# US 8,541,064 B2 · Methods and systems for producing thermoplastic coated optical fibers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,541,064 B2
- Document ID: US8541064B2
- Status: Granted
- Kind: B2
- Application number: 12/469,316
- Filed: 2009-05-20
- Published: 2009-12-03
- Granted: 2013-09-24
- Earliest claimed: 2008-05-29
- Assignees: Corning Incorporated
- Applicants: James Henry Faler; Bruce Warren Reding; Bradley Kent Shepard; David Andrew Tucker
- Inventors: James Henry Faler; Bruce Warren Reding; Bradley Kent Shepard; David Andrew Tucker
- Web page: https://patentgrep.com/patent/US8541064B2

## CPC

- C03C 25/106: Single coatings
- C03B 37/032: {for glass optical fibres}
- C03C 25/1065: Multiple coatings
- C03C 25/18: Extrusion
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method for producing a coated optical fiber may include drawing an optical fiber from a draw furnace along a first vertical pathway. The optical fiber may then be routed through at least one fluid bearing thereby redirecting the optical fiber along a second vertical pathway. Thereafter, a thermoplastic coating may be applied to the optical fiber with a thermoplastic coating system. The optical fiber may then be wound onto a fiber storage spool with a fiber take-up system. The fiber take-up system may be space apart from the thermoplastic coating system such that the thermoplastic coating may be cooled before the optical fiber is wound onto the fiber storage spool.

## Claims

### Claim 1

A method for producing a coated optical fiber, the method comprising:
drawing an optical fiber from a draw furnace along a first vertical pathway;
routing the optical fiber through at least one first fluid bearing wherein the at least one first fluid bearing redirects the optical fiber along a second vertical pathway, the fluid bearing having a tapered channel therein defined by at least two sidewalls, the fiber being retained between said two sidewalls during said routing step;
applying a thermoplastic coating to the optical fiber with a thermoplastic coating system; and
winding the optical fiber onto a fiber storage spool with a fiber take-up system wherein the fiber take up system is spaced apart from the thermoplastic coating system such that the thermoplastic coating may be cooled before the optical fiber is wound onto the fiber storage spool.

### Claim 2 (depends on 1)

The method of claim 1 wherein the thermoplastic coating is a secondary coating and the method further comprises applying a primary coating to the optical fiber before the secondary coating is applied to the optical fiber.

### Claim 3 (depends on 1)

The method of claim 1 wherein the thermoplastic coating comprises polyethylene, polypropylene, fluorinated ethylene polypropylene, nylon or polyvinyl chloride.

### Claim 4 (depends on 1)

The method of claim 1 wherein the thermoplastic coating is cooled to a temperature from about 30° C. to about 100° C. before it is wound onto the fiber storage spool with the fiber take-up system.

### Claim 5 (depends on 4)

The method of claim 4 wherein the thermoplastic coating is air-cooled.

### Claim 6 (depends on 2)

The method of claim 2 wherein the primary coating comprises a UV-curable coating and the UV-curable coating is cured before the secondary coating is applied to the optical fiber.

### Claim 7 (depends on 6)

The method of claim 6 wherein the UV-curable coating comprises a UV-curable acrylate coating.

### Claim 8 (depends on 6)

The method of claim 6 wherein the UV-curable coating is cured by passing the optical fiber coated with the UV-curable coating through a UV irradiator.

### Claim 9 (depends on 1)

The method of claim 1 wherein the first vertical pathway and the second vertical pathway are collinear.

### Claim 10 (depends on 6)

The method of claim 6 wherein:
the method further comprises routing the optical fiber through a second fluid bearing prior to applying the primary coating to the optical fiber thereby redirecting the optical fiber along a third vertical pathway.

### Claim 11 (depends on 10)

The method of claim 10 wherein the first vertical pathway, the second vertical pathway, and the third vertical pathway are parallel.

### Claim 12 (depends on 1)

The method of claim 1 wherein the thermoplastic coating is a secondary thermoplastic coating and the method further comprises:
applying a primary thermoplastic coating to the optical fiber with a primary thermoplastic coating system before the secondary thermoplastic coating is applied to the optical fiber;
routing the optical fiber through a pulley after the primary thermoplastic coating is applied and before the secondary thermoplastic coating is applied thereby redirecting the optical fiber along a third vertical pathway, wherein the pulley is spaced from the primary thermoplastic coating system such that the primary thermoplastic coating may be cooled before the optical fiber is routed into the pulley.

### Claim 13 (depends on 12)

The method of claim 12 wherein the primary thermoplastic coating comprises polyethylene, polypropylene, fluorinated ethylene polypropylene, nylon, or polyvinyl chloride.

### Claim 14 (depends on 12)

The method of claim 12 wherein the primary thermoplastic coating applied to the optical fiber is cooled to a temperature from about 30° C. to about 100° C. before the optical fiber is routed through the pulley.

### Claim 15 (depends on 14)

The method of claim 14 wherein the primary thermoplastic coating applied to the optical fiber is air cooled.

### Claim 16 (depends on 12)

The method of claim 12 wherein the first vertical pathway, the second vertical pathway, and the third vertical pathway are parallel.