# US 8,278,185 B2 · Method for forming device isolation layer of semiconductor device and non-volatile memory device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,185 B2
- Document ID: US8278185B2
- Status: Granted
- Kind: B2
- Application number: 12/473,307
- Filed: 2009-05-28
- Published: 2010-07-01
- Granted: 2012-10-02
- Earliest claimed: 2008-12-26
- Assignees: Hynix Semiconductor Inc.
- Inventors: Jae-Hyoung Koo; Jin-Woong Kim; Mi-Ri Lee; Chi-Ho Kim; Jin-Ho Bin
- Web page: https://patentgrep.com/patent/US8278185B2

## CPC

- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10B 41/30: characterised by the memory core region
- H10B 43/30: characterised by the memory core region
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A method for forming a device isolation layer of a semiconductor device or a non-volatile memory device is provided. A method for forming a device isolation layer of a semiconductor device includes: forming trenches having a first predetermined depth by etching a substrate; forming a first insulation layer having a second predetermined depth inside the trenches; forming a liner oxide layer having a predetermined thickness on internal walls of the trenches with the first insulation layer formed therein; and forming a second insulation layer for forming a device isolation layer over the substrate with the liner oxide layer formed therein, wherein the second insulation layer has a lower etch rate than that of the first insulation layer.

## Claims

### Claim 1

A method for forming a device isolation layer of a non-volatile memory device, comprising:
forming a tunnel insulation layer, a charge storage layer, and a hard mask layer over a substrate;
forming trenches having a first depth by etching the hard mask layer, the charge storage layer, the tunnel insulation layer, and the substrate;
forming a first insulation layer having a second depth inside the trenches; and
forming a liner oxide layer having a given thickness on internal walls of the trenches, which are not covered by the first insulation layer, and on a surface of the first insulation layer through an oxidation process of the hard mask; and
forming a second insulation layer over the liner oxide layer,
wherein the second insulation layer has a lower etch rate than that of the first insulation layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming of the first insulation layer includes:
forming a flowable oxide layer over the hard mask layer with the trenches;
forming the first insulation layer by performing a thermal treatment;
planarizing the first insulation layer until a surface of the hard mask layer is exposed; and
removing the first insulation layer while leaving the first insulation layer in the second depth inside the trenches.

### Claim 3 (depends on 1)

The method of claim 1, wherein the forming of the liner oxide layer includes:
oxidizing internal walls of the trenches with the first insulation layer to form the liner oxide layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein a surface of the first insulation layer is lower than a surface of the hard mask layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the predetermined thickness of the liner oxide layer is a thickness ranging from approximately 20 Å to approximately 150 Å.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first insulation layer is an SOD layer formed of PSZ, and the second insulation layer is formed of HDP oxide.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
planarizing the second insulation layer until a surface of the hard mask layer is exposed after the forming of the second insulation layer; and
removing the hard mask layer.