# US 8,278,555 B2 · Electric wire conductor and a method of producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,555 B2
- Document ID: US8278555B2
- Status: Granted
- Kind: B2
- Application number: 12/312,033
- Filed: 2007-10-30
- Published: 2010-03-25
- Granted: 2012-10-02
- Earliest claimed: 2006-10-30
- Assignees: Autonetworks Technologies, Ltd.; Sumitomo Wiring Systems, Ltd.; Sumitomo Electric Industries, Ltd.
- Inventors: Yasuyuki Otsuka; Yoshihiro Nakai; Taichirou Nishikawa
- Web page: https://patentgrep.com/patent/US8278555B2

## CPC

- H01B 1/023: {Alloys based on aluminium}
- C21D 9/60: with induction heating
- C22C 21/02: with silicon as the next major constituent
- C22C 21/08: with silicon
- C22F 1/00: Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working (apparatus for mechanical working of metal B21, B23, B24)
- C22F 1/02: in inert or controlled atmosphere or vacuum (adjusting the composition of the atmosphere C21D1/76)
- C22F 1/04: of aluminium or alloys based thereon
- Y02P 10/25: Process efficiency
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A conductor includes elemental wires made from an aluminum alloy containing Si whose content is 0.3-1.2 mass %, Mg whose content makes an Mg/Si weight ratio in a range from 0.8 to 1.8, and a remainder essentially including Al and an unavoidable impurity. The conductor has tensile strength of 240 MPa or more, breaking elongation of 10% or more, impact absorption energy of 8 J/m or more, and electrical conductivity of 40% IACS or more. The production method includes the step of preparing a strand by bunching elemental wires with the above composition, and the step of subjecting the wire to solution treatment, quenching, and aging heat treatment. Solution treatment temperature is 500-580° C., and aging heat treatment temperature is 150-220° C. Heating in solution treatment is high frequency induction heating.

## Claims

### Claim 1

A conductor comprising a plurality of elemental wires made from an aluminum alloy, the aluminum alloy containing:
Si whose content is 0.3 to 1.2 mass %;
Mg whose content makes an Mg/Si weight ratio in a range from 0.8 to 1.8; and
a remainder essentially including Al and an unavoidable impurity, wherein the conductor has tensile strength of 240 MPa or more, breaking elongation of 10% or more, impact absorption energy of 8 J/m or more, and electrical conductivity of 40% IACS or more, wherein,
the aluminum alloy further contains one or two elements selected from the group consisting of no more than 500 ppm Ti and no more than 50 ppm B.

### Claim 2 (depends on 1)

The conductor according to claim 1, wherein the aluminum alloy further contains one or more elements selected from the group consisting of Fe, Cu, Cr, and Mn, where a total content of the one or more elements is 0.5 mass % or less.

### Claim 3 (depends on 1)

The conductor according to claim 1, wherein the conductor has a cross-sectional area of 0.75 mm2 or less.

### Claim 4

A method of producing a conductor, the method comprising the steps of:
preparing a strand by bunching a plurality of elemental wires made from an aluminum alloy containing Si whose content is 0.3 to 1.2 mass %, Mg whose content makes an Mg/Si weight ratio in a range from 0.8 to 1.8, and a remainder essentially including Al and an unavoidable impurity; and
subjecting the strand to solution treatment, then subjecting the strand to quenching, and then subjecting the strand to aging heat treatment, wherein
the aluminum alloy further contains one or two elements selected from the group consisting of no more than 500 ppm Ti and no more than 50 ppm B.

### Claim 5 (depends on 4)

The method according to claim 4, wherein a heating temperature when subjecting the strand to the solution treatment is 500 to 580° C., and a heating temperature when subjecting the strand to the aging heat treatment is 150 to 220° C.

### Claim 6 (depends on 4)

The method according to claim 4, wherein heating during the solution treatment is high frequency induction heating.

### Claim 7 (depends on 2)

The conductor according to claim 2, wherein the conductor has a cross-sectional area of 0.75 mm2 or less.

### Claim 8 (depends on 1)

The conductor according to claim 1, wherein the conductor has a cross-sectional area of 0.75 mm2 or less.

### Claim 9 (depends on 5)

The method according to claim 5, wherein heating during the solution treatment is high frequency induction heating.