# US 8,277,881 B2 · White reflective coating for modified bitumen membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,881 B2
- Document ID: US8277881B2
- Status: Granted
- Kind: B2
- Application number: 10/851,580
- Filed: 2004-05-21
- Published: 2005-11-24
- Granted: 2012-10-02
- Earliest claimed: 2004-05-21
- Assignees: Building Materials Investment Corporation
- Inventors: Amir Khan; Michael De Souto
- Web page: https://patentgrep.com/patent/US8277881B2

## CPC

- C09D 5/004: {Reflecting paints; Signal paints}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A coating composition useful for building materials products, especially roofing surfaces, is provided. The coating composition provides durable exterior protection to surfaces that it applied to, and it has reflective properties. The coating composition includes a mixture of a polymeric binder, a polymeric carrier and a pigment. The pigment is present in the coating composition in amount that is capable of providing a coating that has an initial energy efficiency rating greater than or equal to 0.65 for a low-sloped roof, or an initial energy efficiency greater than or equal to 0.25 for a steep-sloped roof.

## Claims

### Claim 1

A method of manufacturing a modified bitumen roofing membrane, the method comprising:
providing an aqueous dispersion of a polymeric binder, a polymeric carrier and an effective amount of a pigment that is capable of providing a coating that has an initial energy efficacy rating greater than or equal to 0.65 for a low-sloped roof, or an initial energy efficacy greater than or equal to 0.25 for a steep-sloped roof;
maintaining constant mixing of the aqueous dispersion under low shear conditions of about 60 rpm or less to create a top coating composition;
applying said top coating composition in-plant to an exterior surface of a modified bitumen substrate during manufacture of the roofing membrane; and
curing said top coating composition at the temperature of the environment in which the coated substrate is located.

### Claim 2 (depends on 1)

The method of claim 1 wherein the polymeric binder is a thermoplastic polymer selected from the group consisting of acrylic or methacrylic polymers or copolymers, epoxy resins, and polyvinyl acetate.

### Claim 3 (depends on 1)

The method of claim 1 wherein the polymeric carrier is water or a hydrocarbon solvent.

### Claim 4 (depends on 1)

The method of claim 1 wherein the pigment comprises titanium dioxide, calcium carbonate, colemanite, aluminum trihydrate (ATH), borate compounds or mixtures thereof.

### Claim 5 (depends on 1)

The method of claim 1 where the pigment is titanium dioxide.

### Claim 6 (depends on 1)

The method of claim 1 wherein the polymeric binder and the polymeric carrier form an aqueous polymeric-based emulsion.

### Claim 7 (depends on 1)

The method of claim 1 wherein the polymeric binder and the polymeric carrier form a solvent polymeric-based emulsion.

### Claim 8 (depends on 1)

The method of claim 1 wherein the polymeric binder is present in said mixture in an amount from about 30 to about 60 wt. %.

### Claim 9 (depends on 1)

The method of manufacturing a roofing membrane of claim 1 wherein the polymeric binder is an acrylic polymer that is present in said mixture in an amount from about 30 to about 60 wt. %.

### Claim 10 (depends on 1)

The method of claim 1 wherein the polymeric binder is an acrylic polymer that is present in said mixture in an amount from about 40 to about 50 wt. %.

### Claim 11 (depends on 1)

The method of claim 1 wherein the pigment is present in said mixture in an amount from about 1 to about 20 wt. %.

### Claim 12 (depends on 1)

The method of claim 1 further comprising the addition of one or more optional components selected from the group consisting of dispersants, defoamers, fillers, solvents, microbiocides, thickening agents, coalescent agents, fire retardants, pH modifiers, wetting agents, light stabilizers, and adhesion promoters.

### Claim 13

A method of manufacturing a modified bitumen roofing membrane, the method comprising:
(1) mixing the following ingredients as an aqueous dispersion under low shear conditions of about 60 rpm or less to create a top coating composition:
(a) 2-40% water;
(b) 0.1-0.6% potassium tripolyphosphate;
(c) 0.1-7.0% sodium salt of a carboxylic acid;
(d) 0.1-7.0% oil-based defoamer;
(e) 5-60% binder;
(f) 0.1-7% thickener;
(g) 0.5-7.0% coalescing agent;
(h) 5-45% alumina trihydrate;
(i) 0.1-4% microbiocide;
(j) 1-10% zinc borate;
(k) 0.1-4% zinc oxide;
(l) an effective amount of titanium dioxide that is capable of providing a coating that has an initial energy efficacy rating greater than or equal to 0.65 for a low-sloped roof, or an initial energy efficacy greater than or equal to 0.25 for a steep-sloped roof; and
(2) applying said top coating composition in-plant to an exterior surface of a substrate during manufacture of the roofing membrane.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
(3) curing said top coating composition at the temperature of the environment in which the coated substrate is located.