# US 8,277,982 B2 · Method for improvement of the consumption controlling performance of water-soluble electrolyte chemical cells and fuel cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,982 B2
- Document ID: US8277982B2
- Status: Granted
- Kind: B2
- Application number: 11/427,452
- Filed: 2006-06-29
- Published: 2008-01-03
- Granted: 2012-10-02
- Earliest claimed: 2006-06-29
- Inventors: Yasuo Sakakura
- Web page: https://patentgrep.com/patent/US8277982B2

## CPC

- H01M 8/04: Auxiliary arrangements, e.g. for control of pressure or for circulation of fluids
- H01M 6/50: Methods or arrangements for servicing or maintenance, e.g. for maintaining operating temperature (constructional details of current conducting connections for detecting conditions inside cells or batteries, e.g. details of voltage sensing terminals, H01M50/569)
- H01M 10/42: Methods or arrangements for servicing or maintenance of secondary cells or secondary half-cells (H01M10/60 takes precedence)
- H01M 6/06: Dry cells, i.e. cells wherein the electrolyte is rendered non-fluid
- H01M 10/345: {Gastight metal hydride accumulators}
- Y02E 60/10: Energy storage using batteries
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention provides a hydrogen activating material, which includes as a major constituent an iron-semiconductor alloy containing iron and semiconductor components. It also provides a consumption controlling material for water-soluble electrolyte chemical cells and fuel cells. In addition a hydrogen activating method is also provided.

## Claims

### Claim 1

A method of retaining a high voltage of water-soluble electrolyte chemical cells with regard to an iron-semiconductor alloy in the shape of a plate produced by addition of a semiconductor to molten iron during steel making and rolling under load, comprising locating the iron-semiconductor alloy in the vicinity of the water-soluble electrolyte chemical cells, then severely vibrating the semiconductor by irradiating the iron-semiconductor alloy, from which vibrating-electromagnetic waves are generated on the basis of electrochemical potentials across iron and semiconductor crystals, with sunlight or white light with wavelengths of from 1 nm to 1 mm, thereby enhancing vibrating-electromagnetic waves further generated from the alloy and retaining a high voltage of water-soluble electrolyte chemical cells in the vicinity of the alloy, wherein the content of the semiconductor is 1-10 weight percent and the content of iron is 78-98 weight percent.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said semiconductor is silicon.

### Claim 3

A method of retaining a high voltage of fuel cells with regard to an iron-semiconductor alloy in the shape of a plate produced by addition of a semiconductor to molten iron during steel making and rolling under load, comprising locating the iron-semiconductor alloy in the vicinity of the fuel cells, then severely vibrating the semiconductor by irradiating the iron-semiconductor alloy, from which vibrating-electromagnetic waves are generated on the basis of electrochemical potentials across iron and semiconductor crystals, with sunlight or white light with wavelengths of from 1 nm to 1 mm, thereby enhancing vibrating-electromagnetic waves further generated from the alloy and retaining a high voltage of fuel cells in the vicinity of the alloy, wherein the content of the semiconductor is 1-10 weight percent and the content of iron is 78-98 weight percent.

### Claim 4 (depends on 3)

The method according to claim 3, wherein said semiconductor is silicon.