Insert weld repair
AssigneeUnited Technologies Corporation
InventorPhilip R. Belanger
Life of this patent
Estimating the term…
Abstract
A method of repairing an aperture and adjacent defect wherein one or more defects proximate an aperture are removed from the base material proximate the aperture in an arc shape. An insert containing a profile that corresponds to the arc shaped section of the base material removed is welded to the base material. The weld is accomplished with a single curved path. Next, the insert is removed to create a repaired aperture and a surrounding section that has essentially the same dimensions as the aperture and surrounding section prior to the repair.
Claims14
A method of repairing an aperture and adjacent defect, the method comprising:
- removing one or more defects proximate an aperture that has a diameter less than about 0.30 inches by removing an arc shaped section of base material proximate the aperture;
- providing an insert containing a profile that corresponds to the arc shaped section of the base material removed;
- welding the insert to the base material, wherein the weld is accomplished with a single curved path;
- removing material from the insert to create a repaired aperture and a surrounding section comprising essentially the same dimensions as the aperture and surrounding section prior to the repair.
A method of repairing an aperture and adjacent defect, the method comprising:
- removing one or more defects in a base material adjacent an aperture;
- providing an insert of material containing a profile that corresponds to a profile of the base material removed adjacent the aperture;
- providing a combination top and runoff plate that encompasses the insert of material;
- welding the insert to the base material and combination plate;
- removing material from the insert and combination plate to obtain an aperture and a surrounding section containing a profile with essentially the same profile of the aperture and surrounding section prior to initiating the repair.
The repair of method 7 wherein removing the defects leaves at least a portion of the original aperture in the base material.
The repair of method 7 wherein removing one or more defects comprises removing enough base material to create a weld seam that extends away from an area of high stress concentration proximate the aperture.
Dependencies are inferred from the claim text.