# US 8,278,218 B2 · Electrical conductor line having a multilayer diffusion barrier for use in a semiconductor device and method for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,218 B2
- Document ID: US8278218B2
- Status: Granted
- Kind: B2
- Application number: 13/241,415
- Filed: 2011-09-23
- Published: 2012-01-19
- Granted: 2012-10-02
- Earliest claimed: 2008-07-25
- Assignees: Hynix Semiconductor Inc.
- Inventors: Joon Seok Oh; Seung Jin Yeom; Baek Mann Kim; Dong Ha Jung; Jeong Tae Kim; Nam Yeal Lee; Jae Hong Kim
- Web page: https://patentgrep.com/patent/US8278218B2

## CPC

- H10W 20/035: {combinations of barrier, adhesion or liner layers, e.g. multi-layered barrier layers}
- H10W 20/048: {by using plasmas or gaseous environments, e.g. by nitriding}
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An electrical conductor having a multilayer diffusion barrier of use in a resultant semiconductor device is presented. The electrical conductor line includes an insulation layer, a diffusion barrier, and a metal line. The insulation layer is formed on a semiconductor substrate and having a metal line forming region. The diffusion barrier is formed on a surface of the metal line forming region of the insulation layer and has a multi-layered structure made of TaN layer, an MoxOy layer and an Mo layer. The metal line is formed on the diffusion barrier to fill the metal line forming region of the insulation layer.

## Claims

### Claim 1

A method for forming a electrical conductor line of a semiconductor device, comprising the steps of:
forming a metal line forming region in an insulation layer on a semiconductor substrate;
forming a multi-layered diffusion barrier on the metal line forming region of the insulation layer, the diffusion barrier comprising a TaN layer, an MoxOy layer and a second Mo layer, wherein the step of forming the diffusion barrier comprises the steps of:
forming the TaN layer on the metal line forming region of the insulation layer;
depositing a first Mo layer on the TaN layer;
forming an MoxOy layer by oxidating the first Mo layer; and
depositing the second Mo layer on the MoxOy layer wherein the diffusion barrier is multi-layered having the TaN layer, the MoxOy layer and the second Mo layer; and
forming a metal line on the diffusion barrier to substantially fill in the metal line forming region.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the TaN layer has a thickness of about 5˜50 Å.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the first Mo layer has a thickness of about 5˜25 Å.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the step of forming the MoxOy layer by oxidating the first Mo layer is implemented by utilizing a O2 plasma process or by utilizing O2 stuffing procedure.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the O2 plasma process uses O2 gas and Ar gas with a composition ratio of O2 gas to Ar gas at about 0.1˜0.9.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the O2 plasma is process is conducted at a temperature of about 25˜250° C. at a pressure of about 1˜760 mTorr.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the O2 stuffing procedure uses O2 gas and Ar gas at a composition ratio of O2 gas to Ar gas at about 0.1˜0.9.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the O2 stuffing procedure is conducted at a temperature of about 50˜400° C. at a pressure of about 1˜760 mTorr.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the MoxOy layer has a thickness of about 5˜50 Å.

### Claim 10 (depends on 1)

The method according to claim 1, wherein, in the MoxOy layer, x has a range of about 0.1˜5 and y has a range of about 0.1˜5.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the second In Mo layer is deposited through Physical Vapor Deposition (PVD).

### Claim 12 (depends on 1)

The method according to claim 1, wherein the second Mo layer is deposited at a temperature of between about −25˜25° C.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the second Mo layer has a thickness of between about 100˜400 Å.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the metal layer comprises a copper layer.