# US 8,278,624 B2 · Lutetium oxyorthosilicate scintillator having improved scintillation and optical properties and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,624 B2
- Document ID: US8278624B2
- Status: Granted
- Kind: B2
- Application number: 11/842,813
- Filed: 2007-08-21
- Published: 2011-10-27
- Granted: 2012-10-02
- Earliest claimed: 2006-08-21
- Assignees: Siemens Medical Solutions USA, Inc.; University of Tennessee Research Foundation
- Inventors: Merry A. Koschan; Charles L. Melcher; Piotr Szupryczynski; A. Andrew Carey
- Web page: https://patentgrep.com/patent/US8278624B2

## CPC

- C09K 11/77742: {Silicates}
- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 29/34: Silicates
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

LSO scintillation crystals with improved scintillation and optical properties are achieved by controlled co-doping a LSO crystal melt with amounts of cerium and an additional codopant such as calcium or other divalent cations. Crystal growth atmosphere is optimized by controlling the amount of oxygen in the atmosphere. Zinc is added as an additional material to restabilize crystal growth where calcium co-dopant is added. The decay time of the scintillation crystal can be controlled by controlling the concentration of co-dopant added.

## Claims

### Claim 1

A method of forming LSO scintillation crystals, comprising the steps of:
forming a material mixture for the growth of an LSO crystal, having equimolar amounts of Ce and a co-dopant selected from the group consisting of Ca, Ba, Mg, Li, Na, K, and Sr;
melting said mixture to form a melt; and
growing a crystal from said melt from a seed crystal.

### Claim 2 (depends on 1)

The method of claim 1, wherein said co-dopant is divalent calcium.

### Claim 3 (depends on 1)

The method of claim 1, further comprising adding a predetermined amount of an element selected from the group of Zn, Sn, Pb and Cd to said material mixture.

### Claim 4 (depends on 1)

The method of claim 1, further comprising controlling a growth atmosphere to contain a predetermined amount of oxygen.

### Claim 5 (depends on 4)

The method of claim 4, wherein said amount of oxygen has a range of 0.1-5%.

### Claim 6 (depends on 1)

The method of claim 1, wherein the atomic percent ratio of Ce is 0.1.

### Claim 7 (depends on 1)

The method of claim 1, comprising the step of further varying the amount of co-dopant to vary the scintillation decay time of the resulting LSO crystal.

### Claim 8 (depends on 1)

An LSO scintillation crystal made from the method of claim 1.

### Claim 9

A method of forming an LSO scintillation crystal with controlled, selected scintillation decay times, comprising adding a non-rare-earth co-dopant to a material mixture containing cerium, from which said crystal is formed, wherein the concentration of the co-dopant is varied in accordance with a desired scintillation decay time of the LSO scintillation crystal.

### Claim 10 (depends on 9)

The method of claim 9, wherein said co-dopant is Ca2+.

### Claim 11 (depends on 10)

The method of claim 10, wherein the cerium concentration is 0.1 atomic percent.

### Claim 12 (depends on 10)

The method of claim 10, further comprising adding a predetermined amount of an element selected from the group of Zn, Sn, Pb and Cd to said material mixture.

### Claim 13 (depends on 9)

The method of claim 9, further comprising controlling a crystal growth atmosphere to contain a predetermined amount of oxygen.

### Claim 14 (depends on 13)

The method of claim 13, wherein said amount of oxygen has a range of 0.1-5%.

### Claim 15 (depends on 9)

The method of claim 9, wherein said LSO scintillation crystal has a decay time of less than 38 ns.

### Claim 16 (depends on 9)

The method of claim 9, wherein the co-dopant is Ca2+, and wherein said crystal is formed by melting said mixture to form a melt; and growing a crystal from said melt from a seed crystal.

### Claim 17

An LSO:Ce scintillation crystal doped with an additional, non-rare-earth element, the crystal having a decay time of less than 38 ns.

### Claim 18 (depends on 17)

The LSO:Ce scintillation crystal of claim 17, wherein said decay time is on the order of 37 ns.

### Claim 19 (depends on 17)

The LSO:Ce scintillation crystal of claim 17, wherein said decay time is less than 33 ns.

### Claim 20 (depends on 19)

The LSO:Ce scintillation crystal of claim 19, wherein said decay time is on the order of 28.5 ns.

### Claim 21

A method of forming LSO scintillation crystals, comprising the steps of:
forming a material mixture for the growth of an LSO crystal, having predetermined amounts of Ce and Ca2+;
melting said mixture to form a melt; and
growing a crystal from said melt from a seed crystal.

### Claim 22 (depends on 21)

An LSO crystal formed from the method of claim 21.

### Claim 23

A method of forming LSO scintillation crystals, comprising the steps of:
forming a material mixture for the growth of an LSO crystal, having predetermined amounts of Ce and Ca2+, and a predetermined amount of Zn;
melting said mixture to form a melt; and
growing a crystal from said melt from a seed crystal, in an environment containing a predetermined level of oxygen.

### Claim 24 (depends on 23)

The method of claim 23, wherein said level of oxygen is in the range of 0.1-5%.

### Claim 25

A method of forming LSO scintillation crystals, comprising the steps of:
forming a material mixture for the growth of an LSO crystal, having predetermined amounts of Ce and a co-dopant selected from the group consisting of Ca, Ba, Mg, Li, Na, K, and Sr, without being silicon deficient;
melting said mixture to form a melt; and
growing a crystal from said melt.

### Claim 26 (depends on 25)

The method of claim 25, wherein a predetermined amount of an element selected from the group consisting of group IB elements is added to said material mixture.

### Claim 27 (depends on 25)

The method of claim 25, wherein a predetermined amount of an element selected from the group consisting of Zn, Sn, Cd and Pb is added to said material mixture.

### Claim 28 (depends on 25)

The method of claim 25, further comprising controlling a crystal growth atmosphere to contain a predetermined amount of oxygen.

### Claim 29 (depends on 28)

The method of claim 28, wherein said amount of oxygen has a range of 0.1-5%.

### Claim 30

An LSO:Ce scintillation crystal having a decay time of less than 33 ns.

### Claim 31 (depends on 30)

The LSO:Ce scintillation crystal of claim 30, wherein said decay time is on the order of 28.5 ns.