# US 8,278,589 B2 · Continuous furnace with coupled laser for the surface treatment of materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,589 B2
- Document ID: US8278589B2
- Status: Granted
- Kind: B2
- Application number: 12/282,023
- Filed: 2007-03-06
- Published: 2009-09-17
- Granted: 2012-10-02
- Earliest claimed: 2006-03-07
- Assignees: Consejo Superior de Investigaciones Cientificas
- Inventors: Luis Carlos Estepa Millan; German Francisco Fuente Leis
- Web page: https://patentgrep.com/patent/US8278589B2

## CPC

- B23K 26/12: in a special environment or atmosphere, e.g. in an enclosure
- B23K 26/082: Scanning systems, i.e. devices involving movement of the laser beam relative to the laser head
- B23K 26/0838: {by using an endless conveyor belt}
- B23K 26/127: {in an enclosure}
- C03C 23/0025: {by a laser beam}
- C03C 23/007: {by thermal treatment}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- F27B 9/2469: {the conveyor being constituted by rollable bodies}
- F27B 9/36: Arrangements of heating devices
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS

## Abstract

A continuous furnace 4 to which a laser is coupled by conventional optical means that allows the surface treatment of a part, with which it is possible to achieve temperatures of up to 3000° C. on said surface while the remainder of the part is at a substantially lower temperature. The part in the furnace is heated to a temperature of the order of 500° C. and, via an opening 5, a laser-beam bundle is applied to the part, scanning a line perpendicular to the direction of movement of the part such that the entire surface is scanned by means of the mechanical advance of the part. This scanning should extend beyond the lateral ends of the part. This type of laser-beam generator must be made compatible with the various colors with which the surface of the part is decorated. The furnace is divided into different zones, with independent temperature controls, for successfully achieving the desired values, both for heating and for cooling. The system that generates laser radiation and its deflector comprises a radiation generation/emission cavity (CO2 laser, around 10.6 mm, or diode or Nd lasers in different varieties thereof) and the emitted-beam-handling system, which may consist of a system of galvanometers or a series of combinations of lenses for successfully shaping the beam and applying it in a manner suited to the type of process, material treated and laser used.

## Claims

### Claim 1

A system for treating a surface of a material, comprising:
a continuous kiln, comprising:
a means for conveying a material through the kiln,
an enclosure having an exterior top surface comprising an inlet, and
two or more zones in the enclosure, wherein each zone is maintained at a different temperature, and
a laser positioned such that a laser beam emitted by the laser enters through the enclosure inlet
wherein the zones comprise:
a first zone located before exposure to the laser beam, wherein the temperature is less than the temperature of the surface of the material during contact with the laser beam, and less than the melting point of the material;
a second zone located where exposure to the laser beam occurs;
a third zone located after exposure to the laser beam; and
a fourth zone located after the third zone,
wherein the temperature declines between the third zone and the fourth zone at a controlled rate, and
wherein the material has a top surface and side edges, and
wherein the laser sweeps across the top surface of the material while the material moves through the kiln and is conveyed in a direction perpendicular to the direction of the emitted laser beam, the laser beam sweeping in a pendular motion over a fixed line as the material is conveyed through the kiln and,
wherein the sweep of the laser beam surpasses the side edges of the material.

### Claim 2 (depends on 1)

The system of claim 1, wherein the enclosure inlet and the enclosure are made from the same material, and wherein the enclosure inlet protrudes from the exterior top surface of the enclosure at an angle of less than 90°.

### Claim 3 (depends on 1)

The system of claim 1, wherein the enclosure is thermally insulated.

### Claim 4 (depends on 1)

The system of claim 1, wherein the temperature of the top surface of the material is less than or equal to 3000° C.

### Claim 5 (depends on 1)

The system of claim 1, wherein the laser is selected from CO2 lasers, diodes, and Nd lasers.

### Claim 6 (depends on 1)

The system of claim 1, wherein the laser beam has a wavelength ranging from 0.8 μm to 1.1 μm.

### Claim 7 (depends on 1)

The system of claim 1, further comprising a plane lens to offset decreased laser beam power at the side edges of the material.

### Claim 8 (depends on 1)

The system of claim 1, further comprising a means for heating the area inside the enclosure.

### Claim 9 (depends on 8)

The system of claim 8, wherein the means for heating the area inside the enclosure is selected from electrical elements, gas, and fuel combustion.

### Claim 10 (depends on 1)

The system of claim 1, further comprising:
a means for generating ultraviolet to infrared radiation; and
a means for altering the position of the emitted laser beam.

### Claim 11 (depends on 10)

The system of claim 10, wherein means for generating ultraviolet to infrared radiation comprises a radiation generation and emission cavity.

### Claim 12 (depends on 1)

The system of claim 1, further comprising a means for controlling the direction of the laser beam emitted by the laser.

### Claim 13 (depends on 12)

The system of claim 12, wherein the means for controlling the direction of the emitted beam comprises an opto-mechanical configuration,
wherein the opto-mechanical configuration comprises a galvanometer system or a system of lens and mirror combinations that controllably oscillate, and adjusts the direction and shape of the laser beam to desired settings.

### Claim 14 (depends on 1)

The system of claim 1, further comprising a computer having a processor, computer readable medium, and computer readable medium encoded with software configured to control the required intensity, emission time, stoppage, and movement of the radiation.

### Claim 15

A method for treating the surface of a material, comprising the steps of:
(a) placing a material in a continuous kiln, comprising an enclosure having an exterior top surface comprising an inlet, wherein the material has a top surface and side edges and wherein the material passes through two or more zones in the enclosure, wherein each zone is maintained at a different temperature and wherein the zones in the enclosure comprise:
a first zone located before exposure to the laser beam, wherein the temperature is less than the temperature of the surface of the material during contact with the laser beam, and less than the melting point of the material;
a second zone located where exposure to the laser beam occurs;
a third zone located after exposure to the laser beam; and
a fourth zone located after the third zone,
wherein the temperature declines between the third zone and the fourth zone at a controlled rate;
and
(b) propagating a laser beam through the enclosure inlet, such that the laser beam sweeps across the top surface of the material as it moves through the kiln, in a pendular motion over a fixed line as the material is conveyed through the kiln and in a direction perpendicular to the direction of the material moving through the kiln, and wherein the sweep of the laser beam surpasses the side edges of the material.

### Claim 16 (depends on 15)

The method of claim 15, wherein the portion of the material not exposed to the laser beam has a lower temperature than the portion of the material exposed to the laser beam.