# US 8,278,210 B2 · Manufacturing method of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,210 B2
- Document ID: US8278210B2
- Status: Granted
- Kind: B2
- Application number: 12/718,175
- Filed: 2010-03-05
- Published: 2010-10-07
- Granted: 2012-10-02
- Earliest claimed: 2009-04-07
- Assignees: Renesas Electronics Corporation
- Inventors: Tatsuhiko Miura
- Web page: https://patentgrep.com/patent/US8278210B2

## CPC

- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 12/038: {having a recessed gate, e.g. trench-gate IGBTs}
- H10D 12/481: {having gate structures on slanted surfaces, on vertical surfaces, or in grooves, e.g. trench gate IGBTs}
- H10D 30/0295: {using recessing of the source electrodes}
- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10P 14/44: Physical vapour deposition [PVD]
- H10W 20/033: {in openings in dielectrics}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10D 64/2527: {for vertical devices wherein the source or drain electrodes are recessed in semiconductor bodies}
- H10D 64/256: {for lateral devices wherein the source or drain electrodes are recessed in semiconductor bodies (source or drain electrodes of TFTs H10D30/673)}
- H10W 20/085: {involving intermediate temporary filling with material}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In a modern 0.15 μm power MOSFET, aluminum voids (voids formed in an aluminum-type electrode) are generated frequently in trench portions (source contact trenches) caused by the reduction of a cell pitch for refinement. It is considered to be attributable to the defects which are generated mainly due to a sudden increase of the aspect ratio from 0.84 in the previous generation to 2.8 in the current generation. Accordingly, concave portions of repetitive trenches having a high aspect ratio are filled with an aluminum-type metal by ionized sputtering throughout the processing, from the formation to the filling of an aluminum-type metal seed film.

## Claims

### Claim 1

A manufacturing method of a semiconductor device comprising the steps of:
(a) forming downward a concave portion from an upper surface of a first insulator film over a first main surface of a semiconductor wafer;
(b) forming a barrier metal film to an inner surface of the concave portion and the upper surface of the first insulator film; and
(c) after the step (b), forming an aluminum-type metal layer so as to fill the inside of the concave portion and cover the upper surface of the first insulator film in a sputter processing chamber by ionized sputtering;
wherein the step (c) is conducted in a state of directing upward the first main surface of the semiconductor wafer to a wafer stage having an electrostatic chuck disposed in the sputter processing chamber,
wherein the step (c) includes the sub-steps of:
(c1) forming a seed aluminum-type metal layer so as to cover the barrier metal film at the inner surface of the concave portion and at the upper surface of the first insulator film; and
(c2) continuing the ionized sputtering thereby forming the aluminum-type metal layer to fill the inside of the concave portion and cover the upper surface of the first insulator film, and being integrated with the seed aluminum-type metal layer, and
wherein the electrostatic chuck is in an off state in the sub-step (c1) and the electrostatic chuck is in an on state in the sub-step (c2),
wherein a bias is applied by a second high frequency power for the electrode on the side of the wafer stage in the sub-step (c1), and
wherein a bias is not applied for the electrode on the side of the wafer stage in the sub-step (c2).

### Claim 2 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1, wherein the temperature of the wafer stage is 400° C. or higher and lower than 440° C.

### Claim 3 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1, wherein the sputter processing chamber is a magnetron type.

### Claim 4 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1, wherein a first high frequency power and a DC bias are applied on the side of the target in the step (c).

### Claim 5 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1, wherein the semiconductor device has a power MOSFET or IGBT.

### Claim 6 (depends on 5)

The manufacturing method of a semiconductor device according to claim 5, wherein the aluminum-type metal layer is the source electrode of the power MOSFET or the emitter electrode of the IGBT.

### Claim 7 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1, wherein the aspect ratio of the concave portion is 2 or more.

### Claim 8 (depends on 1)