# US 8,278,209 B2 · Method for manufacturing a semiconductor device using a hardmask layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,209 B2
- Document ID: US8278209B2
- Status: Granted
- Kind: B2
- Application number: 12/536,391
- Filed: 2009-08-05
- Published: 2010-02-11
- Granted: 2012-10-02
- Earliest claimed: 2008-08-08
- Assignees: Dongbu HiTek Co., Ltd.
- Inventors: Chung-Kyung Jung
- Web page: https://patentgrep.com/patent/US8278209B2

## CPC

- H10F 39/811: {Interconnections}
- H10F 39/018: {of hybrid image sensors}
- H10F 39/809: {of hybrid image sensors}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

A semiconductor device and a method for manufacturing the device include connecting a second wafer to a first wafer, forming a hard mask layer on and/or over a backside of the second wafer, forming a hard mask pattern over the second layer and then forming a via hole by etching the first and the second wafers to a predetermined depth using the hard mask pattern as an etching mask.

## Claims

### Claim 1

A method for manufacturing a semiconductor device comprising:
connecting a second wafer to a first wafer; and then
forming a hard mask layer over an exposed surface of the second wafer; and then
forming a photoresist pattern at an exposed surface of the hard mask layer to expose a via hole region; and then
forming a hard mask pattern by etching the hard mask layer using the photoresist pattern as an etching mask; and then
forming a via hole by etching the first wafer and the second wafer to a predetermined depth using the hard mask pattern as an etching mask.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the hard mask layer comprises:
forming a first oxide layer over an exposed surface of the second wafer; and then
forming a nitride layer over an exposed surface of the first oxide layer; and then
forming a second oxide layer over an exposed surface of the nitride layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second wafer comprises a photodiode formed by H2 ion implantation.

### Claim 4 (depends on 1)

The method of claim 1, further comprising, after forming the via hole:
performing two separate cleaning processes to remove residues remaining in the via hole.

### Claim 5 (depends on 4)

The method of claim 4, wherein performing two separate cleaning processes comprises:
performing a first cleaning process using a solvent; and then
performing a second cleaning process using hot deionized water after performing the first cleaning process.

### Claim 6 (depends on 5)

The method of claim 5, wherein the solvent includes a NH4F-based solvent.

### Claim 7 (depends on 5)

The method of claim 5, wherein the temperature of the hot deionized water is in a range of about 79 to 90° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second wafer comprises a PIN diode.

### Claim 9 (depends on 1)

The method of claim 1, wherein the first wafer comprises a dielectric layer that is composed of at least one of un-doped silicate glass, phosphor silicate glass and boro-phospho silicate glass.

### Claim 10

A method for manufacturing a semiconductor device comprising:
connecting a photodiode to an exposed surface of a first dielectric layer having a via contact and a first metal layer embedded in the first dielectric layer and connected to the via contact; and then
forming a second dielectric layer over an exposed surface of the photodiode; and then
forming a via hole extending through the second dielectric layer and the photodiode and partially through the first dielectric layer to expose the first metal layer by performing an etching process using the second dielectric layer as a hard mask; and then
performing a first cleaning process to remove residues from the via hole; and then
performing a second cleaning process to remove any residues remaining in the via hole after performing the first cleaning process; and then
forming a barrier metal layer over the second dielectric layer and sidewalls of the via hole; and then
forming a second metal layer over the barrier metal layer and filling the via hole; and then
selectively removing portions of the barrier metal layer and the second metal layer to expose portions of the via hole.

### Claim 11 (depends on 10)

The method of claim 10, wherein the photodiode comprises a PIN diode.

### Claim 12 (depends on 11)

The method of claim 11, wherein selectively removing portions of the barrier metal layer and the second metal layer comprises selectively removing portions of the barrier metal layer and the second metal layer up to an I layer of the PIN diode.

### Claim 13 (depends on 11)

The method of claim 11, wherein selectively removing portions of the barrier metal layer and the second metal layer comprises performing a wet etching using a resultant material obtained by diluting a compound of H2SO4, Trimethyl Oxyethyl Ammonium-hydroxide (TMH) and H2O2 in hot deionized water.

### Claim 14 (depends on 10)

The method of claim 10, wherein the first dielectric layer comprises at least one of un-doped silicate glass, phosphor silicate glass and boro-phospho silicate glass.

### Claim 15 (depends on 10)

The method of claim 10, wherein the second dielectric layer comprises an Oxide-Nitride-Oxide structure including a first oxide layer, a nitride layer and a second oxide layer.