Geopolymer mortar and method
AssigneeLouisiana Tech University Research Foundation; a division of Louisiana Tech University Foundation, Inc.
InventorsErez Allouche, Carlos Montes
Life of this patent
Estimating the term…
Abstract
A geopolymer mortar formed by mixing about 35% to about 45% by weight pozzolanic material, about 35% to about 45% by weight silicon oxide source, about 15% to about 20% by weight alkaline activator solution, and about 0.3% to about 2.5% by weight copper ion source. The pozzolanic material may be fly ash and the silicon oxide source may be sand. The alkaline activator solution may be a sodium hydroxide solution containing sodium silicate. The geopolymer mortar may have a viscosity in the range of about 25,000 to about 50,000 centipoise. The geopolymer mortar may be formed by further mixing one or more additives, such as surfactants, thermal spheres, anti-sagging agents, adhesion primers, or fibers. The geopolymer mortar may be applied as a protective coating on a surface of a structure.
Claims10
A composition of matter formed by the mixing of the components comprising:
- (a) about 35% to about 45% by weight fly ash;
- (b) about 35% to about 45% by weight sand;
- (c) about 15% to about 20% by weight alkaline activator solution;
- (d) about 0.3% to about 2.5% by weight copper ion source;
- and
- (e) about 0% to about 2.2% by weight fibers.
Dependencies are inferred from the claim text.