# US 8,278,254 B2 · Additives and lubricant formulations having improved antiwear properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,254 B2
- Document ID: US8278254B2
- Status: Granted
- Kind: B2
- Application number: 11/852,442
- Filed: 2007-09-10
- Published: 2009-03-12
- Granted: 2012-10-02
- Earliest claimed: 2007-09-10
- Assignees: Afton Chemical Corporation
- Inventors: Mark T. Devlin; Kenneth J. Garelick; Naresh C. Mathur; Jeffrey M. Guevremont
- Web page: https://patentgrep.com/patent/US8278254B2

## CPC

- C10M 141/10: at least one of them being an organic phosphorus-containing compound
- C10M 2207/122: monocarboxylic
- C10M 2207/126: monocarboxylic
- C10M 2223/045: Metal containing thio derivatives
- C10N 2030/06: Oiliness; Film-strength; Anti-wear; Resistance to extreme pressure
- C10N 2030/40: {Low content or no content compositions}
- C10N 2030/42: {Phosphor free or low phosphor content compositions}
- C10N 2030/43: {Sulfur free or low sulfur content compositions}
- C10N 2030/70: {Soluble oils}
- C10N 2040/25: Internal-combustion engines
- C10N 2040/252: {Diesel engines}
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS

## Abstract

Lubricated surfaces, lubricant compositions for lubricating a surface, and methods for increasing antiwear properties in lubricants. The lubricated surface is provided by a lubricant composition including a base oil of lubricating viscosity, at least one metal salt of phosphorothioic acid, and an amount of at least one hydrocarbon soluble titanium compound effective to provide an increase in antiwear properties of the lubricant composition. A ratio of titanium metal to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.

## Claims

### Claim 1

A lubricated surface comprising a lubricant composition including a base oil of lubricating viscosity, at least one metal salt of phosphorothioic acid, and an amount of at least one hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, said titanium compounds being effective to provide an increase in antiwear properties of the lubricant composition wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.

### Claim 2 (depends on 1)

The lubricated surface of claim 1, wherein the lubricated surface comprises and engine drive train.

### Claim 3 (depends on 1)

The lubricated surface of claim 1, wherein the lubricated surface comprises an internal surface or component of an engine selected from the group consisting of an internal combustion engine and a compression ignition engine.

### Claim 4 (depends on 1)

The lubricated surface of claim 1, wherein the amount of hydrocarbon soluble titanium compound provides an amount of titanium ranging from about 10 ppm to about 1000 ppm in the lubricant composition.

### Claim 5 (depends on 1)

The lubricated surface of claim 1, wherein the amount of hydrocarbon soluble titanium compound provides an amount of titanium ranging from about 50 ppm to about 800 ppm in the lubricant composition.

### Claim 6 (depends on 1)

The lubricated surface of claim 1, wherein the hydrocarbon soluble titanium compound is substantially devoid of phosphorus and sulfur atoms.

### Claim 7 (depends on 1)

The lubricated surface of claim 1, wherein the carboxylic acid comprises a mono-carboxylic acid containing at least about 6 carbon atoms and having a secondary, or tertiary carbon adjacent to a carboxyl group.

### Claim 8 (depends on 1)

The lubricated surface of claim 1, wherein metal salt of phosphorothioic acid comprises zinc dihydrocarbyl dithiophosphate.

### Claim 9 (depends on 1)

The lubricated surface of claim 1, wherein the lubricant composition comprises from about 200 to about 500 ppm phosphorus.

### Claim 10

A vehicle having moving parts and containing a lubricant for lubricating the moving parts, the lubricant comprising an oil of lubricating viscosity, a friction modifier, and an antiwear agent comprising an amount of at least one hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, and an amount of at least one metal salt of phosphorothioic acid, wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1 and the antiwear agent provides a antiwear film thickness that is greater than a film thickness provided by the titanium compound or phosphorus compound alone.

### Claim 11 (depends on 10)

The vehicle of claim 10, wherein the weight ratio of titanium metal to phosphorus in the antiwear agent ranges from about 0.5:1 to about 1.45:1.

### Claim 12 (depends on 10)

The vehicle of claim 10, wherein the moving parts comprise a heavy duty diesel engine.

### Claim 13 (depends on 10)

The vehicle of claim 10, wherein the lubricant composition comprises from about 100 to about 900 ppm phosphorus.

### Claim 14

A fully formulated lubricant composition comprising a base oil component of lubricating viscosity, and an antiwear agent comprising an amount of hydrocarbon soluble titanium-containing compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, and an amount of at least one metal salt of phosphorothioic acid, wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.

### Claim 15 (depends on 14)

The fully formulated lubricant composition of claim 14, wherein the weight ratio of titanium metal to phosphorus in the antiwear agent ranges from about 0.5:1 to about 1.45:1.

### Claim 16 (depends on 14)

The fully formulated lubricant composition of claim 14, wherein the lubricant composition comprises from about 10 to about 1000 ppm titanium.

### Claim 17 (depends on 14)

The lubricant composition of claim 14 wherein the lubricant composition comprises a low ash, low sulfur, and low phosphorus lubricant composition suitable for compression ignition engines such that the finished oil contains about 0.7 wt % or less sulfur and about 0.1 wt % or less phosphorus.

### Claim 18

A method for increasing an antiwear film thickness adjacent to a lubricated surface, comprising contacting the surface with a lubricant composition comprising a base oil of lubricating viscosity and an amount of an antiwear agent comprising a hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, and a metal salt of phosphorothioic acid, wherein the antiwear agent has a titanium metal to phosphorus ratio by weight that provides a synergistic increase in the antiwear film thickness compared to an antiwear film thickness provided by a lubricant composition containing only one of the titanium compound and the metal salt of phosphorothioic acid.

### Claim 19 (depends on 18)

The method of claim 18, wherein the weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent comprises from about 0.3:1 to about 1.5:1.

### Claim 20 (depends on 18)

The method of claim 18, wherein the lubricant composition further comprises a friction modifier selected from the group consisting essentially of an organomolybdenum friction modifier, a glycerol ester friction modifier, and a mixture thereof.

### Claim 21

An additive concentrate for a lubricant composition comprising an antiwear agent including at least one metal salt of phosphorothioic acid, and an amount of at least one hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, said titanium compounds being effective to provide an increase in antiwear properties of the lubricant composition, wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.

### Claim 22 (depends on 21)

The additive concentrate of claim 21, wherein the amount of hydrocarbon soluble titanium compound provides an amount of titanium ranging from about 50 ppm to about 800 ppm in the lubricant composition.

### Claim 23 (depends on 21)

The additive concentrate of claim 21, wherein an amount of the metal salt of phosphorothioic acid in the additive concentrate is sufficient to provide the lubricant composition with from about 100 to about 900 ppm phosphorus.