# US 8,278,409 B2 · Copolymers of epsilon-caprolactone and glycolide for melt blown nonwoven applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,409 B2
- Document ID: US8278409B2
- Status: Granted
- Kind: B2
- Application number: 12/107,614
- Filed: 2008-04-22
- Published: 2009-10-22
- Granted: 2012-10-02
- Earliest claimed: 2008-04-22
- Assignees: Ethicon, Inc.
- Inventors: Modesto Erneta; Dennis D. Jamiolkowski; Jianguo Jack Zhou; Sasa Andjelic
- Web page: https://patentgrep.com/patent/US8278409B2

## CPC

- C08G 63/08: Lactones or lactides
- B29C 48/05: Filamentary, e.g. strands
- B29C 48/397: {using a single screw}
- B29C 48/625: characterised by the ratio of the threaded length of the screw to its outside diameter [L/D ratio]
- B29C 48/9185: {in the direction of the stream of the material}
- D04H 1/56: in association with fibre formation, e.g. immediately following extrusion of staple fibres
- D04H 3/02: characterised by the method of forming fleeces or layers, e.g. reorientation of yarns or filaments
- D04H 3/16: with bonds between thermoplastic filaments produced in association with filament formation, e.g. immediately following extrusion
- B29C 2948/92514: Pressure
- B29C 2948/9259: Angular velocity
- B29C 2948/92704: Temperature
- B29C 2948/92885: Screw or gear
- B29C 2948/92895: Barrel or housing
- B29C 2948/92904: Die; Nozzle zone
- Y10T 442/68: Melt-blown nonwoven fabric
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Copolymers exhibiting the following combinations of properties, including without limitation, ε-caprolactone in an amount ranging from about 12 to about 70 mole percent, glycolide in an amount ranging from about 30 to about 88 mole percent, crystallinity ranging from about 10 to about 50% as measured by WAXD or about 10 to about 50 J/g as measured by DSC, and an inherent viscosity ranging from about 0.5 to about 1.45 dL/g as measured in a 0.1 g/dl solution of HFIP at 25° C.; a method for melt blowing such copolymers and nonwoven constructs produced therefrom are described herein.

## Claims

### Claim 1

A copolymer for use in the production of nonwoven constructs, the copolymer comprising ε-caprolactone in an amount ranging from 12 to 20 mole percent, glycolide in an amount ranging from 80 to 88 mole percent, crystallinity ranging from 10 and 50% as measured by WAXD or 10 to 50 J/g as measured by DSC, and an inherent viscosity ranging from 0.5 to 1.45 dL/g as measured in a 0.1 g/dl solution of HFIP at 25° C., wherein the copolymer is the reaction product of a predominant amount of a prepolymer of ε-caprolactone and glycolide having a mole ratio of ε-caprolactone/glycolide of less than 30/70, with a balance of glycolide.

### Claim 2 (depends on 1)

The copolymer of claim 1, wherein the crystallinity ranging from 10 to 35% as measured by WAXD or 10 to 35 J/g as measured by DSC.

### Claim 3 (depends on 2)

The copolymer of claim 2, wherein the crystallinity ranging from 25 to 35% as measured by WAXD or 25 to 35 J/g as measured by DSC.

### Claim 4 (depends on 1)

The copolymer of claim 1, wherein the inherent viscosity ranging from 0.74 to 1.45 dL/g as measured in a 0.1 g/dL solution of HFIP at 25° C.