Magnetic alloy, amorphous alloy ribbon, and magnetic part
AssigneeHitachi Metals, Ltd.
InventorsYoshihito Yoshizawa, Motoki Ohta
Life of this patent
Estimating the term…
Loading patent…
AssigneeHitachi Metals, Ltd.
InventorsYoshihito Yoshizawa, Motoki Ohta
Estimating the term…
A soft magnetic alloy that in an FeCo nanocrystal soft magnetic material, exhibits a high saturation magnetic flux density of 1.85 T or more, and that ensures prolonged nozzle life and easy ribbon production; an amorphous alloy ribbon for use in production thereof; and magnetic parts utilizing the soft magnetic alloy. The soft magnetic alloy has the composition of the formula Fe100-x-y-aCoaCuxBy (in the formula, x, y and a each represent atomic % and satisfy the relationships 1<x≦3, 10≦y≦20 and 10<a<25). At least part of the structure thereof consists of a crystal phase of 60 nm or less (not including 0) crystal grain diameter. The soft magnetic alloy has a saturation magnetic flux density of 1.85 T or more and a coercive force of 200 A/m or less.
A magnetic alloy represented by the compositional formula:
Dependencies are inferred from the claim text.