# US 8,278,001 B2 · Low-porosity anode diffusion media for high concentration direct methanol fuel cells and method of making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,278,001 B2
- Document ID: US8278001B2
- Status: Granted
- Kind: B2
- Application number: 12/711,817
- Filed: 2010-02-24
- Published: 2010-09-02
- Granted: 2012-10-02
- Earliest claimed: 2008-02-15
- Assignees: Panasonic Corporation; The Penn State Research Foundation
- Inventors: Seung Hun Jung; Chao-Yang Wang; Takashi Akiyama
- Web page: https://patentgrep.com/patent/US8278001B2

## CPC

- H01M 8/023: Porous and characterised by the material
- H01M 8/04186: of liquid-charged or electrolyte-charged reactants
- H01M 8/04197: {Preventing means for fuel crossover}
- H01M 8/1009: with one of the reactants being liquid, solid or liquid-charged (H01M8/12 takes precedence)
- H01M 8/1011: Direct alcohol fuel cells [DAFC], e.g. direct methanol fuel cells [DMFC]
- H01M 8/0234: Carbonaceous material
- H01M 8/0239: Organic resins; Organic polymers
- H01M 8/0243: in the form of mixtures
- H01M 8/0245: in the form of layered or coated products
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A direct oxidation fuel cell (DOFC) having a liquid fuel and an anode electrode configured to generate power. The anode electrode includes a gas diffusion layer (GDL) and a microporous layer, such that a decrease in the porosity of the GDL achieves an increase in the power density of the DOFC.

## Claims

### Claim 1

A direct oxidation fuel cell (DOFC) comprising:
an anode electrode configured to generate power, the anode electrode having a gas diffusion layer (GDL) loaded with at least one polymer and a microporous layer;
wherein the GDL has a porosity such that it increases the power density of the DOFC,
wherein said porosity is adjusted by adjusting the polymer content of the GDL and,
wherein said porosity is selected based on at least one of the group consisting of:
operating temperature of the DOFC and
current density of the DOFC,
wherein, the DOFC is configured to have at least one selected from the group consisting of: an operating temperature of about 50° C. and porosity of about 0.59%; an operating temperature of 70° C. and porosity of about 0.48%; a current density of about 300 mA/cm2 and porosity of about 0.53%; and a current density is 200 mA/cm2 and porosity is about 0.41%,
wherein one of the at least one polymer is a fluorinated polymer, and
wherein the GDL is loaded at between 30 wt % to 70 wt % with the at least one fluorinated polymer.

### Claim 2 (depends on 1)

The DOFC of claim 1 wherein one of the at least one fluorinated polymers is ethylene propylene.

### Claim 3 (depends on 1)

The DOFC of claim 1, wherein the fuel cell further comprises a concentrated liquid fuel.

### Claim 4 (depends on 3)

The DOFC of claim 3, wherein said concentrated liquid fuel is methanol.

### Claim 5 (depends on 4)

The DOFC of claim 4, wherein said concentrated liquid methanol is at least 2 molar (M) concentration.

### Claim 6

A method of making a direct oxidation fuel cell (DOFC) comprising:
configuring an anode electrode comprising a gas diffusion layer (GDL) and a microporous layer (MPL),
selecting at least one of:
a operating temperature of the DOFC and
a current density of the DOFC, and
adjusting the porosity of the GDL based on the operating temperature of the DOFC or the current density of the DOFC by adjusting a fluorinated polymer content of the GDL, to achieve a porosity of the GDL such that it increases the power density of the DOFC,
wherein, the DOFC is configured to have at least one selected from the group consisting of: an operating temperature of about 50° C. and porosity of about 0.59%; an operating temperature of 70° C. and porosity of about 0.48%; a current density of about 300 mA/cm2 and porosity of about 0.53%; and a current density is 200 mA/cm2 and porosity is about 0.41%, and
wherein said GDL is loaded at 30 wt % to 70 wt % with the at least one fluorinated polymer.

### Claim 7 (depends on 6)

The method of claim 6, wherein one of the at least one fluorinated polymer is ethylene propylene.

### Claim 8 (depends on 6)

The method of claim 6, wherein said GDL comprises carbon paper.

### Claim 9 (depends on 6)

The method of claim 6, wherein said MPL is prepared from carbon powder and Polytetrafluorethylene (PTFE) suspension.

### Claim 10

A method of operating a direct oxidation fuel cell (DMFC) system, comprising steps of:
(a) providing at least one fuel cell assembly including a cathode and an anode with an electrolyte positioned therebetween, said anode comprising a gas diffusion layer (GDL) including a microporous layer, said microporous layer comprising an electrically conductive material and a fluoropolymer, loading of said fluoropolymer in said microporous layer being in the range from about 30 to about 70 wt. %;
b) supplying a concentrated solution of a liquid fuel and water to said anode;
c) operating said at least one fuel cell assembly in at least one selected from the group consisting of: at a temperature of about 50° C. and porosity of about 0.59%;
at a temperature of 70° C. and porosity of about 0.48%; at a current density of about 300 mA/cm2 and porosity of about 0.53%; and at a current density is 200 mA/cm2 and porosity is about 0.41%.