# US 8,524,396 B2 · Method of manufacturing active material, active material, electrode using the same, and lithium-ion secondary battery equipped therewith

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,524,396 B2
- Document ID: US8524396B2
- Status: Granted
- Kind: B2
- Application number: 12/723,256
- Filed: 2010-03-12
- Published: 2010-09-16
- Granted: 2013-09-03
- Earliest claimed: 2009-03-16
- Assignees: TDK Corporation
- Applicants: Atsushi Sano
- Inventors: Atsushi Sano
- Web page: https://patentgrep.com/patent/US8524396B2

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/625: {Carbon or graphite}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of manufacturing an active material having a sufficient discharge capacity at a high discharge current density, an active material obtained thereby, an electrode using the same, and a lithium-ion secondary battery equipped therewith are provided. The method of manufacturing an active material comprises a step of polymerizing a mixture containing an Fe ion, an Li ion, a PO4 ion, a hydroxy acid, and a polyol, the mixture containing the polyol by a molar ratio 1.3 to 16 times that of the hydroxy acid, so as to yield a polymer; and a step of heating the polymer, so as to yield an active material containing an active material particle and carbon. The active material particle is mainly composed of LiFePO4.

## Claims

### Claim 1

A method of manufacturing an active material, the method comprising:
a step of polymerizing a mixture containing an Fe ion, an Li ion, a PO4 ion, a hydroxy acid, and a polyol, the mixture containing the polyol by a molar ratio 1.3 to 16 times that of the hydroxy acid, so as to yield a polymer; and
a step of heating the polymer, so as to yield an active material containing an active material particle and carbon, the active material particle being mainly composed of LiFePO4.

### Claim 2 (depends on 1)

The method of manufacturing the active material according to claim 1, wherein iron nitrate is a source for the Fe ion, lithium chloride is a source for the Li ion, and ammonium hydrogen phosphate is a source for the PO4 ion.

### Claim 3

An active material comprising:
an active material particle group constructed by aggregating active material particles, mainly composed of LiFePO4, having an orientation to a (020) plane and a crystallite size of 30 to 99 nm; and
carbon particles supported on a surface of the active material particle.

### Claim 4 (depends on 3)

An electrode comprising a current collector and an active material layer, disposed on the current collector, containing the active material according to claim 3.

### Claim 5 (depends on 4)

A lithium-ion secondary battery comprising the electrode according to claim 4.