# US 8,279,554 B2 · Magnetic recording medium and magnetic signal reproduction method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,279,554 B2
- Document ID: US8279554B2
- Status: Granted
- Kind: B2
- Application number: 13/364,610
- Filed: 2012-02-02
- Published: 2012-05-31
- Granted: 2012-10-02
- Earliest claimed: 2007-05-31
- Assignees: FUJIFILM Corporation
- Inventors: Hitoshi Noguchi; Osamu Shimizu; Yasushi Endo
- Web page: https://patentgrep.com/patent/US8279554B2

## CPC

- G11B 5/70: on a base layer
- G11B 5/00821: {using stationary heads}
- G11B 5/71: characterised by the lubricant
- G11B 5/70678: {Ferrites}
- G11B 5/714: characterised by the dimension of the magnetic particles
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)

## Abstract

The magnetic signal reproduction system comprises a magnetic recording medium comprising a magnetic layer comprising a ferromagnetic powder and a binder on a nonmagnetic support; and a reproduction head, wherein a number of protrusions equal to or greater than 10 nm in height on the magnetic layer surface, as measured by an atomic force microscope, ranges from 50 to 2500/10,000 μm2, a quantity of lubricant on the magnetic layer surface, denoted as a surface lubricant index, ranges from 0.5 to 5.0, a surface abrasive occupancy of the magnetic layer ranges from 2 to 20 percent, and the reproduction head is a magnetoresistive magnetic head comprising a spin-valve layer.

## Claims

### Claim 1

A magnetic recording medium comprising:
a magnetic layer comprising a ferromagnetic powder and a binder on a nonmagnetic support,
wherein
the number of protrusions equal to or greater than 10 nm in height on the magnetic layer surface, as measured by an atomic force microscope, ranges from 50 to 2500/10,000 μm2,
the quantity of lubricant on the magnetic layer surface, denoted as a surface lubricant index, ranges from 0.5 to 5.0, and
the surface abrasive occupancy of the magnetic layer ranges from 2 to 20 percent.

### Claim 2 (depends on 1)

The magnetic recording medium according to claim 1, wherein the ferromagnetic powder is a hexagonal ferrite powder.

### Claim 3 (depends on 2)

The magnetic recording medium according to claim 2, wherein the hexagonal ferrite powder has a mean plate diameter ranging from 10 to 50 nm.

### Claim 4 (depends on 1)

The magnetic recording medium according to claim 1, wherein the magnetic layer has a thickness ranging from 10 to 150 nm.

### Claim 5

A magnetic signal reproduction method for reproducing signals, that have been recorded on a magnetic recording medium, wherein
the magnetic recording medium comprises a magnetic layer comprising a ferromagnetic powder and a binder on a nonmagnetic support,
the number of protrusions equal to or greater than 10 nm in height on the magnetic layer surface, as measured by an atomic force microscope, ranges from 50 to 2500/10,000 μm2,
the quantity of lubricant on the magnetic layer surface, denoted as a surface lubricant index, ranges from 0.5 to 5.0, and
the surface abrasive occupancy of the magnetic layer ranges from 2 to 20 percent.

### Claim 6 (depends on 5)

The magnetic signal reproduction method according to claim 5, wherein the ferromagnetic powder is a hexagonal ferrite powder.

### Claim 7 (depends on 6)

The magnetic signal reproduction method according to claim 6, wherein the hexagonal ferrite powder has a mean plate diameter ranging from 10 to 50 nm.

### Claim 8 (depends on 5)

The magnetic signal reproduction method according to claim 5, wherein the magnetic layer has a thickness ranging from 10 to 150 nm.