# US 8,278,233 B2 · Translucent polycrystalline sintered body, method for producing the same, and arc tube for high-intensity discharge lamp

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,233 B2
- Document ID: US8278233B2
- Status: Granted
- Kind: B2
- Application number: 12/877,299
- Filed: 2010-09-08
- Published: 2011-03-10
- Granted: 2012-10-02
- Earliest claimed: 2009-09-09
- Assignees: NGK Insulators, Ltd.
- Inventors: Sugio Miyazawa; Keiichiro Watanabe; Tsuneaki Ohashi; Hisanori Yamamoto
- Web page: https://patentgrep.com/patent/US8278233B2

## CPC

- H01J 61/302: {characterised by the material of the vessel}
- C04B 35/115: Translucent or transparent products
- C04B 35/6263: {characterised by their solids loadings, i.e. the percentage of solids}
- C04B 35/6264: {Mixing media, e.g. organic solvents}
- C04B 35/6303: {Inorganic additives}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 2235/3201: Alkali metal oxides or oxide-forming salts thereof
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3244: Zirconium oxides, zirconates, hafnium oxides, hafnates, or oxide-forming salts thereof
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/549: the particle size being expressed by crystallite size or primary particle size
- C04B 2235/6023: Gel casting
- C04B 2235/6581: Total pressure below 1 atmosphere, e.g. vacuum
- C04B 2235/6582: Hydrogen containing atmosphere
- C04B 2235/661: Multi-step sintering
- C04B 2235/663: Oxidative annealing
- C04B 2235/784: Monomodal
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/94: Products characterised by their shape
- C04B 2235/95: Products characterised by their size, e.g. microceramics
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B 2235/963: Surface properties, e.g. surface roughness
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A translucent polycrystalline sintered body is mainly composed of an alumina, is suitable for the manufacture of an arc tube for a high-intensity discharge lamp, and has an average grain diameter of 35 to 70 μm, preferably 50 to 60 μm. In a case where the sintered body is in a 0.5-mm-thick flat plate shape, the in-line transmittance of the sintered body is 30% or more, preferably 50% or more. In this case, the ratio between maximum and minimum in-line transmittance values is 2:1 to 1:1 in the visible region of 360 to 830 nm. The bending strength of the sintered body is 250 MPa or more, preferably 300 MPa or more.

## Claims

### Claim 1

A translucent polycrystalline sintered body suitable for the manufacture of an arc tube for a high-intensity discharge lamp, comprising an alumina as a main component, and comprising, as additives, 30 to 200 ppm by weight of MgO, 200 to 1200 ppm by weight of ZrO2 and 5 to 300 ppm by weight of Y2O3, wherein sintered grains forming the translucent polycrystalline sintered body have an average grain diameter of 35 to 70 μm.

### Claim 2 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, wherein a 0.5-mm-thick flat plate of the translucent polycrystalline sintered body has an in-line transmittance of 30% or more of light at a wavelength of 600 nm.

### Claim 3 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, wherein a 0.5-mm-thick flat plate of the translucent polycrystalline sintered body has a ratio of 2:1 to 1:1 between maximum and minimum in-line transmittance values in the visible region of 360 to 830 nm.

### Claim 4 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, wherein the translucent polycrystalline sintered body has a bending strength of 250 MPa or more.

### Claim 5 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, wherein the translucent polycrystalline sintered body has a total light transmittance of 85% or more.

### Claim 6 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, wherein a weight ratio of a total of ZrO2 and Y2O3 to MgO is 1:1 to 50:1.

### Claim 7 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, wherein a weight ratio of Y2O3 to MgO is 1:1 to 1:40.

### Claim 8 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, comprising, as additives, 10 to 50 ppm by weight of SiO2, 10 to 50 ppm by weight of Na2O, and 10 to 50 ppm by weight of K2O.

### Claim 9 (depends on 1)

A translucent polycrystalline sintered body according to claim 1, wherein 40% or less of the sintered grains in the translucent polycrystalline sintered body have a grain diameter equal to or smaller than ½ of the average grain diameter.

### Claim 10 (depends on 9)

A translucent polycrystalline sintered body according to claim 9, wherein 5% or more and 15% or less of the sintered grains in the translucent polycrystalline sintered body have a grain diameter equal to or larger than 3/2 of the average grain diameter.

### Claim 11

A method for producing a translucent polycrystalline sintered body suitable for the manufacture of an arc tube for a high-intensity discharge lamp, the sintered body comprising an alumina as a main component, and comprising, as additives, 30 to 200 ppm by weight of MgO, 200 to 1200 ppm by weight of ZrO2 and 5 to 300 ppm by weight of Y203, wherein the sintered body has an average grain diameter of 35 to 70 μm, the method comprising
a material blending step of mixing a main component and an additive to prepare a mixture,
a compact preparation step of forming the mixture to prepare a compact,
a preliminary firing step of subjecting the compact to a preliminary firing treatment to prepare a sintered body precursor, and
a principal firing step of subjecting the sintered body precursor to a principal firing treatment to produce the translucent polycrystalline sintered body.

### Claim 12 (depends on 11)

A method according to claim 11, wherein the mixture is a slurry containing at least a solvent, a gelling agent, and a ceramic powder containing the main component and the additive, and the slurry is cast into a mold and then hardened to prepare the compact.

### Claim 13 (depends on 11)

A method according to claim 11, wherein an organic binder in the compact is decomposed and removed in an oxidative atmosphere in the preliminary firing step, and the sintered body precursor is fired at a temperature of 1700° C. to 2000° C. in a hydrogen atmosphere or vacuum in the principal firing step.

### Claim 14 (depends on 13)

A method according to claim 13, wherein the principal firing treatment is carried out multiple times in the principal firing step.

### Claim 15 (depends on 13)

A method according to claim 13, wherein the sintered body precursor is fired at a temperature of 1700° C. to 2000° C. for 3 hours or more in the principal firing step.

### Claim 16 (depends on 13)

A method according to claim 13, wherein MgO in the sintered body precursor is partially removed in the principal firing step.

### Claim 17 (depends on 16)

A method according to claim 16, wherein the MgO content in the sintered body precursor is reduced in the principal firing step to ⅔ of an initial MgO content used in the material blending step.

### Claim 18 (depends on 13)

A method according to claim 13, wherein an annealing treatment is carried out in air at a temperature of 1100° C. to 1600° C. after the principal firing treatment.

### Claim 19

An arc tube for a high-intensity discharge lamp, comprising a translucent polycrystalline sintered body comprising an alumina as a main component, and comprising, as additives, 30 to 200 ppm by weight of MgO, 200 to 1200 ppm by weight of ZrO2 and 5 to 300 ppm by weight of Y2O3, wherein the sintered body has an average grain diameter of 35 to 70 μm.

### Claim 20

An arc tube for a high-intensity discharge lamp, comprising a translucent polycrystalline sintered body produced by a method comprising
a material blending step of mixing a main component and an additive to prepare a mixture,
a compact preparation step of forming the mixture to prepare a compact,
a preliminary firing step of subjecting the compact to a preliminary firing treatment to prepare a sintered body precursor, and
a principal firing step of subjecting the sintered body precursor to a principal firing treatment to produce the translucent polycrystalline sintered body,
wherein the sintered body comprises an alumina as a main component, and as additives, 30 to 200 ppm by weight of MgO, 200 to 1200 ppm by weight of ZrO2 and 5 to 300 ppm by weight of Y2O3, wherein the sintered body has an average grain diameter of 35 to 70 μm.