# US 8,280,479 B2 · Flexible 3D microprobe structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,280,479 B2
- Document ID: US8280479B2
- Status: Granted
- Kind: B2
- Application number: 12/637,485
- Filed: 2009-12-14
- Published: 2011-06-16
- Granted: 2012-10-02
- Earliest claimed: 2009-12-14
- Assignees: National Tsing Hua University
- Inventors: Da-Jeng Yao; Chang-Hsiao Chen; Shih-Chang Chuang; Yen-Chung Chang
- Web page: https://patentgrep.com/patent/US8280479B2

## CPC

- A61B 5/685: {Microneedles}
- A61B: DIAGNOSIS; SURGERY; IDENTIFICATION (usefulness limited to only animals A61D)

## Abstract

The present invention discloses a flexible 3D microprobe structure, which comprises at least one probe, a base and a hinge portion. The probe is connected to the base via the hinge portion. The probe forms a bend angle with respect to a normal of the base by attracting the probe through an electrostatic force to make the hinge portion bend with respect to the base, and thus to form a 3D structure having the bend angle. The probe, the base and the hinge portion are made of a flexible polymeric material to reduce the inflammation response of creatures. Further, a fixing element is used to enhance the structural strength of the flexible 3D microprobe structure.

## Claims

### Claim 1

A flexible 3-dimensional microprobe structure comprises at least one probe, a base, a hinge portion, and a fixing element, wherein said probe and said hinge portion are made of a first flexible polymeric material, and wherein said probe is connected to said base via said hinge portion, and wherein said probe forms a bend angle with respect to a normal of said base, and wherein said fixing element is formed by applying glue to said hinge portion.

### Claim 2 (depends on 1)

The flexible 3-dimensional microprobe structure according to claim 1, wherein said first flexible polymeric material is selected from a group consisting of polyimide, parylene (poly-para-xylylen), a thick SU-8 photoresist, polydimethylsiloxane, and benzocyclobutene.

### Claim 3 (depends on 1)

The flexible 3-dimensional microprobe structure according to claim 1, wherein said base is made of a second flexible polymeric material.

### Claim 4 (depends on 3)

The flexible 3-dimensional microprobe structure according to claim 3, wherein said second flexible polymeric material is selected from a group consisting of polyimide, parylene (poly-para-xylylen), a thick SU-8 photoresist, polydimethylsiloxane, and benzocyclobutene.

### Claim 5 (depends on 1)

The flexible 3-dimensional microprobe structure according to claim 1, wherein said probe, said base and said hinge portion are made of an identical material.

### Claim 6 (depends on 1)

The flexible 3-dimensional microprobe structure according to claim 1, wherein said base has a micro channel, and said glue flows through said micro channel to apply to said hinge portion.

### Claim 7 (depends on 1)

The flexible 3-dimensional microprobe structure according to claim 1, wherein said glue is polyethylene.

### Claim 8 (depends on 1)

The flexible 3-dimensional microprobe structure according to claim 1, wherein said probe has a needle point and a connection member located at one side which is far away from said needle point; said connection member connects said needle point and said hinge portion.

### Claim 9 (depends on 8)

The flexible 3-dimensional microprobe structure according to claim 8, wherein said connection member has an auxiliary fixing element which can increase a contact area between said glue and said flexible 3-dimensional microprobe structure.

### Claim 10 (depends on 9)

The flexible 3-dimensional microprobe structure according to claim 9, wherein said auxiliary fixing element is made of a flexible polymeric material selected from a group consisting of polyimide, parylene(poly-para-xylylen), a thick SU-8 photoresist, polydimethylsiloxane), and benzocyclobutene.

### Claim 11 (depends on 1)

The flexible 3-dimensional microprobe structure according to claim 1, wherein said probe has a structure-reinforcing element which is used to strengthen said probe so as to puncture a detected object by said probe.

### Claim 12 (depends on 11)

The flexible 3-dimensional microprobe structure according to claim 11, wherein said structure-reinforcing element is made of a thick SU-8 photoresist.