# US 8,278,199 B2 · Method of manufacturing a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,199 B2
- Document ID: US8278199B2
- Status: Granted
- Kind: B2
- Application number: 13/242,000
- Filed: 2011-09-23
- Published: 2012-03-29
- Granted: 2012-10-02
- Earliest claimed: 2008-01-25
- Assignees: Renesas Electronics Corporation
- Inventors: Shigenari Okada; Takuya Futase; Yutaka Inaba
- Web page: https://patentgrep.com/patent/US8278199B2

## CPC

- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10P 72/0461: {characterised by the presence of two or more transfer chambers}
- H10P 72/0468: {comprising a chamber adapted to a particular process}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 84/0174: {the gate conductors being silicided}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Reliability of a semiconductor element and its product yield are improved by reducing variations in the electrical characteristic of a metal silicide layer. After forming a nickel-platinum alloy film over a semiconductor substrate, by carrying out a first thermal treatment at a thermal treatment temperature of 210 to 310° C. using a heater heating device, the technique causes the nickel-platinum alloy film and silicon to react with each other to form a platinum-added nickel silicide layer in a (PtNi)2Si phase. After removing unreacted nickel-platinum alloy film, the technique carries out a second thermal treatment having the thermal treatment temperature higher than that of the first thermal treatment to form the platinum-added nickel silicide layer in a PtNiSi phase. The temperature rise rate of each thermal treatment is set to 10° C./s or more.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising the steps of:
(a) preparing a semiconductor substrate made of single crystal silicon;
(b) forming a semiconductor region over the semiconductor substrate;
(c) forming an alloy film of nickel and platinum over the semiconductor substrate including the semiconductor region;
(d) forming a platinum-added nickel silicide layer, in a PtNiSi phase by carrying out a first thermal treatment to cause the alloy film and the semiconductor region to react with each other;
(e) after the step (d), removing the unreacted alloy film over the platinum-added nickel silicide layer in the PtNiSi phase over the semiconductor region; and
(f) after the step (e), carrying out a second thermal treatment with the thermal treatment temperature higher than that of the first thermal treatment,
wherein a temperature rise rate of the first thermal treatment in step (d) is 30 to 250° C./s,
wherein a temperature rise rate of the second thermal treatment in step (f) is 10° C./s or more
wherein a heater heating method is used for the first thermal treatment in step (d), and
wherein the second thermal treatment in step (f) is a spike anneal process.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the temperature of the first thermal treatment in the step (d) is 380 to 400° C.

### Claim 3 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein a composition of the platinum-added nickel silicide layer in the PtNiSi phase after the second thermal treatment in the step (f) is closer to a stoichiometric composition than the composition of the platinum-added nickel silicide layer in the PtNiSi phase after the first thermal treatment in the step (d).

### Claim 4 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the temperature rise rate of the second thermal treatment in the step (f) is 10 to 250° C./s.

### Claim 5 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the thermal treatment temperature of the second thermal treatment in the step (f) is 380 to 525° C.

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein a heater heating method is used for the first thermal treatment in the step (d).

### Claim 7 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein a heater heating method or a lamp heating method is used for the second thermal treatment in the step (f).

### Claim 8 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7,
wherein the second thermal treatment in the step (f) is carried out in an inert gas having the thermal conductivity higher than that of a nitrogen gas or in a gas atmosphere that is the nitrogen gas added with a gas having the thermal conductivity higher than that of the nitrogen gas.

### Claim 9 (depends on 8)

The method of manufacturing a semiconductor device according to claim 8,
wherein the inert gas is helium or neon.

### Claim 10 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the semiconductor region is a semiconductor region for a source or drain.

### Claim 11 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10, further comprising the steps of:
(a1) after the step (a), forming a gate insulating film over the semiconductor substrate; and
(a2) forming a gate electrode made of polycrystalline silicon over the gate insulating film,
wherein, in the step (c), the alloy film is formed over the semiconductor substrate including the semiconductor region so as to cover the gate electrode.

### Claim 12 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, further comprising the step of:
(c1) after the step (c) and before the step (d), forming a barrier film over the alloy film,
wherein, in the step (e), the barrier film and the unreacted alloy film are removed.

### Claim 13 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, further comprising the step of:
(c2) before the step (c), dry-cleaning a surface of the semiconductor region in a main surface of the semiconductor substrate,
wherein, after the step (c2), the step (c) is carried out without exposing the semiconductor substrate to air.