# US 8,278,196 B2 · High surface dopant concentration semiconductor device and method of fabricating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,196 B2
- Document ID: US8278196B2
- Status: Granted
- Kind: B2
- Application number: 12/840,830
- Filed: 2010-07-21
- Published: 2012-01-26
- Granted: 2012-10-02
- Earliest claimed: 2010-07-21
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Yu-Lien Huang; Mao-Rong Yeh; Chun Hsiung Tsai; Tsung-Hung Lee; Da-Wen Lin; Tsz-Mei Kwok
- Web page: https://patentgrep.com/patent/US8278196B2

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10P 32/1204: {from a plasma phase}
- H10D 30/0275: {forming single crystalline semiconductor source or drain regions resulting in recessed gates, e.g. forming raised source or drain regions}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present disclosure provides a high surface dopant concentration semiconductor device and method of fabricating. In an embodiment, a method of forming the semiconductor device includes providing a substrate, forming a doped region in the substrate, forming a stressing layer over the doped region, performing a boron (B) doping implant to the stressing layer, annealing the B doping implant, and after annealing the B doping implant, forming a silicide layer over the stressing layer.

## Claims

### Claim 1

A method of forming a semiconductor device, the method comprising:
providing a substrate;
forming a doped region in the substrate;
forming a stressing layer over the doped region;
performing a boron (B) doping implant to the stressing layer;
annealing the B doping implant; and
after annealing the B doping implant, forming a silicide layer over the stressing layer.

### Claim 2 (depends on 1)

The method of claim 1, forming the stressing layer using silicon germanium (SiGe).

### Claim 3 (depends on 1)

The method of claim 1, forming the silicide layer using nickel silicide (NiSix).

### Claim 4 (depends on 1)

The method of claim 1, performing the boron doping implant as a plasma implant process.

### Claim 5 (depends on 4)

The method of claim 4, performing the plasma implant process using a precursor gas comprising B2H6 and a dilution gas comprising H2, Ar, He, and combinations thereof.

### Claim 6 (depends on 5)

The method of claim 5, performing the plasma implant process using the gas comprising B2H6 and H2 in a proportion range of approximately 5%-10% B2H6 and approximately 90%-95% H2.

### Claim 7 (depends on 1)

The method of claim 1, performing the annealing as a rapid thermal annealing (RTA) process at a temperature range of approximately 900 C-1010 C.

### Claim 8

A method of for increasing surface dopant concentration in a semiconductor device, the method comprising:
providing a substrate;
forming a dummy gate structure on the substrate, wherein the dummy gate structure includes a dummy gate;
forming a doped region in the substrate, wherein a first portion of the doped region is below a portion of the dummy gate structure and a second portion of the doped region is not below the portion of the dummy gate structure;
forming a stressing layer over the doped region;
performing a boron (B) doping implant to the stressing layer;
annealing the B doping implant;
after annealing the B doping implant, forming a silicide layer over the stressing layer; and
replacing the dummy gate with a metal gate.

### Claim 9 (depends on 8)

The method of claim 8, forming the stressing layer using silicon germanium (SiGe), wherein the doped region is a source or a drain region.

### Claim 10 (depends on 8)

The method of claim 8, forming the silicide layer as a contact device using nickel silicide (NiSix).

### Claim 11 (depends on 8)

The method of claim 8, performing the boron doping implant as a plasma implant process having a source RF of approximately 2 MHz and a pulsed DC bias having a pulse frequency in a range of approximately 0.5 KHz-10 KHz.

### Claim 12 (depends on 11)

The method of claim 11, performing the plasma implant process using a precursor gas comprising B2H6 and a dilution gas comprising H2, Ar, He, and combinations thereof at a pressure range of approximately 6 mtorr to 200 mtorr.

### Claim 13 (depends on 12)

The method of claim 12, performing the plasma implant process using the gas comprising B2H6 and H2 in a proportion range of approximately 5%-10% B2H6 and approximately 90%-95% H2.

### Claim 14 (depends on 8)

The method of claim 8, performing the annealing as a rapid thermal annealing (RTA) process.