# US 8,278,189 B2 · Method for thinning wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,189 B2
- Document ID: US8278189B2
- Status: Granted
- Kind: B2
- Application number: 12/874,231
- Filed: 2010-09-02
- Published: 2012-03-08
- Granted: 2012-10-02
- Earliest claimed: 2010-09-02
- Assignees: United Microelectronics Corp.
- Inventors: Cheng-Yu Hsieh
- Web page: https://patentgrep.com/patent/US8278189B2

## CPC

- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- H10P 72/74: {using temporarily an auxiliary support}
- H10P 72/7416: {used during dicing or grinding}
- H10P 72/7422: {used to protect an active side of a device or wafer}
- H10P 72/7438: {with parts of the auxiliary support remaining in the finished device}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a method of thinning a wafer. First, a wafer is provided. The wafer includes an active surface, a back surface and a side surface. The active surface is disposed opposite to the back surface. The side surface is disposed between the active surface and the back surface and encompasses the peripheral of the wafer. Next, a protective structure is formed on the wafer to at least completely cover the side surface. Last, a thinning process is performed upon the wafer from the back surface.

## Claims

### Claim 1

A method for thinning a wafer, comprising:
providing a wafer comprising an active surface, a back surface disposed opposite to the active surface, and a side surface disposed between and directly adjacent to the active surface and the back surface, wherein the side surface encompasses the peripheral of the wafer;
forming a protective structure on the wafer, wherein the protective structure at least completely covers and directly contacts the side surface;
performing a thinning process upon the wafer from the back surface; and
completely removing the protective structure.

### Claim 2 (depends on 1)

The method for thinning a wafer of claim 1, wherein the protective structure only covers the side surface of the wafer.

### Claim 3 (depends on 1)

The method for thinning a wafer of claim 1, wherein the protective structure further covers the active surface of the wafer.

### Claim 4 (depends on 1)

The method for thinning a wafer of claim 1, wherein the protective structure further covers the back surface of the wafer.

### Claim 5 (depends on 1)

The method for thinning a wafer of claim 1, wherein the protective structure comprise a protective side surface and a protective front surface, wherein the protective side surface is corresponding to the side surface, the protective front surface is corresponding and substantially parallel to the active surface.

### Claim 6 (depends on 5)

The method for thinning a wafer of claim 5, wherein a first angle is disposed between the active surface and the side surface, a second angle is disposed between the protective front surface and the protective side surface, wherein the first angle is greater than the second angle.

### Claim 7 (depends on 6)

The method for thinning a wafer of claim 6, wherein the second angle is substantially 90 degrees.

### Claim 8 (depends on 1)

The method for thinning a wafer of claim 1, wherein during the thinning process, there is no step structure between the active surface and the side surface.

### Claim 9 (depends on 1)

The method for thinning a wafer of claim 1, further comprising:
providing a carrier comprising a carrier front surface, a carrier back surface disposed opposite to the carrier front surface, and a carrier side surface disposed between the carrier front surface and the carrier back surface, wherein the carrier side surface encompasses the peripheral of the carrier and the carrier front surface is attached onto the active surface of the wafer; and
when forming the protective structure, simultaneously forming the protective structure on the carrier side surface.

### Claim 10 (depends on 9)

The method for thinning a wafer of claim 9, wherein the protective structure comprises a protective side surface and a protective front surface, wherein the protective side surface is corresponding to the side surface and the carrier side surface, the protective front surface is corresponding and substantially parallel to the back surface.

### Claim 11 (depends on 10)

The method for thinning a wafer of claim 10, wherein a third angle is disposed between the back surface and the side surface, a fourth angle is disposed between the protective front surface and the protective side surface, wherein the third angle is greater than the fourth angle.

### Claim 12 (depends on 11)

The method for thinning a wafer of claim 11, wherein the fourth angle is substantially 90 degrees.

### Claim 13 (depends on 9)

The method for thinning a wafer of claim 9, wherein the carrier is another wafer.

### Claim 14 (depends on 1)

The method for thinning a wafer of claim 1, wherein the step of forming the protective structure comprises forming a resin on the side surface of the wafer.

### Claim 15 (depends on 14)

The method for thinning a wafer of claim 14, wherein the resin includes epoxy resin.

### Claim 16 (depends on 14)

The method for thinning a wafer of claim 14, further comprising adding a plurality of particles into the resin, wherein the hardness of the particles is greater than that of the resin.

### Claim 17 (depends on 16)

The method for thinning a wafer of claim 16, wherein the particles comprise aluminum oxide, aluminum nitride, silicon oxide or silicon nitride.

### Claim 18 (depends on 14)

The method for thinning a wafer of claim 14, further comprising solidifying the resin to form the protective structure.

### Claim 19 (depends on 18)

The method for thinning a wafer of claim 18, wherein the step of solidifying the resin comprises using a thermal treatment or a radiance treatment with light energy.

### Claim 20

A method for thinning a wafer, comprising:
providing a wafer comprising an active surface, a back surface disposed opposite to the active surface, and a side surface disposed between the active surface and the back surface, wherein the side surface encompasses the peripheral of the wafer;
forming a protective structure on the wafer, wherein the protective structure only covers the side surface and the side surface is completely covered by the protective structure; and
performing a thinning process upon the wafer from the back surface.