# US 8,278,382 B2 · Method for preparing a transparent polymer material including mineral nanoparticles with a shape factor strictly higher than 1.0

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,382 B2
- Document ID: US8278382B2
- Status: Granted
- Kind: B2
- Application number: 13/130,677
- Filed: 2009-11-27
- Published: 2011-11-17
- Granted: 2012-10-02
- Earliest claimed: 2008-12-08
- Assignees: RENAULT s.a.s.; Essilor International (Compagnie Generale d'Optique); Solvay SA
- Inventors: Virginie Boucher; Sophie Duquesne; Serge Bourbigot; Didier Sy; Marc Lacroix; Alexandra Roos; Nathalie Cornet; Laure Meynie
- Web page: https://patentgrep.com/patent/US8278382B2

## CPC

- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C08J 3/201: {Pre-melted polymers}
- C08J 5/005: {Reinforced macromolecular compounds with nanosized materials, e.g. nanoparticles, nanofibres, nanotubes, nanowires, nanorods or nanolayered materials}
- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08L 25/04: Homopolymers or copolymers of styrene
- C08L 33/06: of esters containing only carbon, hydrogen and oxygen, which oxygen atoms are present only as part of the carboxyl radical
- C08L 77/00: Compositions of polyamides obtained by reactions forming a carboxylic amide link in the main chain (of polyhydrazides C08L79/06; of polyamideimides or polyamide acids C08L79/08); Compositions of derivatives of such polymers
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The present invention provides a method of preparing a transparent polymer material, the method comprising steps i) and ii) in any order, the steps consisting in: i) mixing: mineral nanoparticles having a form factor strictly greater than 1.0; and a polymer matrix comprising a quantity of at least 80% by weight of a polycarbonate (PC) first thermoplastic polymer and of a second transparent thermoplastic polymer other than the first thermoplastic polymer, in order to obtain a mixture; and ii) heating the polymer matrix to the molten state, on its own or in the mixture; to obtain the transparent, polymer material, the mixture of step i) comprising a quantity of mineral nanoparticles having a form factor strictly greater than 1.0 that is strictly less than 5% by weight.

## Claims

### Claim 1

A method of preparing a transparent polymer material, said method comprising the steps of, in any order:
i) mixing:
mineral nanoparticles having a form factor strictly greater than 1.0; and
a polymer matrix comprising a quantity of at least 80% by weight of a polycarbonate (PC) first thermoplastic polymer and of a second transparent thermoplastic polymer other than the first thermoplastic polymer;
in order to obtain a mixture; and
ii) heating the polymer matrix to the molten state, on its own or in the mixture;
in order to obtain the transparent polymer material, the mixture of step i) comprising a quantity of mineral nanoparticles having a form factor strictly greater than 1.0 that is strictly less than 5% by weight, and step i) not involving mineral nanoparticles in the form of a premixture obtained with a thermoplastic polymer in the molten state selected from the group consisting of polycarbonate (PC), polystyrene (PS), and polymethyl methacrylate (PMMA).

### Claim 2 (depends on 1)

A method according to claim 1, wherein the polymer matrix includes at least 90% by weight of the polycarbonate first thermoplastic polymer.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the form factor is greater than or equal to 2.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the second polymer is selected from the consisting of homopolymers of styrene, of acrylate, and of acrylamide, and a mixture thereof.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the second polymer is selected from the group consisting of copolymers of styrene, of acrylate, of acrylamide, and of polycarbonate monomer, and a mixture thereof.

### Claim 6 (depends on 1)

A method according to claim 1, wherein the mineral nanoparticles having a form factor strictly greater than 1.0 are selected from the group consisting of nanoparticles of carbonates of alkaline earth metals, of phyllosilicates, and of metallic oxides.

### Claim 7 (depends on 1)

A method according to claim 1, wherein the mineral nanoparticles having a form factor strictly greater than 1.0 are selected from the group consisting of nanoparticles of calcium carbonate, of montmorillonite, of alumina, and of boehmite.

### Claim 8 (depends on 1)

A method according to claim 1, wherein the mixture of step i) includes a quantity of at most 2% by weight of mineral nanoparticles having a form factor strictly greater than 1.0.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the mixture of step i) further comprises mineral nanoparticles having a form factor equal to 1.

### Claim 10 (depends on 9)

A method according to claim 9, wherein the mineral nanoparticles having a form factor equal to 1 are selected from the group consisting of nanoparticles of carbonates of alkaline-earth metals, of sulfates of alkaline-earth metals, of metallic oxides, of metalloid oxides, and of siloxanes.

### Claim 11 (depends on 9)

A method according to claim 9, wherein the mixture of step i) comprises a quantity of at most 10% by weight mineral nanoparticles.

### Claim 12 (depends on 1)

A method according to claim 1, wherein the size of the mineral nanoparticles is at most 300 nm.

### Claim 13 (depends on 1)

A method according to claim 1, the mixture of step i) further includes at least one antioxidant.

### Claim 14 (depends on 13)

A method according to claim 13, wherein the mixture of step i) includes a quantity of at most 5% by weight antioxidant.

### Claim 15 (depends on 13)

A method according to claim 13, wherein the antioxidant comprises a phosphite.

### Claim 16 (depends on 2)

A method according to claim 2, wherein the polymer matrix includes at least 95% by weight of the polycarbonate first thermoplastic polymer.

### Claim 17 (depends on 3)

A method according to claim 3, wherein the form factor is greater than or equal to 5.

### Claim 18 (depends on 17)

A method according to claim 17 wherein the form factor is greater than or equal to 10.

### Claim 19 (depends on 18)

A method according to claim 18, wherein the form factor is greater than or equal to 50.

### Claim 20 (depends on 19)

A method according to claim 19, wherein the form factor is greater than or equal to 100.

### Claim 21 (depends on 20)

A method according to claim 20, wherein the form factor is greater than or equal to 200.

### Claim 22 (depends on 8)

A method according to claim 8, wherein the mixture of step i) includes a quantity of at most 1% by weight of mineral nanoparticles having a form factor strictly greater than 1.0.

### Claim 23 (depends on 22)

A method according to claim 22, wherein the mixture of step i) includes a quantity of at most 0.5% by weight of mineral nanoparticles having a form factor strictly greater than 1.0.

### Claim 24 (depends on 12)

A method according to claim 12, wherein the size of the mineral nanoparticles is at most 100 nm.

### Claim 25 (depends on 24)

A method according to claim 24, wherein the size of the mineral nanoparticles is at least 10 nm, and at most 70 nm.

### Claim 26 (depends on 14)

A method according to claim 14, wherein the mixture of step i) includes a quantity of at most 2% by weight antioxidant.