# US 8,278,739 B2 · Crystalline semiconductor film, semiconductor device, and method for manufacturing thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,739 B2
- Document ID: US8278739B2
- Status: Granted
- Kind: B2
- Application number: 11/715,473
- Filed: 2007-03-08
- Published: 2007-09-27
- Granted: 2012-10-02
- Earliest claimed: 2006-03-20
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Tomoaki Moriwaka
- Web page: https://patentgrep.com/patent/US8278739B2

## CPC

- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10D 62/405: {Orientations of crystalline planes}
- H10D 86/0214: {using temporary substrates}
- H10D 86/0229: {characterised by control of the annealing or irradiation parameters}
- H10W 72/0198: {batch processes}
- H10W 72/9223: {with redistribution layers [RDL]}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing is: forming an insulating film over a substrate; forming an amorphous semiconductor film over the insulating film; forming over the amorphous semiconductor film, a silicon nitride film in which a film thickness is equal to or more than 200 nm and equal to or less than 1000 nm, equal to or less than 10 atomic % of oxygen is included, and a relative proportion of nitrogen to silicon is equal to or more than 1.3 and equal to or less than 1.5; irradiating the amorphous semiconductor film with a continuous-wave laser light or a laser light with repetition rate of equal to or more than the wave length of 10 MHz transmitting the silicon nitride film to melt and later crystallize the amorphous semiconductor film to form a crystalline semiconductor film.

## Claims

### Claim 1

A method for manufacturing a semiconductor device comprising:
forming an insulating film over a substrate;
forming an amorphous semiconductor film having a film thickness of equal to or more than 20 nm and equal to or less than 80 nm over the insulating film;
forming, over the amorphous semiconductor film, a silicon nitride film in which a film thickness is 200 nm to 1000 nm, equal to or less than 10 atomic % of oxygen is included, and a relative proportion of nitrogen to silicon is equal to or more than 1.3 and equal to or less than 1.5; and
forming a crystalline semiconductor film from the amorphous semiconductor film by irradiating the amorphous semiconductor film with a laser light through the silicon nitride film such that energy of the laser light is absorbed in the amorphous semiconductor film,
wherein at a first plane of the crystalline semiconductor film, a ratio of crystal grains of an orientation of <001> within a range of ±10° of angle fluctuation is equal to or more than 60% and less than 100%,
wherein at a second plane of the crystalline semiconductor film, a ratio of crystal grains of an orientation of any one of <001>, <101>, <201>, <301>, <401>, <501>, or <601> within a range of ±10° of angle fluctuation is equal to or more than 60% and less than 100%,
wherein at a third plane of the crystalline semiconductor film, a ratio of crystal grains of an orientation of any one of <001>, <101>, <201>, <301>, <401>, <501>, or <601> within a range of ±10° of angle fluctuation is equal to or more than 60% and less than 100%,
wherein a normal vector of the first plane is perpendicular to the surface of the substrate,
wherein a normal vector of the second plane is parallel to the surface of the substrate and is parallel to the direction of crystal growth of crystal grain,
wherein a normal vector of the third plane is parallel to the surface of the substrate and is perpendicular to the direction of crystal growth of crystal grain, and
wherein the laser light is a continuous-wave laser light or a laser light with repetition rate of equal to or more than 10 MHz.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the silicon nitride film including oxygen is formed by plasma CVD in an atmosphere including SiH4, NH3, and N20.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the silicon nitride film including oxygen is formed by plasma CVD in an atmosphere including SiH4 and NH3.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the amorphous semiconductor film has a film thickness of equal to or more than 20 nm and equal to or less than 80 nm.

### Claim 5

A method for manufacturing a semiconductor device comprising:
forming an insulating film over a substrate;
forming an amorphous semiconductor film having a film thickness of equal to or more than 20 nm and equal to or less than 80 nm over the insulating film;
forming, over the amorphous semiconductor film, a silicon nitride film in which a film thickness is 200 nm to 1000 nm, equal to or less than 10 atomic % of oxygen is included, and a relative proportion of nitrogen to silicon is equal to or more than 1.3 and equal to or less than 1.5;
forming a crystalline semiconductor film from the amorphous semiconductor film by irradiating the amorphous semiconductor film with a laser light through the silicon nitride film such that energy of the laser light is absorbed in the amorphous semiconductor film; and
forming a semiconductor element using the crystalline semiconductor film,
wherein at a first plane of the crystalline semiconductor film, a ratio of crystal grains of an orientation of <001> within a range of ±10′ of angle fluctuation is equal to or more than 60% and less than 100%,
wherein at a second plane of the crystalline semiconductor film, a ratio of crystal grains of an orientation of any one of <001>, <101>, <201>, <301>, <401>, <501>, or <601> within a range of ±10″ of angle fluctuation is equal to or more than 60% and less than 100%,
wherein at a third plane of the crystalline semiconductor film, a ratio of crystal grains of an orientation of any one of <001>, <101>, <201>, <301>, <401>, <501>, or <601> within a range of ±10′ of angle fluctuation is equal to or more than 60% and less than 100%,
wherein a normal vector of the first plane is perpendicular to the surface of the substrate,
wherein a normal vector of the second plane is parallel to the surface of the substrate and is parallel to the direction of crystal growth of crystal grain,
wherein a normal vector of the third plane is parallel to the surface of the substrate and is perpendicular to the direction of crystal growth of crystal grain, and
wherein the laser light is a continuous-wave laser light or a laser light with repetition rate of equal to or more than 10 MHz.

### Claim 6 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the silicon nitride film including oxygen is formed by plasma CVD in an atmosphere including SiH4, NH3, and N2O.

### Claim 7 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the silicon nitride film including oxygen is formed by plasma CVD in an atmosphere including SiH4 and NH3.

### Claim 8 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the amorphous semiconductor film has a film thickness of equal to or more than 20 nm and equal to or less than 80 nm.

### Claim 9 (depends on 1)

The method for manufacturing a crystalline semiconductor film according to claim 1, wherein the irradiating is performed while scanning the continuous-wave laser light or the laser light with repetition rate of equal to or more than 10 MHz.

### Claim 10 (depends on 9)

The method for manufacturing a crystalline semiconductor film according to claim 9, wherein a crystal grain in the crystalline semiconductor film formed by the irradiating is long along a direction of the scanning.

### Claim 11 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the irradiating is performed while scanning the continuous-wave laser light or the laser light with repetition rate of equal to or more than 10 MHz.

### Claim 12 (depends on 11)

The method for manufacturing a semiconductor device according to claim 11, wherein a crystal grain in the crystalline semiconductor film formed by the irradiating is long along a direction of the scanning.

### Claim 13 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the semiconductor device is used for a display device.

### Claim 14 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the semiconductor device is a thin film transistor.