# US 8,277,960 B2 · Inhomogeneous compounds having high magnetic resistance, the production and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,960 B2
- Document ID: US8277960B2
- Status: Granted
- Kind: B2
- Application number: 12/992,987
- Filed: 2009-05-20
- Published: 2011-06-09
- Granted: 2012-10-02
- Earliest claimed: 2008-05-30
- Assignees: Johannes Gutenberg-Universitat Mainz
- Inventors: Frederick Casper; Claudia Felser
- Web page: https://patentgrep.com/patent/US8277960B2

## CPC

- H10N 50/85: Materials of the active region
- H01F 1/408: {half-metallic, i.e. having only one electronic spin direction at the Fermi level, e.g. CrO2, Heusler alloys (H01F10/1936 takes precedence)}
- Y10T 428/11: Magnetic recording head
- Y10T 428/115: Magnetic layer composition
- Y10T 428/32: Composite [nonstructural laminate] of inorganic material having metal-compound-containing layer and having defined magnetic layer
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to inorganic, intermetallic, inhomogeneous compounds having a magnetic resistance effect and an intrinsic field sensitivity of at least 7% at 1 T at room temperature. The invention further relates to a method for the production and use thereof, particularly as magnetic field sensors or in spin electronics.

## Claims

### Claim 1

An inhomogeneous inorganic compound containing an overall phase system comprising a main phase and at least one secondary phase, of which
the main phase is an intermetallic compound,
wherein the intermetallic compound
has at least three elements per formula unit,
is semiconducting or has a metal-semiconductor transition,
has a magnetoresistance with an intrinsic field sensitivity of at least 0.1% per 0.1 T,
has cubic symmetry with a maximum structural distortion of 10%
belongs to half-Heusler phases
has 8 or 18 valence electrons and
is paramagnetic
and wherein the secondary phase
is metallic and comprises at least one element which occurs in the intermetallic compound.

### Claim 2 (depends on 1)

The compound as claimed in claim 1, wherein the main phase constitutes at least 70 wt % of the overall phase system.

### Claim 3 (depends on 1)

The compound as claimed in claim 1, wherein at least one secondary phase is distributed randomly in the main phase.

### Claim 4 (depends on 1)

The compound as claimed in claim 1, wherein said compound has a magnetoresistance effect above 23° C.

### Claim 5 (depends on 1)

The compound as claimed in claim 1, wherein the intermetallic compound is a lutetium or lanthanum compound with a group VIIIb element and a metal or semimetal of main group V.

### Claim 6 (depends on 1)

The compound as claimed in claim 1, wherein the intermetallic compound is a lutetium or lanthanum compound with a group Ib element and a metal or semimetal of main group IV.

### Claim 7 (depends on 5)

The compound as claimed in claim 5, wherein the intermetallic compound is LuNiBi, LuPtBi, LuPdBi, LuNiSb, LuPdSb, LuPtSb, LaPtBi or LaPdBi.

### Claim 8 (depends on 6)

The compound as claimed in claim 6, wherein the intermetallic compound is LuAuSn or LuAuPb.

### Claim 9 (depends on 1)

The compound as claimed in claim 1, wherein the magnetoresistance MR is positive.

### Claim 10 (depends on 1)

A method for producing an inhomogeneous compound as claimed in claim 1 comprising combining three different elements to form the compound, at least one element present in excess,
wherein the type and amount of elements selected form compounds in which
the resulting compound is cubically crystallized with a maximum lattice parameter distortion of 10%,
the compound belongs to half-Heusler phases,
the compound is semiconducting or has a metal-semiconductor transition,
the compound has a magnetoresistance with an intrinsic field sensitivity of at least 0.1% per 0.1 T,
the compound has 8 or 18 valence electrons and
the compound is paramagnetic.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein said combining step comprises melting the three elements by an arc welding device in an inert gas atmosphere.

### Claim 12 (depends on 1)

Read heads in storage media comprising the compounds as claimed in claim 1.

### Claim 13 (depends on 1)

The compound as claimed in claim 1, wherein the overall phase system consists of the main phase and at least one secondary phase and the secondary phase consists of at least one element which occurs in the intermetallic compound.