# US 8,278,392 B2 · Process for producing propylene resin composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,392 B2
- Document ID: US8278392B2
- Status: Granted
- Kind: B2
- Application number: 12/656,841
- Filed: 2010-02-17
- Published: 2010-06-17
- Granted: 2012-10-02
- Earliest claimed: 2004-04-13
- Assignees: Sumitomo Chemical Company, Limited
- Inventors: Satoru Moritomi; Takashi Sanada; Mitsuyoshi Shimano
- Web page: https://patentgrep.com/patent/US8278392B2

## CPC

- C08F 297/083: {the monomers being ethylene or propylene}
- C08F 297/08: polymerising mono-olefins
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/035: containing four or more polymers in a blend
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Disclosed are processes for producing polypropylene resin compositions including two or three sorts of propylene-based polymeric materials, the processes including a first step of melt-kneading at least a propylene-α-olefin block copolymer containing a polymer portion composed mainly of propylene and a propylene-α-olefin copolymer portion having a relatively high intrinsic viscosity and a second step of melt-kneading the product of the first step with a propylene-ethylene block copolymer containing a polymer portion composed mainly of propylene and a propylene-ethylene copolymer portion having a relatively low intrinsic viscosity or a polymer portion composed mainly of propylene having a relatively low intrinsic viscosity. In the composition produced by these processes, no or substantially no fish eyes develop.

## Claims

### Claim 1

A process for producing a polypropylene resin composition comprising 5-50% by weight of a component (I) defined below and 50-95% by weight of a component (II) defined below, the amounts in % by weight being on the basis of a total of the weight of the component (I) expressed by WI and the weight of the component (II) expressed by WII, wherein the process comprises a 1st step and a 2nd step each defined below:
component (I):
a propylene-α-olefin block copolymer (I) which consists of 2-65% by weight of a polymer portion (I-A) obtained by polymerizing, in a first stage, monomers mainly including propylene and 35-98% by weight of a polymer portion (I-B) obtained by polymerizing, in a second stage, propylene and α-olefin other than propylene, the amounts in % by weight being on the basis of the whole weight of the copolymer (I), wherein the content of the α-olefin contained in the polymer portion (I-B) is 10-50% by weight on the basis of the whole weight of the monomers contained in the polymer portion (I-B), and the intrinsic viscosity [η] B of the polymer portion (I-B) is not less than 4 dl/g but not more than 10 dl/g;
component (II):
a propylene-ethylene block copolymer (II) which comprises 60-99% by weight of a polymer portion (II-A) obtained by polymerizing, in a first stage, monomers mainly including propylene and 1-40% by weight of a polymer portion (II-B) obtained by polymerizing, in a second stage, monomers including ethylene and propylene, the amounts in % by weight being on the basis of the whole weight of the copolymer (II), wherein the content of ethylene contained in the polymer portion (II-B) is 10-50% by weight on the basis of the whole weight of the monomers contained in the polymer portion (II-B), the intrinsic viscosity [η] B of the polymer portion (II-B) is not less than 1 dl/g but less than 3 dl/g, and the ratio of the intrinsic viscosity [η]B of the polymer portion (II-B) to the intrinsic viscosity [η]A of the polymer portion (II-A), [η]B/[η]A, is not less than 1 but not more than 4.5;
1st step:
a step of melt-kneading the component (I) of an amount of WI and the component (II) of an amount less than WI together to produce an intermediate composition;
2nd step:
a step of melt-kneading the rest of the component (II) and the intermediate composition obtained in the 1st step together to produce a final composition.

### Claim 2 (depends on 1)

The process according to claim 1, wherein in the 1st step a product resulting from the melt-kneading is not solidified to form the intermediate composition in an unsolidified state and in the 2nd step the rest of the component (II) and the unsolidified intermediate composition are combined.

### Claim 3

A process for producing a polypropylene resin composition comprising 5-50% by weight of a component (I) defined below and 50-95% by weight of a component (II) defined below, the amounts in % by weight being on the basis of a total of the weight of the component (I) expressed by WI and the weight of the component (II) expressed by WII, wherein the process comprises a 1st step and a 2nd step each defined below:
component (I):
a propylene-α-olefin block copolymer (I) which consists of 2-65% by weight of a polymer portion (I-A) obtained by polymerizing, in a first stage, monomers mainly including propylene and 35-98% by weight of a polymer portion (I-B) obtained by polymerizing, in a second stage, propylene and α-olefin other than propylene, the amounts in % by weight being on the basis of the whole weight of the copolymer (I), wherein the content of the α-olefin contained in the polymer portion (I-B) is 10-50% by weight on the basis of the whole weight of the monomers contained in the polymer portion (I-B), and the intrinsic viscosity [η]B of the polymer portion (I-B) is not less than 4 dl/g but not more than 10 dl/g;
component (II):
a propylene-ethylene block copolymer (II) which comprises 60-99% by weight of a polymer portion (II-A) obtained by polymerizing, in a first stage, monomers mainly including propylene and 1-40% by weight of a polymer portion (II-B) obtained by polymerizing, in a second stage, monomers including ethylene and propylene, the amounts in % by weight being on the basis of the whole weight of the copolymer (II), wherein the content of ethylene contained in the polymer portion (II-B) is 10-50% by weight on the basis of the whole weight of the monomers contained in the polymer portion (II-B) the intrinsic viscosity [η]B of the polymer portion (II-B) is not less than 1 dl/g but less than 3 dl/g, and the ratio of the intrinsic viscosity [η]B of the polymer portion (II-B) to the intrinsic viscosity [η]A of the polymer portion (II-A), [η]B/[η]A, is not less than 1 but not more than 4.5;
1st step:
a step of melt-kneading the component (I) of an amount of WI to produce a melt-kneaded material;
2nd step:
a step of melt-kneading the component (II) of an amount of WII and the melt-kneaded material obtained in the 1st step together to produce a composition.