# US 8,278,236 B2 · Method for catalytically coating ceramic honeycomb bodies

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,236 B2
- Document ID: US8278236B2
- Status: Granted
- Kind: B2
- Application number: 12/158,843
- Filed: 2006-11-22
- Published: 2009-12-10
- Granted: 2012-10-02
- Earliest claimed: 2005-12-24
- Assignees: Umicore AG & Co. KG
- Inventors: Marcus Pfeifer; Paul Spurk; Markus Koegel; Egbert S. J. Lox; Thomas Kreuzer
- Web page: https://patentgrep.com/patent/US8278236B2

## CPC

- B01J 37/0215: {Coating}
- B01J 35/56: Foraminous structures having flow-through passages or channels, e.g. grids or three-dimensional [3D] monoliths
- B01J 35/57: Honeycombs
- B01J 35/60: characterised by their surface properties or porosity
- C23C 18/02: by thermal decomposition
- C23C 18/08: characterised by the deposition of metallic material
- B01J 35/657: {larger than 1000 nm}
- Y10T 428/24157: Filled honeycomb cells [e.g., solid substance in cavities, etc.]
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a process for coating ceramic honeycomb bodies with a coating suspension containing, in a carrier liquid, catalyst components as solids and/or in dissolved form. The honeycomb bodies have parallel flow channels running through them. The walls of the flow channels generally have an open pore structure. To coat the channel walls and in particular also the interior surfaces of the pores with the coating suspension, it is proposed that the flow channels be temporarily alternately closed and the coating suspension be forced through the open pore structure of the channel walls. The coating is subsequently dried and calcined. To close the flow channels, it is possible to use thermally or chemically decomposable or soluble compositions which are decomposed or dissolved either during calcination or by means of a subsequent chemical treatment. The coated honeycomb bodies are preferably used for the purification of exhaust gases from automobiles.

## Claims

### Claim 1

Process for the catalytic coating of ceramic honeycomb bodies through which parallel flow channels separated from one another by channel walls having a surface and an open pore structure run from an entry end face to an exit end face, in which coating is carried out using a catalyst suspension containing solids suspended in a carrier liquid, characterized in that the flow channels are alternately temporarily closed at the entry and exit end face, the catalyst suspension is allowed to flow through the honeycomb body from the entry face to the exit face so as to completely fill pores of the channel walls with the catalytic coating and reduce the catalytic coating on the surface of the channel walls and the alternately closed flow channels are subsequently opened again.

### Claim 2 (depends on 1)

Process according to claim 1, characterized in that the catalyst suspension is sucked or pumped through the honeycomb body.

### Claim 3 (depends on 1)

Process according to claim 1, characterized in that the honeycomb body is dipped into the catalyst suspension or the catalyst suspension is poured over it.

### Claim 4 (depends on 2)

Process according to claim 2, characterized in that the flow channels are alternately closed by means of a sealing composition which is solid at the customary working temperatures in the coating of honeycomb bodies and melts or vaporizes at elevated temperature, can be dissolved out by means of solvents, can be decomposed thermally or can be reacted chemically.

### Claim 5 (depends on 4)

Process according to claim 4, characterized in that a natural or synthetic wax which has a melting point above 80° C. and burns during calcination of the coated honeycomb body is used as sealing composition.

### Claim 6 (depends on 1)

Process according to claim 1, characterized in that the honeycomb bodies have a porosity in the range from 30 to 90% and an average pore diameter of from 10 to 50 μm.

### Claim 7 (depends on 1)

Process according to claim 1, characterized in that the solids of the suspension have an average particle size d50 in the range from 3 to 5 μm.

### Claim 8 (depends on 1)

Process according to claim 1, characterized in that the solids of the suspension have an average particle size d50 in the range from 1 to 3 μm.

### Claim 9 (depends on 1)

Process according to claim 1, characterized in that the solids of the suspension have an average particle size d50 of less than 1 μm.

### Claim 10 (depends on 4)

Process according to claim 4, characterized in that the sealing composition is melted and burnt.

### Claim 11

Process for the catalytic coating of ceramic honeycomb bodies through which parallel flow channels separated from one another by channel walls having a surface and an open pore structure run from an entry end face to an exit end face, in which coating is carried out using a catalyst suspension containing solids suspended in a carrier liquid, characterized in that the flow channels are alternately temporarily closed at the entry and exit end face, the catalyst suspension is allowed to flow through the honeycomb body from the entry face to the exit face so as to completely fill pores of the channel walls with the catalytic coating and reduce the catalytic coating on the surface of the channel walls and the alternately closed flow channels are subsequently opened again, the flow channels being alternately closed by means of a sealing composition which: (i) is solid at working temperatures in the coating of honeycomb bodies and melts or vaporizes at elevated temperature above the working temperatures; (ii) can be dissolved out by means of solvents; and (iii) can be decomposed thermally or can be reacted chemically.

### Claim 12

Process for the catalytic coating of ceramic honeycomb bodies through which parallel flow channels separated from one another by channel walls having a surface and an open pore structure run from an entry end face to an exit end face, in which coating is carried out using a catalyst suspension containing solids suspended in a carrier liquid, characterized in that the flow channels are alternately temporarily closed at the entry and exit end face, the catalyst suspension is allowed to flow through the honeycomb body from the entry face to the exit face so as to completely fill pores of the channel wall with the catalytic coating and reduce the catalytic coating on the surface of the channel walls and the alternately closed flow channels are subsequently opened again, the honeycomb bodies having a porosity in the range from 30 to 90% and an average pore diameter of from 10 to 50 μm.

### Claim 13

Process for the catalytic coating of ceramic honeycomb bodies through which parallel flow channels separated from one another by channel walls having a surface and an open pore structure run from an entry end face to an exit end face, in which coating is carried out using a catalyst suspension containing solids suspended in a carrier liquid, characterized in that the flow channels are alternately temporarily closed at the entry and exit end face, the catalyst suspension is allowed to flow through the honeycomb body from the entry face to the exit face so as to completely fill pores of the channel walls with the catalytic coating and reduce the catalytic coating on the surface of the channel walls and the alternately closed flow channels are subsequently opened again, the solids of the suspension having an average particle size d50 in the range from 3 to 5 μm.

### Claim 14

Process for the catalytic coating of ceramic honeycomb bodies through which parallel flow channels separated from one another by channel walls having an open pore structure run from an entry end face to an exit end face, in which coating is carried out using a catalyst suspension containing solids suspended in a carrier liquid, characterized in that the flow channels are alternately temporarily closed at the entry and exit end face, the catalyst suspension is allowed to flow through the honeycomb body from the entry face to the exit face so as to completely fill pores of the channel wall with the catalytic coating and reduce the catalytic coating on the surface of the channel walls and the alternately closed flow channels are subsequently opened again, the honeycomb bodies having a porosity in the range from 30 to 90% and an average pore diameter of from 10 to 50 μm and the solids of the suspension having an average particle size d50 in the range from 3 to 5 μm.

### Claim 15

Process for the catalytic coating of ceramic honeycomb bodies through which parallel flow channels separated from one another by channel walls having a surface and an open pore structure run from an entry end face to an exit end face, in which coating is carried out using a catalyst suspension containing solids suspended in a carrier liquid, characterized in that the flow channels are alternately temporarily closed at the entry and exit end face, the catalyst suspension is allowed to flow through the honeycomb body from the entry face to the exit face so as to completely fill pores of the channel wall with the catalytic coating and reduce the catalytic coating on the surface of the channel walls and the alternately closed flow channels are subsequently opened again, the honeycomb bodies having a porosity in the range from 30 to 90% and an average pore diameter of from 10 to 50 μm and the solids of the suspension having an average particle size d50 in the range from 3 to 5 μm, and the flow channels being alternately closed by means of a sealing composition which: (i) is solid at working temperatures in the coating of honeycomb bodies and melts or vaporizes at elevated temperatures above the working temperatures; (ii) can be dissolved out by means of solvents; and (iii) can be decomposed thermally or can be reacted chemically.