# US 8,278,187 B2 · Method for reprocessing semiconductor substrate by stepwise etching with at least two etching treatments

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,187 B2
- Document ID: US8278187B2
- Status: Granted
- Kind: B2
- Application number: 12/797,650
- Filed: 2010-06-10
- Published: 2010-12-30
- Granted: 2012-10-02
- Earliest claimed: 2009-06-24
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Kazuya Hanaoka
- Web page: https://patentgrep.com/patent/US8278187B2

## CPC

- H10P 90/1916: {with separation or delamination along an ion implanted layer, e.g. Smart-cut}
- H10P 90/16: {by reclaiming or re-processing}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed is a method for reprocessing a semiconductor substrate which is by-produced in manufacturing a silicon-on-insulator substrate. The method includes: forming an embrittlement layer in a single crystal semiconductor substrate; bonding the single crystal semiconductor substrate with a base substrate having an insulating surface; and separating the single crystal semiconductor substrate along the embrittlement layer to give a silicon-on-insulator substrate and a semiconductor substrate to be reprocessed. The above steps provide, in the peripheral portion on the semiconductor substrate, a projection comprising the embrittlement layer and a single crystal semiconductor layer over the embrittlement layer. The method is characterized by an etching step to selectively remove the projection without etching a portion where the projection is absent, which allows the semiconductor substrate to be reused for the production of another silicon-on-insulator substrate.

## Claims

### Claim 1

A method for manufacturing a single crystal semiconductor film, the method comprising:
oxidizing a surface of a single crystal semiconductor substrate to form an insulating film over the single crystal semiconductor substrate;
irradiating the single crystal semiconductor substrate with ion beam through the insulating film;
bonding the single crystal semiconductor substrate with a base substrate having an insulating surface;
separating the single crystal semiconductor substrate from the base substrate to allow a thin film of the single crystal semiconductor substrate and the insulating film to be left on the base substrate;
performing a first etching treatment on a remaining single crystal semiconductor substrate, which is separated from the base substrate in the separation step, with a first etchant containing hydrofluoric acid, ammonium fluoride, and a surfactant; and then
performing a second etching treatment on the remaining single crystal semiconductor substrate with a second etchant containing hydrofluoric acid, nitric acid, and acetic acid.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein the second etchant has a composition which is obtained by adjusting a volume of 70 wt % nitric acid to more than or equal to 0.2 times and less than or equal to 0.5 times as large as a volume of 97.7 wt % acetic acid and to more than or equal to one time and less than or equal to 10 times as large as a volume of 50 wt % hydrofluoric acid and further adjusting the volume of 50 wt % hydrofluoric acid to more than or equal to 0.1 times and less than or equal to 0.2 times as large as the volume of 97.7 wt % acetic acid.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein the insulating film contains a halogen element.

### Claim 4 (depends on 1)

The method according to claim 1,
wherein the insulating film contains chlorine.

### Claim 5 (depends on 1)

The method according to claim 1,
wherein the bonding of the single crystal semiconductor substrate with the base substrate is performed at a pressure lower than an atmospheric pressure.

### Claim 6 (depends on 1)

The method according to claim 1, further comprising a step of polishing the remaining single crystal semiconductor substrate after the second etching treatment.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the base substrate is a glass substrate.

### Claim 8

A method for manufacturing a single crystal semiconductor film, the method comprising:
oxidizing a surface of a single crystal semiconductor substrate to form an insulating film over the single crystal semiconductor substrate;
irradiating the single crystal semiconductor substrate with ion beam through the insulating film;
bonding the single crystal semiconductor substrate with a base substrate having an insulating surface;
separating the single crystal semiconductor substrate from the base substrate to allow a thin film of the single crystal semiconductor substrate and the insulating film to be left on the base substrate;
performing a first etching treatment on a remaining single crystal semiconductor substrate, which is separated from the base substrate in the separation step, with a first etchant containing hydrofluoric acid, ammonium fluoride, and a surfactant; and then
performing a second etching treatment on the remaining single crystal semiconductor substrate with a second etchant which is prepared by mixing the first etchant, nitric acid, and acetic acid.

### Claim 9 (depends on 8)

The method according to claim 8,
wherein the second etchant has a composition which is obtained by adjusting a volume of 70 wt % nitric acid to more than or equal to 0.2 times and less than or equal to 0.5 times as large as a volume of 97.7 wt % acetic acid and to more than or equal to one time and less than or equal to 10 times as large as a volume of 50 wt % hydrofluoric acid and further adjusting the volume of 50 wt % hydrofluoric acid to more than or equal to 0.1 times and less than or equal to 0.2 times as large as the volume of 97.7 wt % acetic acid.

### Claim 10 (depends on 8)

The method according to claim 8,
wherein the insulating film contains a halogen element.

### Claim 11 (depends on 8)

The method according to claim 8,
wherein the insulating film contains chlorine.

### Claim 12 (depends on 8)

The method according to claim 8,
wherein the bonding of the single crystal semiconductor substrate with the base substrate is performed at a pressure lower than an atmospheric pressure.

### Claim 13 (depends on 8)

The method according to claim 8, further comprising a step of polishing the remaining single crystal semiconductor substrate after the second etching treatment.

### Claim 14 (depends on 8)

The method according to claim 8, wherein the base substrate is a glass substrate.