# US 8,277,768 B2 · System and method for production of high purity silicon solids and solids therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,768 B2
- Document ID: US8277768B2
- Status: Granted
- Kind: B2
- Application number: 12/271,329
- Filed: 2008-11-14
- Published: 2010-05-20
- Granted: 2012-10-02
- Earliest claimed: 2008-11-14
- Assignees: Texas Instruments Incorporated
- Inventors: Michael Louis Hayden; Jeffrey Allen Hanson; Keith Melcher; Robert Mark Reynolds; Patricia Ann Constandine
- Web page: https://patentgrep.com/patent/US8277768B2

## CPC

- C01B 33/02: Silicon (forming single crystals or homogeneous polycrystalline material with defined structure C30B)
- C01B 33/037: Purification (by zone-melting C30B13/00)
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Systems and methods and resulting compositions of matter including silicon solids from a mixture of silicon and water. The mixture is collected at a collection stage from at least one wafer abrasion process performed on a silicon surface having an impurity concentration ≦0.1 ppb and extracting one portion of the water from the mixture using at least one dryer stage to form a dry cake. The dry cake includes at least 99.99% silicon by weight excluding water and non-silicon species, where a concentration of water in the dry cake is between 0.05% and 1% by weight, and where a concentration of non-silicon species in the dry cake is between 0.05% and 1% by weight.

## Claims

### Claim 1

A method of producing a silicon solids from a mixture comprising silicon and water, the method comprising:
collecting said mixture, said mixture collected from at least one wafer abrasion process performed on a silicon surface having an impurity concentration≦1 ppb;
extracting one portion of said water from said mixture using at least one dryer stage to form a dry cake, said dry cake comprising at least 99.99% silicon by weight excluding water and silica, wherein a concentration of water in said dry cake is between 0.05% and 1% by weight, wherein a concentration of silica in said dry cake is between 0.05% and 1% by weight, and wherein a concentration of other non-silicon species in said dry cake is less than or equal to 0.01% by weight.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
prior to said extracting, removing another portion of said water from said mixture using a plurality of filtration stages to reduce a concentration of said water in said mixture to between 10% and 40% by weight.

### Claim 3 (depends on 2)

The method of claim 2, wherein said extracting further comprises purging said dryer stage with at least one non-oxidizing gas.

### Claim 4 (depends on 3)

The method of claim 3, wherein said non-oxidizing gas comprises nitrogen or argon.

### Claim 5 (depends on 2)

The method of claim 2, wherein said plurality of filtration stages comprises at least a first filtration stage and at least a second filtration stage, and wherein said removing comprises:
introducing said mixture into a receiver mixing tank;
diverting a portion of said mixture in said receiver mixing tank to at least one settling tank through said first filtration stage;
transferring a portion of said mixture in said settling tank into said second filtration stage.

### Claim 6 (depends on 5)

The method of claim 5, wherein said second filtration stage comprises a plate-type filter press.

### Claim 7 (depends on 5)

The method of claim 5, wherein said first filtration stage comprises a microfilter stage.

### Claim 8 (depends on 7)

The method of claim 7, wherein said first filtration stage reduces a concentration of water in said mixture to between 90 and 99% by weight.

### Claim 9 (depends on 5)

The method of claim 5, wherein said removing further comprises purging at least one among said receiver mixing tank, said settling tank, said first filtration stage, and said second filtration stage with a non-oxidizing gas.

### Claim 10 (depends on 1)

The method of claim 1, wherein said mixture collected in said collecting step is a water and silicon mixture of 0.01% to 0.1% silicon by weight in deionized water.

### Claim 11

A method of producing a silicon solids from a mixture principally comprising silicon and water, the method comprising:
collecting said mixture, said mixture collected from at least one clean abrasion process performed on a silicon surface having an impurity concentration≦1 ppb;
removing a first portion of said water from said mixture using a plurality of filtration stages to reduce a concentration of said water in said mixture to between 10% and 40% by weight; and
extracting a second portion of said water from said mixture using at least one dryer stage to form a dry cake, said dry cake comprising at least 99.99% silicon by weight excluding water and silica, wherein a concentration of water in said dry cake is between 0.05% and 1% by weight, wherein a concentration of silica in said dry cake is between 0.05% and 1% by weight, and wherein a concentration of other non-silicon species in said dry cake is less than or equal to 0.01% by weight.