# US 8,278,171 B2 · Fabrication method for semiconductor device having laminated electronic conductor on bit line

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,171 B2
- Document ID: US8278171B2
- Status: Granted
- Kind: B2
- Application number: 13/081,777
- Filed: 2011-04-07
- Published: 2011-07-28
- Granted: 2012-10-02
- Earliest claimed: 2005-05-30
- Assignees: Spansion LLC
- Inventors: Kenichi Fujii; Masahiko Higashi
- Web page: https://patentgrep.com/patent/US8278171B2

## CPC

- H10P 30/21: {of electrically active species}
- H10B 43/30: characterised by the memory core region
- H10B 69/00: Erasable-and-programmable ROM [EPROM] devices not provided for in groups H10B41/00 - H10B63/00, e.g. ultraviolet erasable-and-programmable ROM [UVEPROM] devices
- H10D 30/0413: {of FETs having charge-trapping gate insulators, e.g. MNOS transistors}
- H10P 30/204: {into Group IV semiconductors}
- H10W 15/00: Highly-doped buried regions of integrated devices
- H10W 15/01: {Manufacture or treatment}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

There are provided a semiconductor device and a fabrication method therefor including an ONO film (18) formed on a semiconductor substrate (10), a word line (24) formed on the ONO film (18), a bit line (20) formed in the semiconductor substrate (10), and a conductive layer (32) that is in contact with the bit line (20), runs in a length direction of the bit line (20), and includes a polysilicon layer or a metal layer. In accordance with the present invention, a semiconductor device and a fabrication method therefor are provided wherein degradation of the writing and erasing characteristics and degradation of the transistor characteristics such as a junction leakage are suppressed, and the bit line resistance is decreased.

## Claims

### Claim 1

A method of fabricating a semiconductor device comprising:
forming a tunnel oxide film and a trap layer overlaying the tunnel oxide film on a semiconductor substrate;
forming a bit line in the semiconductor substrate;
forming an opening in contact with the bit line in the tunnel oxide film and in the trap layer; and
forming a conductive layer in the opening and running in a length direction of the bit line, wherein the conductive layer runs substantially the entire length of the bit line, and wherein the conductive layer comprises a polysilicon layer or a metal layer in contact with the bit line.

### Claim 2 (depends on 1)

The method as claimed in claim 1, further comprising forming a protection film on the trap layer, wherein forming the opening includes forming the opening in the protection film.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein forming the conductive layer includes:
forming the polysilicon layer or the metal layer on the protection film and in the opening; and
polishing the protection film and either the polysilicon layer or the metal layer.

### Claim 4 (depends on 3)

The method as claimed in claim 3, further comprising forming a metal silicide layer on the conductive layer.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein forming the metal silicide layer includes forming a metal layer to be silicided on the conductive layer and on a silicon nitride film.

### Claim 6 (depends on 2)

The method as claimed in claim 2, further comprising:
removing the protection film; and
forming a top oxide film over the trap layer and the conductive layer.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein forming the top oxide film comprises forming the top oxide film having a thickness less than that of the protection film.

### Claim 8 (depends on 6)

The method as claimed in claim 6, further comprising forming a word line on the top oxide film.

### Claim 9 (depends on 2)

The method as claimed in claim 2, further comprising forming a portion of an oxide film over the protection film and the conductive layer, wherein a top oxide film comprises the protection film and the portion of the oxide film.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein forming the conductive layer includes:
forming the polysilicon layer or the metal layer in the opening and on the trap layer; and
etching the polysilicon layer or the metal layer in regions other than the opening.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein a width of the conductive layer is greater than that of the tunnel oxide film and the trap layer.

### Claim 12 (depends on 10)

The method as claimed in claim 10, further comprising forming a metal silicide layer on the conductive layer.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein forming the opening includes etching the trap layer and the tunnel oxide film by using a mask layer and sidewalls as an etching mask, wherein the mask layer is provided above the trap layer, and wherein the sidewalls are formed at both sides of an opening in the mask layer.