# US 8,278,129 B2 · Manufacturing method of nitride semi-conductor layer, and a nitride semi-conductor light emitting device with its manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,129 B2
- Document ID: US8278129B2
- Status: Granted
- Kind: B2
- Application number: 12/622,085
- Filed: 2009-11-19
- Published: 2010-10-28
- Granted: 2012-10-02
- Earliest claimed: 2009-04-22
- Assignees: Panasonic Corporation; Riken
- Inventors: Takayoshi Takano; Kenji Tsubaki; Hideki Hirayama; Sachie Fujikawa
- Web page: https://patentgrep.com/patent/US8278129B2

## CPC

- H10P 14/3216: {Nitrides}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/825: containing nitrogen, e.g. GaN
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2901: {Materials}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3416: {Nitrides}
- H10P 14/3442: {N-type}
- H10P 14/3444: {P-type}
- H10P 14/3602: {In-situ cleaning}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

In a process of fabricating a nitride nitride semi-conductor layer of AlaGabIn(1-a-b)N(0<a<1, 0<b<1, 1−a−b>0), the AlGaInN layer is grown at a growth rate less than 0.09 μm/h according to the metal organic vapor phase epitaxy (MOPVE) method. The AlGaInN layer fabricated by the process in the present invention exhibits a high quality with low defect, and increases internal quantum yield.

## Claims

### Claim 1

A process of fabricating a nitride semi-conductor light emission layer of AlGaInN that is set to emit light having its wavelength of 250 to 300 nm,
said nitride semi-conductor light emission layer comprising a well layer of AlaGabIn(1-a-b)N(0<a<1, 0<b<1, 1−a−b>0) and a barrier layer of AlcGafIn(1-c-f)N(0 <e<1, 0<f<1, 1−e−f>0, e>a),
wherein said well layer is fabricated by growing at a growth rate less than 0.09 μm/h according to the metal organic vapor phase epitaxy (MOVPE) method, and
wherein said barrier layer is fabricated by growing at a growth rate less than 0.09 μm/h according to the metal organic vapor phase epitaxy (MOVPE) method.

### Claim 2 (depends on 1)

A process of fabricating a nitride semi-conductor light emitting device,
wherein said process comprises steps of fabricating a p-type nitride semiconductor layer, an n-type nitride semiconductor layer, and said light emission layer therebetween;
wherein said light emission layer is formed according to the process as defined in claim 1.

### Claim 3 (depends on 2)

The process of fabricating a nitride semi-conductor light emitting device according to claim 2,
wherein said p-type nitride semiconductor layer of AlcGadIn(1-c-d)N(0<c<1 , 0<d<1, 1−c−d>0) layer is fabricated by growing at a growth rate less than 0.09 μm/h according to the metal organic vapor phase epitaxy (MOVPE) method.

### Claim 4 (depends on 1)

The process of fabricating said nitride semi-conductor light emission layer as set forth in claim 1,
wherein said well layer of AlaGabIn(1-a-b)N(0<a<1, 0<b<1, 1−a−b>0) is fabricated by growing at a growth rate equal to or less than 0.03 μm/h according to the metal organic vapor phase epitaxy (MOVPE) method, and
wherein said barrier layer of AlcGafIn(1-c-f)N(0<e<1, 0<f<1, 1−e−f>0, e>a) is fabricated by growing at a growth rate equal to or less than 0.03 μm/h according to the metal organic vapor phase epitaxy (MOVPE) method.

### Claim 5 (depends on 1)

The process of fabricating said nitride semi-conductor light emission layer as set forth in claim 1,