# US 8,278,809 B2 · Spark plug with alumina-based insulator

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,809 B2
- Document ID: US8278809B2
- Status: Granted
- Kind: B2
- Application number: 13/257,709
- Filed: 2010-03-09
- Published: 2012-01-12
- Granted: 2012-10-02
- Earliest claimed: 2009-03-26
- Assignees: Ngk Spark Plug Co., Ltd.
- Inventors: Hirokazu Kurono; Toshitaka Honda; Katsuya Takaoka; Hiroki Takeuchi; Kuniharu Tanaka; Takeshi Mitsuoka
- Web page: https://patentgrep.com/patent/US8278809B2

## CPC

- C04B 35/113: based on beta-aluminium oxide
- C04B 35/117: Composites
- H01T 13/38: Selection of materials for insulation
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3213: Strontium oxides or oxide-forming salts thereof
- C04B 2235/3215: Barium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3222: Aluminates other than alumino-silicates, e.g. spinel (MgAl2O4)
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3227: Lanthanum oxide or oxide-forming salts thereof
- C04B 2235/3229: Cerium oxides or oxide-forming salts thereof
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01T: SPARK GAPS; OVERVOLTAGE ARRESTERS USING SPARK GAPS; SPARKING PLUGS; CORONA DEVICES; GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES (overvoltage protection circuits H02H)

## Abstract

A spark plug exhibits a satisfactory withstand voltage characteristic and sufficient mechanical strength in a high temperature environment exceeding 700° C. The spark plug has a center electrode, an insulator, and a ground electrode, characterized in that the insulator is formed of an alumina-based sintered material containing an Si component, a Group 2 element (2A) component, and a rare earth element (RE) component; that the alumina-based sintered material has an RE-β-alumina crystal phase; and that the mean crystal grain size DA(RE) of the RE-β-alumina crystal phase and that of alumina DA(Al) satisfy the following relationship (1): 0.2≦DA(RE)/DA(Al)≦3.0.

## Claims

### Claim 1

A spark plug comprising:
a center electrode;
a generally cylindrical insulator surrounding the center electrode; and
a ground electrode disposed such that one end of the ground electrode faces the center electrode via a spark discharge gap,
characterized in that the insulator is formed of an alumina-based sintered material containing an Si component, a Group 2 element component, said Group included in the periodic table defined by Recommendations 1990 presented by the International Union of Pure and Applied Chemistry, or IUPAC (Group 2 may be referred to as Group 2A as previously defined by IUPAC, or as defined by the Chemical Abstracts Service (CAS)), and a rare earth element (RE) component;
that the alumina-based sintered material has an RE-β-alumina crystal phase containing at least the RE component, and
that the mean crystal grain size DA(RE) of the RE-β-alumina crystal phase and that of alumina DA(Al) satisfy the following relationship (1):
0.2≦DA(RE)DA(Al)≦3.0.

### Claim 2 (depends on 1)

A spark plug according to claim 1, wherein
the alumina-based sintered material includes three or fewer RE-β-alumina crystal phase portions where the crystal grain size DE(RE) thereof and
the mean crystal grain size DA(Al) of alumina satisfy the following relationship (2):
DE(RE)/DA(Al)>2.

### Claim 3 (depends on 1)

A spark plug according to claim 1, wherein the RE-β-alumina crystal phase is represented by the following compositional formula: RE(2A)x(Al)yOz(wherein x is 0 to 2.5, y is 11 to 16, and z is 18 to 28).

### Claim 4 (depends on 1)

A spark plug according to claim 1, wherein, when the RE-β-alumina crystal phase is observed under a transmission electron microscope, a circular spot having a diameter of 0.3 nm in which the RE-β-alumina crystal phase is present contains an alkali metal component in an oxide converted amount of 0.01 to 8mass %.

### Claim 5 (depends on 1)

A spark plug according to claim 1, wherein
the alumina-based sintered material is produced by mixing an alumina material and a secondary material formed of the Si component, an Mg component, the Group 2A component, and the RE component in a slurry, molding the granulated product, and firing a compact; and
the particle size ratio of the mean particle size of the alumina material contained in the slurry to that of the secondary material (Dalumina material/Dsecondary material) satisfies the following relationship:
1.3≦(Dalumina material/Dsecondary material)≦4.

### Claim 6 (depends on 1)

A spark plug according to claim 1, wherein
the Group 2A component contains Mg and Ba as essential elements and at least one element other than Mg and Ba among elements in Group 2A, and
the RE component is at least one member selected from the group consisting of an La component, a Pr component, and an Nd component.

### Claim 7 (depends on 1)

A spark plug according to claim 1,
wherein the insulator is held by a metallic shell, and
a screw portion formed around the outer surface of said metallic shell has a nominal diameter of 10 mm or smaller.

### Claim 8 (depends on 2)

A spark plug according to claim 2, wherein the RE-β-alumina crystal phase is represented by the following compositional formula: RE(2A)x(Al)yOz, (wherein x is 0 to 2.5, y is 11 to 16, and z is 18 to 28).

### Claim 9 (depends on 2)

A spark plug according to claim 2, wherein, when the RE-β-alumina crystal phase is observed under a transmission electron microscope, a circular spot having a diameter of 0.3 nm in which the RE-β-alumina crystal phase is present contains an alkali metal component in an oxide-converted amount of 0.01 to 8 mass %,

### Claim 10 (depends on 3)

A spark plug according to claim 3, wherein, when the RE-β-alumina crystal phase is observed under a transmission electron microscope, a circular spot having a diameter of 0.3 nm in which the RE-β-alumina crystal phase is present contains an alkali metal component in an oxide-converted amount of 0.01 to 8 mass %.

### Claim 11 (depends on 2)

A spark plug according to claim 2, wherein
the alumina-based sintered material is produced by mixing an alumina material and a secondary material formed of the Si component, an Mg component, the Group 2A component, and the RE component in a slurry, molding the granulated product, and firing a compact; and
the particle size ratio of the mean particle size of the alumina material contained in the slurry to that of the secondary material (Dalumina material/Dsecondary material) satisfies the following relationship:
1.3≦(Dalumina material/Dsecondary material)≦4.

### Claim 12 (depends on 3)

A spark plug according to claim 3, wherein
the alumina-based sintered material is produced by mixing an alumina material and a secondary material formed of the Si component, an Mg component, the Group 2A component, and the RE component in a slurry, molding the granulated product, and firing a compact; and
the particle size ratio of the mean particle size of the alumina material contained in the slurry to that of the secondary material (Dalumina material/Dsecondary material) satisfies the following relationship:
1.3≦(Dalumina material/Dsecondary material)≦4.

### Claim 13 (depends on 4)

A spark plug according to claim 4, wherein
the alumina-based sintered material is produced by mixing an alumina material and a secondary material formed of the Si component, an Mg component, the Group 2A component, and the RE component in a slurry, molding the granulated product, and firing a compact; and
the particle size ratio of the mean particle size of the alumina material contained in the slurry to that of the secondary material (Dalumina material/Dsecondary material) satisfies the following relationship:
1.3≦(Dalumina material/Dsecondary material)≦4.

### Claim 14 (depends on 2)

A spark plug according to claim 2, wherein
the Group 2A component contains Mg and Ba as essential elements and at least one element other than Mg and Ba among elements in Group 2A, and
the RE component is at least one member selected from the group consisting of an La component, a Pr component, and an Nd component.

### Claim 15 (depends on 3)

A spark plug according to claim 3, wherein
the Group 2A component contains Mg and Ba as essential and at least one element other than Mg and Ba among elements in Group 2A, and
the RE component is at least one member selected from the group consisting of an La component, a Pr component, and an Nd component.

### Claim 16 (depends on 4)

A spark plug according to claim 4, wherein
the Group 2A component contains Mg and Ba as essential elements and at least one element other than Mg and Ba among elements in Group 2A, and
the RE component is at least one member selected from the group consisting of an La component, a Pr component, and an Nd component.

### Claim 17 (depends on 5)

A spark plug according to claim 5, wherein
the Group 2A component contains Mg and Ba as essential and at least one element other than Mg and Ba among elements in Group 2A, and
the RE component is at least one member selected from the group consisting of an La component, a Pr component, and an Nd component.

### Claim 18 (depends on 2)

A spark plug according to claim 2, wherein
the insulator is held by a metallic shell, and
a screw portion formed around the outer surface of the metallic shell has a nominal diameter of 10 mm or smaller.

### Claim 19 (depends on 3)

A spark plug according to claim 3, wherein
the insulator is held by a metallic shell, and
a screw portion formed around the outer surface of the metallic shell has a nominal diameter of 10 mm or smaller.

### Claim 20 (depends on 4)

A spark plug according to claim 4, wherein
the insulator is held by a metallic shell, and
a screw portion formed around the outer surface of the metallic shell has a nominal diameter of 10 mm or smaller.

### Claim 21 (depends on 5)

A spark plug according to claim 5, wherein
the insulator is held by a metallic shell, and
a screw portion formed around the outer surface of the metallic shell has a nominal diameter of 10 mm or smaller.

### Claim 22 (depends on 6)

A spark plug according to claim 6, wherein
the insulator is held by a metallic shell, and
a screw portion formed around the outer surface of the metallic shell has a nominal diameter of 10 mm or smaller.