Back to results
US 8,461,067 B2Granted
Use of pre-coated mat for preparing gypsum board
AssigneeGeorgia-Pacific Gypsum LLC
InventorsRussell Smith, Brian Randall
Life of this patent
Estimating the term…
Abstract
A gypsum board which comprises a set gypsum core sandwiched between and faced with fibrous mats, wherein a free surface of one of said mats is pre-coated with a combination of a mineral pigment, optionally an inorganic adhesive binder and an organic binder, preferably a hydrophobic, UV resistant polymer latex adhesive binder applied to said surface as an aqueous coating composition, said aqueous coating composition upon drying and setting providing a pre-coated mat satisfying certain morphology requirements.
Claims20
A gypsum board comprising:
- a gypsum core;
- a fiber mat comprising a first side and second side opposite the first side, the second side having a bond to the gypsum core such that a tensile strength of the bond is at least 16 pounds per square inch;
- and
- a coating penetrating the fiber mat from the first side into the fiber mat to a depth of about 30 percent to about 50 percent of the thickness of the fiber mat, the coating comprising a mineral pigment and an organic binder,
- wherein the penetration of the coating is relatively uniform over the first side of the fiber mat.
2 more elements
A gypsum board comprising:
- a gypsum core;
- a first fiber mat comprising a first side and second side opposite the first side, the second side having a bond to the gypsum core such that a tensile strength of the bond is at least 16 pounds per square inch;
- a first coating penetrating the first fiber mat from the first side into the fiber mat to a depth of about 30 percent to about 50 percent of the thickness of the first fiber mat;
- a second fiber mat comprising a first side and second side opposite the first side, the second side being bonded to the gypsum core;
- and
- a second coating penetrating the second fiber mat from the first side into the fiber mat to a depth of about 30 percent to about 50 percent of the thickness of the second fiber mat,
- wherein both the first fiber mat and the second fiber mat each comprise glass fibers nominally about 10 to 16 microns in diameter and about one-quarter to about one inch in length, and the first fiber mat in the absence of coating has a basis weight of 1 to 3 pounds per 100 square feet, and
- wherein the penetration of the coating is relatively uniform over the first side of the first fiber mat.
5 more elements
A gypsum board comprising:
- a gypsum core;
- a fiber mat comprising a first side and second side opposite the first side, the second side having a bond to the gypsum core such that a tensile strength of the bond is at least 16 pounds per square inch;
- and
- a coating penetrating the fiber mat from the first side into the fiber mat to a depth of about 30 percent to about 50 percent of the thickness of the fiber mat, the coating comprising a mineral pigment and an organic binder,
- wherein the penetration of the coating remains within the depth of about 30 percent to about 50 percent over at least 50 percent of the first side of the fiber mat.
2 more elements
Dependencies are inferred from the claim text.