# US 8,277,694 B2 · Sintered compact of composite oxide, amorphous film of composite oxide, process for producing said film, crystalline film of composite oxide and process for producing said film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,694 B2
- Document ID: US8277694B2
- Status: Granted
- Kind: B2
- Application number: 12/668,216
- Filed: 2008-07-04
- Published: 2010-06-10
- Granted: 2012-10-02
- Earliest claimed: 2007-07-13
- Assignees: JX Nippon Mining & Metals Corporation
- Inventors: Masakatsu Ikisawa; Masataka Yahagi; Kozo Osada; Takashi Kakeno
- Web page: https://patentgrep.com/patent/US8277694B2

## CPC

- C23C 14/086: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C04B 35/01: based on oxide ceramics
- C04B 35/457: based on tin oxides or stannates
- C04B 35/6262: {of calcined, sintered clinker or ceramics}
- C04B 35/6263: {characterised by their solids loadings, i.e. the percentage of solids}
- C04B 35/62675: {characterised by the treatment temperature}
- C04B 35/62695: {Granulation or pelletising (devices for shaping artificial aggregates from ceramic mixtures B28B1/004)}
- C04B 35/63416: {Polyvinylalcohols [PVA]; Polyvinylacetates}
- C23C 14/5806: {Thermal treatment}
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3286: Gallium oxides, gallates, indium oxides, indates, thallium oxides, thallates or oxide forming salts thereof, e.g. zinc gallate
- C04B 2235/3293: Tin oxides, stannates or oxide forming salts thereof, e.g. indium tin oxide [ITO]
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/6562: Heating rate
- C04B 2235/72: Products characterised by the absence or the low content of specific components, e.g. alkali metal free alumina ceramics
- C04B 2235/77: Density
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Provided is an amorphous film substantially comprised of indium, tin, calcium and oxygen, wherein tin is contained at a ratio of 5 to 15% based on an atomicity ratio of Sn/(In+Sn+Ca) and calcium is contained at a ratio of 0.1 to 2.0% based on an atomicity ratio of Ca/(In+Sn+Ca), and remnant is indium and oxygen. The film can be further crystallized by annealing at a temperature of 260° C. or lower in which resistivity of the film will be 0.4 mΩcm or less. An ITO thin film for use as a display electrode or the like in a flat panel display can be made into an amorphous ITO film by way of sputter deposition without heating the substrate or adding water during deposition. This ITO film is characterized in that it will crystallize by annealing at a temperature of 260° C. or less, which is not such a high temperature, and have low resistivity after being crystallized. Thus, the present invention aims to provide a method of producing such a film and a sintered compact for producing such a film.

## Claims

### Claim 1

A sintered compact of composite oxide comprising indium, tin, calcium and oxygen, wherein tin is contained at a ratio of 5 to 15% based on an atomicity ratio of Sn/(In+Sn+Ca) and calcium is contained at a ratio of 0.1 to 2.0% based on an atomicity ratio of Ca/(In+Sn+Ca), and remnant is indium and oxygen, and wherein resistivity of the sintered compact is 0.2 mΩcm or less and wherein said sintered compact has a relative density of at least 99.9%.

### Claim 2 (depends on 1)

A method of producing a film of composite oxide, wherein the sintered compact of composite oxide according to claim 1 is sputtered to produce an amorphous film having the same composition.

### Claim 3 (depends on 2)

A method of producing a film of composite oxide according to claim 2, wherein, after producing the amorphous film, the film is crystallized by annealing at a temperature of 260° C. or lower.

### Claim 4 (depends on 3)

A method according to claim 3, wherein a crystalline film of composite oxide is formed by said annealing step and comprises indium, tin, calcium and oxygen, wherein tin is contained at a ratio of 5 to 15% based on an atomicity ratio of Sn/(In+Sn+Ca) and calcium is contained at a ratio of 0.1 to 2.0% based on an atomicity ratio of Ca/(In+Sn+Ca), and remnant is indium and oxygen.

### Claim 5 (depends on 4)

The method according to claim 4, wherein resistivity of the crystalline film is 0.4 mΩcm or less.

### Claim 6

A sintered compact of composite oxide comprising indium, tin, calcium, magnesium and oxygen, wherein tin is contained at a ratio of 5 to 15% based on an atomicity ratio of Sn/(In+Sn+Ca+Mg) and a total amount of calcium and magnesium is at a ratio of 0.1 to 2.0% based on an atomicity ratio of (Ca+Mg)/(In+Sn+Ca+Mg), and remnant is indium and oxygen, and wherein resistivity of the sintered compact is 0.2 mΩcm or less.

### Claim 7

A method of producing a film of composite oxide, comprising the step of sputtering a sintered compact of composite oxide to produce an amorphous film having the same composition as the sintered compact, wherein the sintered compact of composite oxide comprises indium, tin, calcium, magnesium and oxygen, wherein tin is contained at a ratio of 5 to 15% based on an atomicity ratio of Sn/(In+Sn+Ca+Mg) and a total amount of calcium and magnesium is at a ratio of 0.1 to 2.0% based on an atomicity ratio of (Ca+Mg)/(In+Sn+Ca+Mg), and remnant is indium and oxygen, and wherein resistivity of the sintered compact is 0.2 mΩcm or less.

### Claim 8 (depends on 7)

A method of producing a film of composite oxide according to claim 7, wherein, after producing the amorphous film of composite oxide, the amorphous film is crystallized by annealing at a temperature of 260° C. or lower.

### Claim 9 (depends on 8)

A method according to claim 8, wherein a crystalline film of composite oxide formed by the annealing step comprises indium, tin, calcium, magnesium and oxygen, wherein tin is contained at a ratio of 5 to 15% based on an atomicity ratio of Sn/(In+Sn+Ca+Mg) and a total amount of calcium and magnesium is at a ratio of 0.1 to 2.0% based on an atomicity ratio of (Ca+Mg)/(In+Sn+Ca+Mg), and remnant is indium and oxygen.

### Claim 10 (depends on 9)

The method according to claim 9, wherein resistivity of the crystalline film is 0.4 mΩcm or less.