# US 8,279,576 B2 · Electrostatic chuck

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,279,576 B2
- Document ID: US8279576B2
- Status: Granted
- Kind: B2
- Application number: 12/753,992
- Filed: 2010-04-05
- Published: 2010-10-07
- Granted: 2012-10-02
- Earliest claimed: 2009-04-07
- Assignees: NGK Insulators, Ltd.
- Inventors: Keiichi Nakamura; Shunsuke Tanaka
- Web page: https://patentgrep.com/patent/US8279576B2

## CPC

- H10P 72/722: {Details of electrostatic chucks}
- Y10T 279/23: with magnetic or electrostatic means
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A ceramic electrostatic chuck according to the present invention includes a dielectric layer with a support layer in contact with the back side of the dielectric layer, and an embedded electrostatic electrode. A wafer is placed on the dielectric layer and the dielectric layer is formed of sintered aluminum nitride containing Sm and has a volume resistivity in the range of 4×109 to 4×1010 Ωcm at room temperature. The support layer is formed of sintered aluminum nitride containing Sm and Ce and has a volume resistivity of 1×1013 Ωcm or more at room temperature.

## Claims

### Claim 1

A ceramic electrostatic chuck that includes an embedded electrode, the electrostatic chuck comprising:
a dielectric layer on which a wafer can be placed, the dielectric layer being formed of sintered aluminum nitride containing Sm and having a volume resistivity in the range of 4×109 to 4×1010 Ωcm at room temperature; and
a support layer that is in contact with the back side of the dielectric layer, is formed of sintered aluminum nitride containing Sm and Ce, and has a volume resistivity of 1×1013 Ωcm or more at room temperature,
wherein the dielectric layer is formed of sintered aluminum nitride that contains an Al—Sm—O compound. Sm being contained in an amount 1.2% to 4% by weight in terms of Sm2O3, the Al2O3/Sm2O3 equivalent weight ration of Al in terms of Al2O3 to Sm in terms of Sm2O3 being in the range of 0.8 to 1.5,
wherein the support layer is harmed of sintered aluminum nitride that contains oxides of Sm and Ce, Sm being contained in an amount 0.96% to 2.2% by weight in terms of Sm2O3Ce being contained in an amount 0.2% to 0.5% by weight in terms of CeO2, and
wherein Ce is contained only in the support layer.

### Claim 2 (depends on 1)

The electrostatic chuck according to claim 1, wherein the electrode is formed of molybdenum metal or a molybdenum alloy and is disposed within the dielectric layer, within the support layer, or at an interface between the dielectric layer and the support layer.

### Claim 3 (depends on 1)

The electrostatic chuck according to claim 1, wherein the support layer includes a heating resistor.