# US 8,278,020 B2 · Polyester synthesis

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,020 B2
- Document ID: US8278020B2
- Status: Granted
- Kind: B2
- Application number: 12/207,959
- Filed: 2008-09-10
- Published: 2010-03-11
- Granted: 2012-10-02
- Earliest claimed: 2008-09-10
- Assignees: Xerox Corporation
- Inventors: Jordan H. Wosnick
- Web page: https://patentgrep.com/patent/US8278020B2

## CPC

- G03G 9/08753: {Epoxyresins}
- C08G 59/027: {obtained by epoxidation of unsaturated precursor, e.g. polymer or monomer}
- C08G 63/912: {derived from hydroxycarboxylic acids}
- C08G 63/918: {Polycarboxylic acids and polyhydroxy compounds in which at least one of the two components contains aliphatic unsaturation}
- G03G 9/0802: {Preparation methods}
- G03G 9/0819: {characterised by the dimensions of the particles}
- G03G 9/0827: {characterised by their shape, e.g. degree of sphericity}
- G03G 9/08755: {Polyesters}
- G03G 9/08791: {characterised by the presence of specified groups or side chains}
- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The present disclosure provides methods for modifying polymeric resin materials after polymerization to make fine adjustments in the chemical or physical properties of the resin, or in modifying the structure of the polymer chains. The resulting resins may be useful in forming toner particles. In embodiments, a polymeric resin may have epoxy groups added to its backbone to increase its melting point. The resulting polymer, sometimes referred to herein as an epoxidized polymer, may, in turn, be reacted with wax-like components, to increase the compatibility of the polyester with waxes utilized in forming toner particles. In other embodiments, the resulting epoxidized polymer may be reacted with components possessing carboxylic acid groups to adjust the acid value and weight average molecular weight of the resin.

## Claims

### Claim 1

A process comprising:
contacting at least one unsaturated polyester with at least one epoxidizing agent selected from the group consisting of peroxyacids, peroxyphthalates, hydrogen peroxide with a suitable catalyst, and combinations thereof to form an epoxidized polyester resin;
wherein the epoxidized polyester resin has a melting point of from about 58° C. to about 80° C., a number average molecular weight of from about 3,000 g/mol to about 50,000 g/mol, and a weight average molecular weight of from about 10,000 g/mol to about 100,000 g/mol;
contacting the epoxidized polyester resin with at least one colorant, an optional wax, and an optional surfactant to form toner particles; and
recovering the toner particles.

### Claim 2 (depends on 1)

A process as in claim 1, wherein the at least one unsaturated polyester is selected from the group consisting of poly(propoxylated bisphenol co-fumarate), poly(ethoxylated bisphenol co-fumarate), poly(butyloxylated bisphenol co-fumarate), poly(co-propoxylated bisphenol co-ethoxylated bisphenol co-fumarate), poly(1,2-propylene fumarate), poly(propoxylated bisphenol co-maleate), poly(ethoxylated bisphenol co-maleate), poly(butyloxylated bisphenol co-maleate), poly(co-propoxylated bisphenol co-ethoxylated bisphenol co-maleate), poly(1,2-propylene maleate), poly(propoxylated bisphenol co-itaconate), poly(ethoxylated bisphenol co-itaconate), poly(butyloxylated bisphenol co-itaconate), poly(co-propoxylated bisphenol co-ethoxylated bisphenol co-itaconate), poly(1,2-propylene itaconate), poly(pentadecalactone), poly(pentadecenlactone), poly(hexadecenlactone), poly(hexadecen-7-olide), polycaprolactone, polydodecalactone, poly(pentadecalactone co-pentadecenlactone), poly(pentadecalactone co-hexadecenlactone), and combinations thereof.

### Claim 3 (depends on 1)

A process as in claim 1, wherein the epoxidizing agent is selected from the group consisting of meta-chloroperbenzoic acid, magnesium monoperoxyphthalate, hydrogen peroxide and a suitable catalyst, in an amount of from about 1% by weight of the polyester to about 200% by weight of the polyester.

### Claim 4 (depends on 1)

A process as in claim 1, wherein from about 1% to about 90% of the unsaturated groups in the polymer backbone are epoxidized, and wherein the epoxidized polyester resin has a different melting point than the at least one unsaturated polyester.

### Claim 5 (depends on 1)

A process as in claim 1, further comprising contacting the epoxidized polyester resin with a wax-like component selected from the group consisting of long-chain aliphatic alcohols, long-chain aliphatic amines, and combinations thereof, in an amount of from about 0.1% by weight of the epoxidized resin to about 50% by weight of the epoxidized polyester resin.

### Claim 6 (depends on 1)

A process as in claim 1, further comprising contacting the epoxidized polyester resin with a component possessing carboxylic acid groups selected from the group consisting of , glycolic acid, lactic acid, hydroxypropanoic acid, other hydroxyalkanoic acids, citric acid, glycine, other amino acids, and combinations thereof, in an amount of from about 0.1% by weight of the epoxidized resin to about 50% by weight of the epoxidized polyester resin.

### Claim 7 (depends on 6)

A process as in claim 6, wherein the epoxidized polyester resin that has been contacted with the component possessing carboxylic acid groups has an acid value of from about 2 milligrams of potassium hydroxide per gram of resin to about 30 milligrams of potassium hydroxide per gram of resin, a weight average molecular weight of from about 10,000 g/mol to about 100,000 g/mol, and a number average molecular weight of from about 3,000 g/mol to about 50,000 g/mol.

### Claim 8

A process comprising:
contacting at least one unsaturated polyester with at least one epoxidizing agent selected from the group consisting of peroxyacids, peroxyphthalates, hydrogen peroxide and a suitable catalyst, and combinations thereof to form an epoxidized polyester resin;
contacting the epoxidized polyester resin with a component selected from the group consisting of wax-like components and components possessing carboxylic acid groups to form a modified epoxidized polyester resin;
wherein the epoxidized polyester resin has a melting point of from about 58° C. to about 80° C., a number average molecular weight of from about 3,000 g/mol to about 50,000 g/mol, and a weight average molecular weight of from about 10,000 g/mol to about 100,000 g/mol;
contacting the modified epoxidized polyester resin with at least one colorant, an optional wax, and an optional surfactant to form toner particles; and
recovering the toner particles.

### Claim 9 (depends on 8)

A process as in claim 8, wherein the at least one unsaturated polyester is selected from the group consisting of poly(propoxylated bisphenol co-fumarate), poly(ethoxylated bisphenol co-fumarate), poly(butyloxylated bisphenol co-fumarate), poly(co-propoxylated bisphenol co-ethoxylated bisphenol co-fumarate), poly(1,2-propylene fumarate), poly(propoxylated bisphenol co-maleate), poly(ethoxylated bisphenol co-maleate), poly(butyloxylated bisphenol co-maleate), poly(co-propoxylated bisphenol co-ethoxylated bisphenol co-maleate), poly(1,2-propylene maleate), poly(propoxylated bisphenol co-itaconate), poly(ethoxylated bisphenol co-itaconate), poly(butyloxylated bisphenol co-itaconate), poly(co-propoxylated bisphenol co-ethoxylated bisphenol co-itaconate), poly(1,2-propylene itaconate), poly(pentadecalactone), poly(pentadecenlactone), poly(hexadecenlactone), poly(hexadecen-7-olide), polycaprolactone, polydodecalactone, poly(pentadecalactone co-pentadecenlactone), poly(pentadecalactone co-hexadecenlactone), and combinations thereof.

### Claim 10 (depends on 8)

A process as in claim 8, wherein the epoxidizing agent is selected from the group consisting of meta-chloroperbenzoic acid, magnesium monoperoxyphthalate, and hydrogen peroxide with a suitable catalyst, in an amount of from about 1% by weight of the polyester to about 200% by weight of the polyester.

### Claim 11 (depends on 8)

A process as in claim 8, wherein from about 1% to about 90% of the unsaturated groups in the polymer backbone are epoxidized.

### Claim 12 (depends on 8)

A process as in claim 8, wherein the wax-like component is selected from the group consisting of long-chain aliphatic alcohols, long-chain aliphatic amines, and combinations thereof, in an amount of from about 0.1% by weight of the epoxidized resin to about 50% by weight of the epoxidized resin.

### Claim 13 (depends on 8)

A process as in claim 8, wherein the component possessing carboxylic acid groups is selected from the group consisting of , glycolic acid, lactic acid, hydroxypropanoic acid, other hydroxyalkanoic acids, citric acid, glycine, other amino acids, and combinations thereof, in an amount of from about 0.1% by weight of the epoxidized resin to about 50% by weight of the epoxidized resin.

### Claim 14 (depends on 13)

A process as in claim 13, wherein the modified epoxidized resin that has been contacted with the component possessing carboxylic acid groups has an acid value of from about 2 milligrams of potassium hydroxide per gram of resin to about 30 milligrams of potassium hydroxide per gram of resin, a weight average molecular weight of from about 10,000 g/mol to about 100,000 g/mol, and a number average molecular weight of from about 3,000 g/mol to about 50,000 g/mol.

### Claim 15

A toner comprising:
an epoxidized polyester resin optionally in combination with at least one other resin selected from the group consisting of amorphous polyester resins and crystalline polyester resins;
wherein the epoxidized polyester resin has a melting point of from about 58° C. to about 80° C., a number average molecular weight of from about 3,000 g/mol to about 50,000 g/mol, and a weight average molecular weight of from about 10,000 g/mol to about 100,000 g/mol; and
one or more optional ingredients selected from the group consisting of colorants, waxes, and combinations thereof.

### Claim 16 (depends on 15)

A toner as in claim 15, wherein the epoxidized resin comprises a modified epoxidized resin including the epoxidized resin in combination with a component selected from the group consisting of wax-like components and components possessing carboxylic acid groups, and wherein the epoxidized polyester resin has a different melting point than a polyester resin that has not been epoxidized.

### Claim 17 (depends on 16)

A toner as in claim 16, wherein the wax-like component is selected from the group consisting of long-chain aliphatic alcohols, long-chain aliphatic amines, and combinations thereof, in an amount of from about 0.1% by weight of the epoxidized resin to about 50% by weight of the epoxidized resin.

### Claim 18 (depends on 16)

A toner as in claim 16, wherein the component possessing carboxylic acid groups is selected from the group consisting of , glycolic acid, lactic acid, hydroxypropanoic acid, other hydroxyalkanoic acids, citric acid, glycine, other amino acids, and combinations thereof, present in an amount of from about 0.1% by weight of the epoxidized resin to about 50% by weight of the epoxidized resin, and wherein the modified epoxidized resin has an acid value of from about 2 milligrams of potassium hydroxide per gram of resin to about 30 milligrams of potassium hydroxide per gram of resin.

### Claim 19 (depends on 15)

A toner as in claim 15, wherein particles comprising the toner have a volume average diameter of from about 1 micron to about 20 microns, and a circularity of from about 0.9 to about 0.99.