene-butadiene polymers;
- and,
- (g) styrene-isoprene polymers;
- wherein said copolymers comprise between about 5% to 10% by weight of the elastomeric paint coating composition;
- wherein said mineral oil comprises between from about 5% to 15% by weight of said elastomeric paint coating composition;
- wherein said solvents comprise aromatic and aliphatic solvents, said aromatic solvents including toluene, xylene, aromatic 150 and aromatic 100, and said aliphatic solvents including heptane, cyclohexane, mineral spirits and VM & P, said solvents comprising between about 80% to about 90% by weight of the elastomeric paint coating composition;
- wherein said elastomeric paint coating composition includes pigments comprising at least one of luminescent pigment, fluorescent pigment, and thermochromic pigment, and said comprised between about 3% to 8% by weight of the elastomeric paint coating composition;
- wherein said at least one additive selected from the group consisting of adhesion modifier, matting powder, antistatic agent, defomer, wetting agent, antioxidant, anti-ultraviolet agent, and a fragrance, and said additives being added to adjust the coating composition for flow, viscosity, and surface characteristics;
- and
- applying said elastomeric protective coating onto the top coat treatment of the thermoplastic elastomeric article, wherein said elastomeric protective coating comprises:
- (a) one or more copolymer resins selected from the group consisting of a tailback, radical block and multiblock copolymer, and optionally diblock copolymer;
- (b) an alpha cyanoacrylate;
- (c) mineral oil;
- (d) solvents;
- and,
- (e) additives;
- and
- wherein said elastomeric paint and elastomeric protective coating furnishing protection to the imprinted article to provide scratch resistance and allow stretching of the article during its usage.