# US 8,399,597 B2 · Phenolic resin formulation and coatings for abrasive products

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,399,597 B2
- Document ID: US8399597B2
- Status: Granted
- Kind: B2
- Application number: 12/284,349
- Filed: 2008-09-19
- Published: 2009-06-11
- Granted: 2013-03-19
- Earliest claimed: 2007-09-21
- Assignees: Saint-Gobain Abrasives, Inc.; Saint-Gobain Abrasifs
- Applicants: Abdul Habid Pullichola; Adiseshaiah K. Seshu; Kottotil Mohan Das; Jagmohan Verma; Olivier Pons Y Moll; Philippe Espiard
- Inventors: Abdul Habid Pullichola; Adiseshaiah K. Seshu; Kottotil Mohan Das; Jagmohan Verma; Olivier Pons Y Moll; Philippe Espiard
- Web page: https://patentgrep.com/patent/US8399597B2

## CPC

- B24D 3/28: Resins {or natural or synthetic macromolecular compounds (B24D3/22 takes precedence)}
- B24D 11/001: {Manufacture of flexible abrasive materials}
- C08G 8/24: with mixtures of two or more phenols which are not covered by only one of the groups C08G8/10 - C08G8/20
- C08G 8/28: Chemically modified polycondensates
- C09D 161/12: with polyhydric phenols
- C09D 161/14: Modified phenol-aldehyde condensates
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A resorcinol-modified phenolic resin composition is formed by reacting a basic catalyst, formaldehyde, water and a benzene-ol to form an intermediate composition to which resorcinol is subsequently added to reduce the presence of free formaldehyde. Optionally, an alkanolamine can be combined and reacted with the resorcinol-modified phenolic resin composition to form a resorcinol-alkanolamine-modified phenolic resin composition. The resorcinol-modified phenolic resin and the resorcinol-alkanolamine-modified phenolic resin compositions can be employed to coat abrasive products having a relatively low free formaldehyde content.

## Claims

### Claim 1

A modified phenolic resin composition formed by a method comprising the steps of:
a) combining a basic catalyst, formaldehyde, water and a benzene-ol to form a basic reaction mixture undergoing chemical reaction;
b) terminating the chemical reaction of the reaction mixture when water tolerance of the reaction mixture is in a range of between about 300% and about 500% to thereby form an intermediate composition; and
c) adding resorcinol to the intermediate composition in an amount of between 2.5% and 7.5% based on the weight of the benzene-ol combined to form the reaction mixture, whereby the resorcinol undergoes chemical reaction with the intermediate composition to form a composition that includes a resorcinol-modified phenolic resin,
wherein the resorcinol-modified phenolic resin has a free formaldehyde content of between about 0.01 weight % and about 0.3 weight % of 100 g of the resin, and
wherein the tensile strength of the resin composition is at least 12% to 26% greater than the tensile strength of an equivalent resin composition where the only difference is that the equivalent resin composition has not been modified with any resorcinol.

### Claim 2 (depends on 1)

The resin composition of claim 1, wherein the benzene-ol is phenol.

### Claim 3 (depends on 2)

The resin composition of claim 2, wherein viscosity of the resorcinol-modified phenolic resin remains essentially constant for at least about 1 hour.

### Claim 4 (depends on 2)

The resin composition of claim 2, wherein water tolerance of the resorcinol-modified-phenolic resin independently remains essentially constant for at least about 1 hour.

### Claim 5 (depends on 2)

The resin composition of claim 2, wherein the resorcinol-modified phenolic resin has a free formaldehyde content of between about 0.05 weight % and about 0.2 weight % of 100 g of the resin.

### Claim 6 (depends on 1)

The resin composition of claim 1, wherein the method further includes removing at least a portion of the water present in the resorcinol-modified phenolic resin composition.

### Claim 7 (depends on 1)

The resin composition of claim 1, wherein the basic catalyst is selected from the group consisting of sodium hydroxide, lithium hydroxide, barium hydroxide and hydrates thereof, and a combination thereof.

### Claim 8 (depends on 7)

The resin composition of claim 7, wherein the basic catalyst is sodium hydroxide.

### Claim 9 (depends on 8)

The resin composition of claim 8, wherein the amount of the sodium hydroxide is between about 1 weight % and about 5 weight % of the amount of the benzene-ol combined to form the reaction mixture.

### Claim 10 (depends on 9)

The resin composition of claim 9, wherein the amount of the sodium hydroxide is about 2 weight % of the amount of the benzene-ol combined to form the reaction mixture.

### Claim 11 (depends on 1)

The resin composition of claim 1, wherein the resorcinol added to the intermediate composition is in an aqueous medium.

### Claim 12 (depends on 11)

The resin composition of claim 11, wherein the amount of resorcinol added to the intermediate composition is in a range of between about 5 weight % and about 7.5 weight % of the amount of the benzene-ol combined to form the reaction mixture.

### Claim 13 (depends on 12)

The resin composition of claim 12, wherein the amount of resorcinol added to the reaction mixture is about 5 weight % of the amount of the benzene-ol combined to form the reaction mixture.

### Claim 14 (depends on 1)

The resin composition of claim 1, wherein the chemical reaction of the reaction mixture is terminated by adjusting the temperature of the reaction mixture to a temperature equal to or less than about 50° C.

### Claim 15 (depends on 1)

The resin composition of claim 1, wherein the chemical reaction is terminated when the water tolerance of the reaction mixture is in a range of between 300% and about 500%.

### Claim 16 (depends on 1)

The resin composition of claim 1, wherein reaction of the reaction mixture is initiated by exposing the reaction mixture to a temperature in a range of between about 50° C. and about 90° C.

### Claim 17 (depends on 16)

The resin composition of claim 16, wherein the resorcinol is allowed to react with the intermediate composition at a temperature in a range of between about 50° C. and about 70° C.

### Claim 18 (depends on 1)

The resin composition of claim 1, wherein the water content of the intermediate composition is at least about 50 wt % of the total weight of the intermediate composition.

### Claim 19 (depends on 1)

The resin composition of claim 1, wherein the modified phenolic resin composition has a viscosity in a range of between about 2,000 cps and about 20,000 cps at about 25° C.

### Claim 20 (depends on 1)

The resin composition of claim 1, wherein the method further includes adding an alkanolamine to the resorcinol-modified phenolic resin composition in an amount in a range of between about 0.1 weight % and about 15 weight % based on the weight of the benzene-ol combined to form the reaction mixture, whereby the alkanolamine undergoes chemical reaction with the resorcinol-modified phenolic resin composition to form a composition that includes a resorcinol-alkanolamine-modified phenolic resin.

### Claim 21 (depends on 20)

The resin composition of claim 20, wherein the alkanolamine is NH2(C2H5OH) or NH(C2H5OH)2.

### Claim 22 (depends on 20)

The resin composition of claim 20, wherein the amount of the alkanolamine is in a range of between about 0.1 weight % and about 5 weight % based on the weight of the benzene-ol combined to form the reaction mixture.

### Claim 23 (depends on 20)

The resin composition of claim 20, wherein the temperature of the combined alkanolamine and the resorcinol-modified phenolic resin composition is adjusted to a temperature in a range of between about 50° C. and about 70° C.

### Claim 24 (depends on 23)

The resin composition of claim 23, wherein the temperature of the combined alkanolamine and the resorcinol-modified phenolic resin composition is maintained for a reaction period in a range of between about 45 minutes and about 90 minutes.

### Claim 25 (depends on 24)

The resin composition of claim 24, wherein the temperature of the combined alkanolamine and the resorcinol-modified phenolic resin composition is maintained at about 60° C. for a period of time of about 60 minutes.

### Claim 26 (depends on 24)

The resin composition of claim 24, wherein the method further includes removing at least a portion of the water present in the resorcinol-alkanolamine-modified phenolic resin composition.

### Claim 27 (depends on 20)

The resin composition of claim 20, wherein viscosity of the resorcinol-ethanol-amine-modified phenolic resin remains essentially constant for at least about 1 hour.

### Claim 28 (depends on 20)

The resin composition of claim 20, wherein water tolerance of the resorcinol-ethanol-amine-modified phenolic resin independently remains essentially constant for at least about 1 hour.

### Claim 29 (depends on 20)

The resin composition of claim 20, wherein the resorcinol-ethanol-amine-modified phenolic resin has a free formaldehyde content of between about 0.01 weight % and about 0.3 weight % of 100 g of the resin.

### Claim 30 (depends on 29)

The resin composition of claim 29, wherein the resorcinol-ethanol-amine-modified phenolic resin has a free formaldehyde content of between about 0.05 weight % and about 0.2 weight % of 100 g of the resin.

### Claim 31 (depends on 1)

The resin composition of claim 1, wherein the amount of resorcinol added to the reaction mixture is in a range of between about 2.5 weight % and about 5 weight % of the amount of benzene-ol combined to form the reaction mixture.

### Claim 32 (depends on 1)

The resin composition of claim 1, wherein the chemical reaction is terminated when the water tolerance of the reaction mixture is 390%.

### Claim 33 (depends on 1)

The resin composition of claim 1, wherein the resin composition is a component in a coated or bonded abrasive product as a cured resin.

### Claim 34 (depends on 20)

The resin composition of claim 20, wherein the resin composition is a component in a coated or bonded abrasive product as a cured resin.