# US 8,278,177 B2 · Semiconductor device and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,177 B2
- Document ID: US8278177B2
- Status: Granted
- Kind: B2
- Application number: 13/240,303
- Filed: 2011-09-22
- Published: 2012-01-12
- Granted: 2012-10-02
- Earliest claimed: 2006-07-28
- Assignees: Fujitsu Semiconductor Limited
- Inventors: Yosuke Shimamune; Masahiro Fukuda; Young Suk Kim; Akira Katakami; Akiyoshi Hatada; Naoyoshi Tamura; Hiroyuki Ohta
- Web page: https://patentgrep.com/patent/US8278177B2

## CPC

- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/015: {removing at least parts of gate spacers, e.g. disposable spacers}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A first p-type SiGe mixed crystal layer is formed by an epitaxial growth method in a trench, and a second p-type SiGe mixed crystal layer is formed. On the second SiGe mixed crystal layer, a third p-type SiGe mixed crystal layer is formed. The height of an uppermost surface of the first SiGe mixed crystal layer from the bottom of the trench is lower than the depth of the trench with the surface of the silicon substrate being the standard. The height of an uppermost surface of the second SiGe mixed crystal layer from the bottom of the trench is higher than the depth of the trench with the surface of the silicon substrate being the standard. Ge concentrations in the first and third SiGe mixed crystal layers are lower than a Ge concentration in the second SiGe mixed crystal layer.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising:
forming a gate insulating film on a silicon substrate;
forming a gate electrode on the gate insulating film;
forming impurity diffused layers in the silicon substrate by ion-implanting with the gate electrode as a mask;
forming a trench in the impurity diffused layers;
forming a first crystal layer on a bottom of the trench, the first crystal layer located within or higher than a same plane with an interface between the silicon substrate and the gate insulating film; and
forming a second crystal layer on the first crystal layer;
forming a silicide layer on the second crystal layer;
wherein said second crystal layer has a lattice constant closer to a lattice constant of silicon than a lattice constant of the first crystal layer.

### Claim 2

A method of manufacturing a semiconductor device, comprising:
forming a gate insulating film on a silicon substrate;
forming a gate electrode on the gate insulating film;
forming impurity diffused layers in the silicon substrate by ion-implanting with the gate electrode as a mask;
forming a trench in the impurity diffused layers;
forming a first crystal layer on a bottom of the trench, the first crystal layer located within or higher than a same plane with an interface between the silicon substrate and the gate insulating film; and
forming a second crystal layer on the first crystal layer;
forming a silicide layer on the second crystal layer;
wherein the first crystal layer is constituted of silicon germanium having a first germanium concentration, and the second crystal layer is constituted of silicon germanium having a second germanium concentration which is lower than the first germanium concentration.

### Claim 3 (depends on 2)

The method of manufacturing a semiconductor device according to claim 2, wherein
the first germanium concentration is 20 atom % or higher, and the second germanium concentration is lower than 20 atom %.

### Claim 4 (depends on 2)

The method of manufacturing a semiconductor device according to claim 2, wherein
the first crystal layer is formed at a first growing temperature, and the second crystal layer is formed at a second growing temperature which is higher than the first growing temperature.

### Claim 5

The method of manufacturing a semiconductor device, comprising:
forming a gate insulating film on a silicon substrate;
forming a gate electrode on the gate insulating film;
forming impurity diffused layers in the silicon substrate by ion-implanting with the gate electrode as a mask;
forming a trench in the impurity diffused layers;
forming a first crystal layer on a bottom of the trench, the first crystal layer located within or lower than a same plane with an interface between the silicon substrate and the gate insulating film; and
forming a second crystal layer on the first crystal layer;
forming a silicide layer on the second crystal layer;
wherein the first crystal layer has a lattice constant closer to a lattice constant of silicon than a lattice constant of the second crystal layer.

### Claim 6

The method of manufacturing a semiconductor device, comprising:
forming a gate insulating film on a silicon substrate;
forming a gate electrode on the gate insulating film;
forming impurity diffused layers in the silicon substrate by ion-implanting with the gate electrode as a mask;
forming a trench in the impurity diffused layers;
forming a first crystal layer on a bottom of the trench, the first crystal layer located within or lower than a same plane with an interface between the silicon substrate and the gate insulating film; and
forming a second crystal layer on the first crystal layer;
forming a silicide layer on the second crystal layer;
wherein the first crystal layer is constituted of silicon germanium having a first germanium concentration, and the second crystal layer is constituted of silicon germanium having a second germanium concentration which is higher than the first germanium concentration.

### Claim 7 (depends on 6)

The method of manufacturing a semiconductor device according to claim 6, wherein:
the first germanium concentration is lower than 20 atom %, and the second germanium concentration is 20 atom % or higher.

### Claim 8 (depends on 6)

A method of manufacturing a semiconductor device according to claim 6, wherein:
the first crystal layer is formed at a first growing temperature, and the second crystal layer is formed at a second growing temperature which is lower than the first growing temperature.