# US 8,278,735 B2 · Yttrium and titanium high-k dielectric films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,735 B2
- Document ID: US8278735B2
- Status: Granted
- Kind: B2
- Application number: 12/901,239
- Filed: 2010-10-08
- Published: 2012-03-15
- Granted: 2012-10-02
- Earliest claimed: 2010-09-09
- Assignees: Intermolecular, Inc.
- Inventors: Imran Hashim; Indranil De; Tony Chiang; Edward Haywood; Hanhong Chen; Nobi Fuchigami; Pragati Kumar; Sandra Malhotra; Sunil Shanker
- Web page: https://patentgrep.com/patent/US8278735B2

## CPC

- H10D 1/68: Capacitors having no potential barriers
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/3464: {using more than one target (C23C14/56 takes precedence)}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/45531: {specially adapted for making ternary or higher compositions}
- H10P 14/6329: {using physical ablation of a target, e.g. physical vapour deposition or pulsed laser deposition}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69394: {the material containing titanium, e.g. TiO2}
- H10P 14/69396: {the material containing at least one rare earth metal element, e.g. oxides of lanthanides, scandium or yttrium}
- H10P 14/69397: {the material containing two or more metal elements}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

This disclosure provides (a) methods of making an oxide layer (e.g., a dielectric layer) based on yttrium and titanium, to have a high dielectric constant and low leakage characteristic and (b) related devices and structures. An oxide layer having both yttrium and titanium may be fabricated either as an amorphous oxide or as an alternating series of monolayers. In several embodiments, the oxide is characterized by a yttrium contribution to total metal that is specifically controlled. The oxide layer can be produced as the result of a reactive process, if desired, via either a PVD process or, alternatively, via an atomic layer deposition process that employs specific precursor materials to allow for a common process temperature window for both titanium and yttrium reactions.

## Claims

### Claim 1

An apparatus, comprising:
a first conductive layer;
a second conductive layer; and
a dielectric between the first conductive layer and the second conductive layer, the dielectric including a yttrium-titanium-oxide, layer having a yttrium-to-total-metal constituency of between approximately one to five percent yttrium.

### Claim 2 (depends on 1)

The apparatus of claim 1, wherein the dielectric has substantially no XRAY diffraction peak associated with crystalline titanium oxide or crystalline yttrium oxide so that the yttrium-titanium-oxide layer represents an amorphous state.

### Claim 3 (depends on 1)

The apparatus of claim 1, wherein the yttrium-titanium-oxide, layer has a yttrium-to-total metal constituency of between one and two percent yttrium.

### Claim 4 (depends on 1)

The apparatus of claim 1, wherein one of the conductive layers includes a material selected from a group consisting of: ruthenium, ruthenium oxide, platinum, a metal nitride, iridium, iridium oxide, silicon and a silicide.

### Claim 5 (depends on 1)

The apparatus of claim 1, wherein the dielectric has a dielectric constant of at least fifty-five.

### Claim 6 (depends on 1)

The apparatus of claim 1, wherein the dielectric has a thickness of less than twenty nanometers.

### Claim 7 (depends on 1)

The apparatus of claim 1, embodied as a component of a memory cell.

### Claim 8 (depends on 7)

The apparatus of claim 7, further comprising a control transistor to selectively couple charge to one of the conductors, the control transistor cooperating with the capacitor structure to form a dynamic access memory cell.

### Claim 9 (depends on 8)

The apparatus of claim 8, embodied as an integrated circuit-based array of the dynamic access memory cells.

### Claim 10 (depends on 1)

The apparatus of claim 1, wherein the first conductive layer, the second conductive layer, and the dielectric form a capacitor having a shape selected from a group consisting of: a crown-shaped capacitor, a pillar-shaped capacitor, and a cylinder-shaped capacitor.

### Claim 11 (depends on 1)

The apparatus of claim 1, wherein the dielectric is substantially amorphous.

### Claim 12

An apparatus, comprising:
a first conductive layer;
a second conductive layer; and
an amorphous oxide layer between the first conductive layer and the second conductive layer, the amorphous oxide layer comprising yttrium and titanium and wherein the amorphous oxide layer is characterized by a structure having substantially no crystalline yttrium oxide and substantially no crystalline titanium oxide, and wherein the amorphous oxide layer has a dielectric constant equal to or greater than fifty-five.

### Claim 13 (depends on 12)

The apparatus of claim 12, wherein the amorphous oxide layer is characterized by a metal constituency of between approximately one to five percent yttrium.

### Claim 14 (depends on 12)

The apparatus of claim 12, wherein the amorphous oxide layer is composed substantially of yttrium-titanium-oxide.

### Claim 15 (depends on 12)

The apparatus of claim 12, wherein the amorphous oxide layer is further characterized by a metal constituency of between one to two percent yttrium.

### Claim 16 (depends on 12)

The apparatus of claim 12, wherein one of the conductive layers includes a material selected from a group consisting of: ruthenium, ruthenium oxide, platinum, metal nitrides, iridium, iridium oxide, tungsten, tungsten oxide, molybdenum and molybdenum oxide.

### Claim 17 (depends on 12)

The apparatus of claim 12, wherein the amorphous oxide layer has a thickness of less than twenty nanometers.

### Claim 18 (depends on 12)

The apparatus of claim 12, embodied as a component of a memory cell.

### Claim 19 (depends on 18)

The apparatus of claim 18, further comprising a control transistor to selectively couple charge to one of the conductive layers, the control transistor cooperating with the capacitor structure to form a dynamic access memory cell.

### Claim 20 (depends on 18)

The apparatus of claim 18 embodied as an integrated circuit-based array of the dynamic access memory cells.

### Claim 21 (depends on 18)

The apparatus of claim 18, wherein the amorphous oxide layer is substantially noncrystalline in structure.

### Claim 22 (depends on 12)

The apparatus of claim 12, wherein the first conductive layer, the second conductive layer, and the amorphous oxide layer form a capacitor having a shape selected from a group consisting of: a crown-shaped capacitor, a pillar shaped capacitor, and a cylinder-shaped capacitor.