# US 8,278,383 B2 · Methods of preparing polymer-organoclay composites and articles derived therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,383 B2
- Document ID: US8278383B2
- Status: Granted
- Kind: B2
- Application number: 13/430,801
- Filed: 2012-03-27
- Published: 2012-07-26
- Granted: 2012-10-02
- Earliest claimed: 2006-06-26
- Assignees: Sabic Innovative Plastics IP B.V.
- Inventors: Kwok Pong Chan; Sarah Elizabeth Genovese; Erik C. Hagberg; David Bruce Hall; John Lester Maxam; Tara J. Mullen; Roy Ray Odle; Albert Santo Stella; James Mitchell White
- Web page: https://patentgrep.com/patent/US8278383B2

## CPC

- C08F 2/44: Polymerisation in the presence of compounding ingredients, e.g. plasticisers, dyestuffs, fillers
- B29B 7/007: {for continuous mixing}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS

## Abstract

A method for preparing a polymer-organoclay composite composition comprises combining a solvent and an unexfoliated organoclay to provide a first mixture, wherein the unexfoliated organoclay comprises alternating inorganic silicate layers and organic layers, and has an initial spacing between the silicate layers; exposing the first mixture to an energized condition of a sufficient intensity and duration to increase the initial spacing of the inorganic silicate layers, to provide a second mixture; contacting the second mixture with a polymer composition so that the polymer composition fills at least one region located between at least one pair of silicate layers, wherein the polymer composition is at least partially soluble in the solvent; and removing at least a portion of the solvent from the second mixture, wherein the inorganic silicate layers remain separated by the polymer after removal of the solvent.

## Claims

### Claim 1

A method for preparing a polymer-organoclay composite comprising:
combining a solvent and an unexfoliated organoclay to form a first mixture, wherein the organoclay comprises alternating inorganic silicate layers and organic layers, and has an initial spacing between the silicate layers, and further wherein the organoclay comprises a quaternary phosphonium or pyridinium cation of formula (2), formula (3), formula (4) or formula (5):
wherein Ar1, Ar2, Ar3 and Ar4 are independently C6-C50 aromatic radicals; “a” is a number from 1 to about 200; “c” is a number from 0 to 3; R1 is independently at each occurrence a halogen atom, a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, or a C2-C20 aromatic radical; and R2 is a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, a C6-C50 aromatic radical, or a polymer chain,
wherein Ar12, Ar13, Ar14 and Ar15 are independently C6-C50 aromatic radicals; and Ar16 is a C6-C200 aromatic radical, or a polymer chain comprising at least one aromatic group,
wherein Ar6, Ar7, and Ar8 are independently C6-C50 aromatic radicals; “b” is a number from 0 to 2; R3 is independently at each occurrence a halogen atom, a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, or a C2-C20 aromatic radical; and Ar11 is a C6-C200 aromatic radical, or a polymer chain comprising at least one aromatic group,
wherein Ar6, Ar7, and Ar8 are independently C6-C50 aromatic radicals; “b” is a number from 0 to 2; “d” is a number from 0 to 4; R3 and R4 are independently at each occurrence a halogen atom, a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, or a C6-C20 aromatic radical; Z is a bond, a divalent C1-C20 aliphatic radical, a divalent C5-C20 cycloaliphatic radical, a divalent C6-C20 aromatic radical, an oxygen linking group, a sulfur linking group, a SO2 linking group, or a Se linking group; and Ar9 is a C10-C200 aromatic radical, or a polymer chain comprising at least one aromatic group;
exposing the first mixture to an energized condition of a sufficient intensity and duration to increase the initial spacing of the inorganic silicate layers, to form a second mixture;
contacting the first or second mixture with a polymer precursor;
polymerizing the polymer precursor to form a polymer, wherein the polymer is located in at least one region located between at least one pair of silicate layers, wherein the polymer is at least partially soluble in the solvent; and
removing at least a portion of the solvent from the second mixture, wherein the inorganic silicate layers remain separated by the polymer after removal of the solvent.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polymerizing occurs at least partly during the exposing.

### Claim 3 (depends on 1)

The method of claim 1, wherein the polymerizing occurs at least partly after the exposing.

### Claim 4 (depends on 1)

The method of claim 1, wherein the polymerizing occurs at least partly during the removal of the solvent.

### Claim 5 (depends on 1)

The method of claim 1, wherein the polymer precursor is a polyamic acid.

### Claim 6 (depends on 1)

The method of claim 1, wherein the polymer precursor comprises a dianhydride component and a diamine component.

### Claim 7 (depends on 1)

The method of claim 1, wherein the energized condition is produced by a sonic energy source.

### Claim 8 (depends on 1)

The method of claim 1, wherein the energized condition is produced by a high shear mixer.

### Claim 9 (depends on 1)

The method of claim 1, wherein the energy is of sufficient intensity and duration to effect a net increase in the initial d-spacing of the organoclay.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first mixture is exposed to an energized condition of sufficient intensity and duration to increase the initial spacing of the inorganic silicate layers by an amount from 5 Angstroms to 90 Angstroms.

### Claim 11 (depends on 1)

The method of claim 1, wherein the increase in the initial spacing of the inorganic silicate layers results in random spacing of the inorganic silicate layers.

### Claim 12 (depends on 1)

The method of claim 1, wherein the net increase in the initial d-spacing of the organoclay is from about 10 to about 500 percent.

### Claim 13

A method for preparing a polymer-organoclay composite comprising:
combining a solvent, an unexfoliated organoclay, a dianhydride component, and a diamine component to form a first mixture, wherein the organoclay comprises alternating inorganic silicate layers and organic layers, and has an initial spacing between the silicate layers, and further wherein the organoclay comprises a quaternary phosphonium or pyridinium cation of formula (2), formula (3), formula (4) or formula (5):
wherein Ar1, Ar2, Ar3 and Ar4 are independently C6-C50 aromatic radicals; “a” is a number from 1 to about 200; “c” is a number from 0 to 3; R1 is independently at each occurrence a halogen atom, a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, or a C2-C20 aromatic radical; and R2 is a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, a C6-C50 aromatic radical, or a polymer chain,
wherein Ar12, Ar13, Ar14 and Ar15 are independently C6-C50 aromatic radicals; and Ar16 is a C6-C200 aromatic radical, or a polymer chain comprising at least one aromatic group,
wherein Ar6, Ar7, and Ar8 are independently C6-C50 aromatic radicals; “b” is a number from 0 to 2; R3 is independently at each occurrence a halogen atom, a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, or a C2-C20 aromatic radical; and Ar11 is a C6-C200 aromatic radical, or a polymer chain comprising at least one aromatic group,
wherein Ar6, Ar7, and Ar8 are independently C6-C50 aromatic radicals; “b” is a number from 0 to 2; “d” is a number from 0 to 4; R3 and R4 are independently at each occurrence a halogen atom, a C1-C20 aliphatic radical, a C5-C20 cycloaliphatic radical, or a C6-C20 aromatic radical; Z is a bond, a divalent C1-C20 aliphatic radical, a divalent C5-C20 cycloaliphatic radical, a divalent C6-C20 aromatic radical, an oxygen linking group, a sulfur linking group, a SO2 linking group, or a Se linking group; and Ar9 is a C10-C200 aromatic radical, or a polymer chain comprising at least one aromatic group;
exposing the first mixture to an energized condition of a sufficient intensity and duration to increase the initial spacing of the inorganic silicate layers, to form a second mixture;
polymerizing the dianhydride component and the diamine component to form a polyamic acid; and
removing at least a portion of the solvent from the polyamic acid mixture to provide a polyimide, wherein the inorganic silicate layers remain separated by the polyimide after removal of the solvent.

### Claim 14 (depends on 13)

The method of claim 13, wherein the polymerizing occurs at least partly during the exposing.

### Claim 15 (depends on 13)

The method of claim 13, wherein the polymerizing occurs at least partly after the exposing.

### Claim 16 (depends on 13)

The method of claim 13, wherein the polymerizing occurs at least partly during the removal of the solvent.

### Claim 17 (depends on 13)

The method of claim 13, wherein the polymer precursor is a polyamic acid.

### Claim 18 (depends on 13)

The method of claim 13, wherein the polymer precursor comprises a dianhydride component and a diamine component.

### Claim 19 (depends on 13)

The method of claim 13, wherein the energized condition is produced by a sonic energy source.

### Claim 20 (depends on 13)

The method of claim 13, wherein the energized condition is produced by a high shear mixer.

### Claim 21 (depends on 13)

The method of claim 13, wherein the energy is of sufficient intensity and duration to effect a net increase in the initial d-spacing of the organoclay.

### Claim 22 (depends on 13)

The method of claim 13, wherein the first mixture is exposed to an energized condition of sufficient intensity and duration to increase the initial spacing of the inorganic silicate layers by an amount from 5 Angstroms to 90 Angstroms.

### Claim 23 (depends on 13)

The method of claim 13, wherein the increase in the initial spacing of the inorganic silicate layers results in random spacing of the inorganic silicate layers.

### Claim 24 (depends on 13)

The method of claim 13, wherein the net increase in the initial d-spacing of the organoclay is from about 10 to about 500 percent.