# US 8,278,211 B2 · Thin film forming method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,211 B2
- Document ID: US8278211B2
- Status: Granted
- Kind: B2
- Application number: 13/004,263
- Filed: 2011-01-11
- Published: 2011-07-07
- Granted: 2012-10-02
- Earliest claimed: 2008-07-11
- Assignees: Canon Anelva Corporation
- Inventors: Hanako Hirayama; Eisaku Watanabe
- Web page: https://patentgrep.com/patent/US8278211B2

## CPC

- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/046: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 14/542: {Controlling the film thickness or evaporation rate}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

According to the present invention, a thin film having a desired thickness is formed on an inner sidewall of a step with excellent step coverage in a film forming step and an etching step at least once, respectively. In an embodiment of the present invention, a target material is deposited on a substrate (17) having a concave step (31, 32) having an opening width or opening diameter of 3 μm or less and an aspect ratio of 1 or more. At this time, a film forming method according to the present invention has a first step of depositing a thin film onto a bottom (33) of the step (31, 32) and a second step of forming a film on an inner sidewall (34) of the step (31, 32) by re-sputtering the thin film deposited on the bottom (33) and the pressure in a process chamber in the second step is set lower than that in the process chamber in the first step and the ratio of anode power to cathode power in the second step is set greater than the power ratio in the first step.

## Claims

### Claim 1

A thin film forming method in which a process chamber including a first electrode for supporting a substrate; a second electrode disposed so as to face the substrate for supporting a target; and a plurality of magnets arranged on a surface facing a surface that supports the target of the second electrode wherein the magnets are arranged in positions corresponding to the respective corners of a plurality of rectangles linked in a checkered pattern and the polarities of the magnets neighboring in a direction of the side of the respective rectangles are opposite to each other, is used to deposit a target material onto a substrate having a concave step, wherein
the magnets form a line of magnetic flux closed so as to form a loop in space near the surface that supports the target of the second electrode to form a point-cusp field, and
different high frequency powers are applied to the first and second electrodes, respectively, from high frequency power sources to generate plasma under the second electrode,
the method comprising:
a first step of depositing a thin film on a bottom of the step; and
a second step of forming a film on an inner sidewall of the step by re-sputtering the thin film deposited on the bottom of the step, wherein
the first step selects and sets a pressure in the process chamber in a range from 2 Pa to 27 Pa, sets a ratio of the power supplied to the first electrode to the power supplied to the second electrode to 0.5 or less, sets the frequency of the high frequency power source supplied to the second electrode to a range from 10 MHz to 300 MHz, and thereby generates high-density plasma under the second electrode to deposit a thin film on the bottom of the step, and
the second step sets the power supplied to the second electrode lower than that of the first step selects and sets a pressure in the process chamber in a range from 0.2 Pa to 2 Pa, sets a ratio of the power supplied to the first electrode to the power supplied to the second electrode to 1 or more, and thereby generates low-density plasma under the second electrode and re-sputters the thin film deposited on the bottom of the step to form a film on the inner sidewall of the step.

### Claim 2 (depends on 1)

A thin film forming method according to claim 1, wherein a ratio of the minimum film thickness on the inner sidewall to the film thickness on the bottom of the step is 0.5 or less.

### Claim 3 (depends on 1)

A thin film forming method according to claim 1, wherein the high frequency power of the high frequency power source supplied to the second electrode is selected and set in a range from 300 W to 10,000 W and the high frequency power of the high frequency power source supplied to the first electrode is selected and set in a range from 0 W to 2,000 W.

### Claim 4 (depends on 1)

A thin film forming method according to claim 1, wherein the first step and the second step are performed in this order at least once, respectively, when forming a film within the step.

### Claim 5 (depends on 1)

A thin film forming method according to claim 1, wherein the second electrode is configured by a material of a single composition or compound compositions having conductivity.

### Claim 6 (depends on 1)

A thin film forming method according to claim 1, wherein the process gas is a gas containing at least a noble gas.

### Claim 7 (depends on 6)

A thin film forming method according to claim 6, wherein the process gas is a mixed gas of a noble gas and a reactive gas and the reactive gas is at least one kind of gas selected from a gas group consisting of oxygen and nitrogen.

### Claim 8 (depends on 6)

A thin film forming method according to claim 6, wherein different process gases are used in the first step and the second step.

### Claim 9 (depends on 1)

A thin film forming method according to claim 1, wherein the high frequency power of the high frequency power source supplied to the second electrode is selected and set in a range from 300 W to 10,000 W and the high frequency power of the high frequency power source supplied to the first electrode is set to 0 W.