# US 8,426,552 B2 · Method for producing acid group-containing polyarylene sulfide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,426,552 B2
- Document ID: US8426552B2
- Status: Granted
- Kind: B2
- Application number: 12/377,704
- Filed: 2007-08-07
- Published: 2010-09-23
- Granted: 2013-04-23
- Earliest claimed: 2006-08-17
- Assignees: DIC Corporation
- Applicants: Toshio Hinokimori; Nobuhiko Yamauchi; Takashi Furusawa
- Inventors: Toshio Hinokimori; Nobuhiko Yamauchi; Takashi Furusawa
- Web page: https://patentgrep.com/patent/US8426552B2

## CPC

- C08G 75/0259: metal hydrogensulfides
- C08G 75/0213: containing elements other than carbon, hydrogen or sulfur
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A method for producing an acid group-containing polyarylene sulfide of the present invention includes a reaction step of reacting a polyhaloaromatic compound (a), an alkali metal hydrosulfide (b), an alkali metal carboxylate (c), and an aromatic compound (d) having an elimination group and an acid group, which function in a nucleophilic reaction, in the presence of a solid alkali metal sulfide.

## Claims

### Claim 1

A method for producing an acid group-containing polyarylene sulfide, comprising a reaction step of reacting a polyhaloaromatic compound (a), an alkali metal hydrosulfide (b), an alkali metal carboxylate (c), and an aromatic compound (d) having an elimination group and an acid group, which function in a nucleophilic reaction, in the presence of a uniformly dispersed fine granular solid alkali metal sulfide, wherein
the alkali metal carboxylate (c) is an alkali metal salt (c2) of a hydrolysate of an aliphatic cyclic compound (c1) that is capable of ring-opening by hydrolysis.

### Claim 2 (depends on 1)

The method for producing an acid group-containing polyarylene sulfide according to claim 1, wherein the reaction step comprises, as essential production steps, steps 1 and 2 shown below:
the step 1 of:
reacting, while dehydrating, a hydrous alkali metal sulfide, or a hydrous alkali metal hydrosulfide and an alkali metal hydroxide,
the aliphatic cyclic compound (c1) that is capable of ring-opening by hydrolysis, and
a non-hydrolyzable organic solvent, to form a slurry (I) that contains the fine granular solid alkali metal sulfide, the alkali metal hydrosulfide (b), and the alkali metal salt (c2) of the hydrolysate of the aliphatic cyclic compound (c1); and subsequently the step 2 of:
reacting, in the slurry (I), the polyhaloaromatic compound (a),
the alkali metal hydrosulfide (b),
the alkali metal salt (c2) of the hydrolysate of the aliphatic cyclic compound (c1), and
the aromatic compound (d) having the elimination group and the acid group, which function in a nucleophilic reaction, to perform polymerization.

### Claim 3 (depends on 2)

The method for producing an acid group-containing polyarylene sulfide according to claim 2, wherein an amount of the aromatic compound (d) having the elimination group and the acid group, which function in the nucleophilic reaction, is within a range from 0.0001 to 0.1 mol per mol of a sulfur atom of the hydrous alkali metal sulfide or hydrous alkali metal hydrosulfide used in the step 1.

### Claim 4 (depends on 2)

The method for producing an acid group-containing polyarylene sulfide according to claim 2, wherein the non-hydrolyzable organic solvent is the polyhaloaromatic compound (a).

### Claim 5 (depends on 2)

The method for producing an acid group-containing polyarylene sulfide according to claim 2, wherein, in the step 1, the aliphatic cyclic compound (c1) that is capable of ring-opening by hydrolysis is used in an amount within a range from 0.01 to 0.9 mol per mol of the hydrous alkali metal sulfide or hydrous alkali metal hydrosulfide.

### Claim 6 (depends on 2)

The method for producing an acid group-containing polyarylene sulfide according to claim 2, wherein the content of the fine granular solid alkali metal sulfide in the slurry (I) obtained in the step 1 is within a range from 0.1 to 0.99 mol based on 1 mol of the hydrous alkali metal sulfide used in the step 1.

### Claim 7 (depends on 6)

The method for producing an acid group-containing polyarylene sulfide according to claim 6, wherein a polymer slurry is substantially in an anhydrous state when a consumption rate of the fine granular solid alkali metal sulfide in the step 2 is 10%.

### Claim 8 (depends on 2)

The method for producing an acid group-containing polyarylene sulfide according to claim 2, wherein, after the completion of the step 1, the aliphatic cyclic compound (c1) that is capable of ring-opening by hydrolysis is further added so that a total amount of the aliphatic cyclic compound (c1) is within range from 0.6 to 10 mol based on 1 mol of a sulfur atom existing in a reaction system.

### Claim 9 (depends on 2)