# US 8,277,691 B2 · High performance carbon nanocomposites for ultracapacitors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,691 B2
- Document ID: US8277691B2
- Status: Granted
- Kind: B2
- Application number: 12/435,992
- Filed: 2009-05-05
- Published: 2009-11-05
- Granted: 2012-10-02
- Earliest claimed: 2008-05-05
- Assignees: ADA Technologies, Inc.
- Inventors: Wen Lu
- Web page: https://patentgrep.com/patent/US8277691B2

## CPC

- H01B 1/04: mainly consisting of carbon-silicon compounds, carbon or silicon
- H01G 11/36: Nanostructures, e.g. nanofibres, nanotubes or fullerenes
- H01G 11/38: Carbon pastes or blends; Binders or additives therein
- H01G 11/42: Powders or particles, e.g. composition thereof
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- Y02E 60/10: Energy storage using batteries
- Y02E 60/13: Energy storage using capacitors
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to composite electrodes for electrochemical devices, particularly to carbon nanotube composite electrodes for high performance electrochemical devices, such as ultracapacitors.

## Claims

### Claim 1

An electrode material for an electrochemical energy storage device, comprising:
(a) a plurality of activated carbon particles;
(b) a plurality of carbon nanotubes; and
(c) a binder comprising a polymeric binder and an ionic liquid, wherein the plurality of activated carbon particles are intermixed and dispersed within an entangled carbon nanotube network comprising the plurality of carbon nanotubes, wherein the plurality of carbon nanotubes and the plurality of activated carbon particles are substantially dispersed in the binder, wherein at least most of the carbon nanotubes are in contact with at least two or more of the activated carbon particles.

### Claim 2 (depends on 1)

The electrode material of claim 1, wherein the plurality carbon nanotubes further comprise one of single walled carbon nanotubes, multi-walled carbon nanotubes, and mixtures thereof and wherein the carbon nanotubes have a length ranging from about 10 to about 1,000 μm and wherein the carbon nanotubes have an electrical conductivity of at most about 200 S/cm.

### Claim 3 (depends on 1)

The electrode material of claim 1, wherein the polymeric binder is a polymer selected from the group consisting essentially of homopolymers and copolymers of polyolefins, polystyrenes, polyvinyls, polyacrylics, polyhalo-olefins, polydienes, polyoxides/esthers/acetals, polysulfides, polyesters/thioesters, polyamides/thioamides, polyurethanes/thiourethanes, polyureas/thioureas, polyimides/thioimides, polyanhydrides/thianhydrides, polycarbonates/thiocarbonates, polyimines, polysiloxanes/silanes, polyphosphazenes, polyketones/thioketones, polysulfones/sulfoxides/sulfonates/sulfoamides, polyphylenes, and mixtures thereof.

### Claim 4 (depends on 1)

The electrode material of claim 1, wherein the polymeric binder comprises poly(vinylidene fluoride-co-hexafluoropropylene).

### Claim 5 (depends on 1)

The electrode material of claim 1, wherein the ionic liquid comprises oppositely charged ions, wherein the ionic liquid has a melting point of no more than about 100 degrees Celsius, a decomposition temperature of at least about 200 degrees Celsius, a viscosity of no more than about 200 Cp, an ionic conductivity of at least about 0.1 mS/cm, and an electrochemical window of at least about 2 Volts and -wherein the ionic liquid comprises:
(A) at least one cation selected from the group consisting essentially of the following compounds and mixtures thereof:
wherein R1, R2, R3, R4, R5, and R6 of the cationic components are identical or different and are selected from the group consisting essentially of:
(i) a hydrogen;
(ii) a halogen;
(iii) a hydroxyl;
(iv) an amine;
(v) a thiol;
(vi) a C1 to C25 straight-chain or branched aliphatic hydrocarbon radical;
(vii) a C5 to C30 cycloaliphatic hydrocarbon radical;
(viii) a C6 to C30 aromatic hydrocarbon radical;
(ix) a C7 to C40 alkylaryl radical;
(x) a C2 to C25 linear or branched aliphatic hydrocarbon radical having interruption by one or more heteroatoms, such as, oxygen, nitrogen or sulfur;
(xi) a C2 to C25 linear or branched aliphatic hydrocarbon radical having interruption by one or more functionalities selected from the group consisting essentially of:
(a′) a carbonyl;
(b′) an ester;
(c′) an amide, where R′ is selected from the group consisting essentially of hydrogen, C1-C12 straight-chain, or branched or cyclic alkane or alkene;
(d′) a sulfonate;
(e′) a sulfonamide, where R′ is selected from the group consisting essentially of hydrogen, C1-C12 straight-chain, or branched or cyclic alkane or alkene;
(xii) a C2 to C25 linear or branched aliphatic hydrocarbon radical terminally functionalized by Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH;
(xiii) a C5 to C30 cycloaliphatic hydrocarbon radical having at least one heteroatom selected from the group consisting essentially of O, N, S, and optionally substituted with at least one of the following Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH;
(xiv) a C7 to C40 alkylaryl radical having at least one heteroatom selected from the group consisting essentially of O, N, S, and optionally substituted with at least one of the following:
(a″) a C2 to C25 straight-chain or branched hydrocarbon radical substituted with at least one of the following Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH;
(b″) a C5 to C30 cycloaliphatic hydrocarbon radical substituted with at least one of the following Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH
(c″) a hydroxyl;
(d″) an amine;
(e″) a thiol;
(xv) a polyether of the type —O—(—R7—O—)n—R8 or block or random type —O—(—R7—O—)n—(—R7—O—)m—R8, wherein at least one of the following is true:
(a′″) R7 is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms;
(b′″) R7′ is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms; and
(c′″) wherein n is from 1 to 40; and
(d′″) R8 is hydrogen, or a C5 to C30 straight-chain or branched hydrocarbon radical, or a C5 to C30 cycloaliphatic hydrocarbon radical, or a C6 to C30 aromatic hydrocarbon radical, or a C7 to C40 alkylaryl radical; and
(xvi) a polyether of the type —O—(—R7—O—)n—C(O)—R8 or block or random type —O—(—R7—O—)m—(—R7′—O—)m—C(O)—R8, wherein at least one of the following is true:
(a″″) R7 is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms;
(b″″) R7′ is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms; and
(c″″) wherein n is from 1 to 40; and
(d″″) R8 is hydrogen, or a C5 to C30 straight-chain or branched hydrocarbon radical, or a C5 to C30 cycloaliphatic hydrocarbon radical, or a C6 to C30 aromatic hydrocarbon radical, or a C7 to C40 alkylaryl radical; and
(B) at least one anion selected from the group consisting essentially of F−; Cl−, Br−; I−; NO3−; N(CN)2−; BF4−; ClO4−; PF6−; RSO3−; RCOO−; where R is an alkyl group, substituted alkyl group, or phenyl group; (CF3)2PF4−; (CF3)3PF3−; (CF3)4PF2−; (CF3)5PF−; (CF3)6P−; (CF2SO3−)2; (CF2CF2SO3−)2; (CF3SO2−)2N−; CF3CF2(CF3)2CO−; (CF3SO2−)2CH−; (SF5)3C−; (CF3SO2)3C−; [O(CF3)2C2(CF3)2O]2PO−; (CF3(CF2)7SO3−; and mixtures thereof.

### Claim 6 (depends on 5)

The electrode material of claim 5, wherein the ionic liquid is one of:
1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide ([EMIM][Tf2N]);
1-ethyl-3-methlimidazolium tetrifluoroborate ([EMIM][BE]); and
mixtures thereof.

### Claim 7 (depends on 1)

The electrode material of claim 1, wherein the activated carbon particles have a specific surface area of at least about 500 m2/g.

### Claim 8 (depends on 1)

The electrode material of claim 1, wherein the electrode material is positioned on a current collector, wherein the current collector and electrode material are in physical contact, wherein the electrode material has a mass ratio of the ionic liquid to the polymeric binder from about 0.01:1 to about 1:0.01, wherein the electrode material comprises: from about 0.5 wt % to about 95 wt % of the activated carbon particles; from about 0.5 wt % to about 95 wt % of the carbon nanotubes; from about 0.5 wt % to about 40 wt % of the polymeric binder; and optionally carbon particles, and wherein the electrode material further comprises from about 0 wt % to about 30.0 wt % carbon black.

### Claim 9 (depends on 8)

The electrode material of claim 8, wherein the mass ratio of the ionic liquid to the polymeric binder is from about 0.1:1 to about 1:0.1, wherein the electrode material comprises: from about 60 to about 65 wt % of the activated carbon particles; from about 10 to about 25 wt % of the carbon nanotubes; from about 7 to about 20 wt % of the polymeric binder; and optionally from about 0 wt % to about 12 wt % carbon black and wherein the electrode material has one or both of a surface resistance from about 2 to about 12 ohms/cm and a specific surface area of from about 500 to about 2,000 m2/g.

### Claim 10

An electrode material for an electrochemical energy storage device, comprising:
an ionic liquid having a plurality of activated carbon particles substantially intermixed and dispersed within an entangled carbon nanotubes network, wherein at least most of carbon nanotubes comprising the entangled carbon nanotube network are in contact with at least two or more activated carbon particles and wherein the ionic liquid substantially binds together the activated carbon particles and the carbon nanotubes.

### Claim 11 (depends on 10)

The electrode material of claim 10, wherein the entangled carbon nanotubes network further comprise one of single walled carbon nanotubes, multi-walled carbon nanotubes, and mixtures thereof and wherein the carbon nanotubes have a length ranging from about 10 to about 1,000 μm and wherein the carbon nanotubes have an electrical conductivity of at most about 200 S/cm.

### Claim 12 (depends on 10)

The electrode material of claim 10, further comprising a polymeric binder selected from the group consisting essentially of homopolymers and copolymers of polyolefins, polystyrenes, polyvinyls, polyacrylics, polyhalo-olefins, polydienes, polyoxides/esthers/acetals, polysulfides, polyesters/thioesters, polyamides/thioamides, polyurethanes/thiourethanes, polyureas/thioureas, polyimides/thioimides, polyanhydrides/thianhydrides, polycarbonates/thiocarbonates, polyimines, polysiloxanes/silanes, polyphosphazenes, polyketones/thioketones, polysulfones/sulfoxides/sulfonates/sulfoamides, polyphylenes, and mixtures thereof.

### Claim 13 (depends on 10)

The electrode material of claim 10, wherein the ionic liquid comprises oppositely charged ions, wherein the ionic liquid has a melting point of no more than about 100 degrees Celsius, a decomposition temperature of at least about 200 degrees Celsius, a viscosity of no more than about 200 Cp, an ionic conductivity of at least about 0.1 mS/cm, and an electrochemical window of at least about 2 Volts and wherein the ionic liquid comprises:
(A) at least one cation selected from the group consisting essentially of the following compounds and mixtures thereof:
wherein R1, R2, R3, R4, R5, and R6 of the cationic components are identical or different and are selected from the group consisting essentially of:
(i) a hydrogen;
(ii) a halogen;
(iii) a hydroxyl;
(iv) an amine;
(v) a thiol;
(vi) a C1 to C25 straight-chain, or branched aliphatic hydrocarbon radical;
(vii) a C5 to C30 cycloaliphatic hydrocarbon radical;
(viii) a C6 to C30 aromatic hydrocarbon radical;
(ix) a C7 to C40 alkylaryl radical;
(x) a C2 to C25 linear or branched aliphatic hydrocarbon radical having interruption by one or more heteroatoms, such as, oxygen, nitrogen or sulfur;
(xi) a C2 to C25 linear or branched aliphatic hydrocarbon radical having interruption by one or more functionalities selected from the group consisting essentially of:
(a′) a carbonyl;
(b′) an ester;
(c′) an amide, where R′ is selected from the group consisting essentially of hydrogen, C1-C12 straight-chain, or branched or cyclic alkane or alkene;
(d′) a sulfonate;
(e′) a sulfonamide, where R′ is selected from the group consisting essentially of hydrogen, C1-C12 straight-chain, or branched or cyclic alkane or alkene;
(xii) a C2 to C25 linear or branched aliphatic hydrocarbon radical terminally functionalized by Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH;
(xiii) a C5 to C30 cycloaliphatic hydrocarbon radical having at least one heteroatom selected from the group consisting essentially of O, N, S, and optionally substituted with at least one of the following Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH;
(xiv) a C7 to C40 alkylaryl radical heteroatom selected from the group consisting essentially of O, N, S, and optionally substituted with at least one of the following:
(a″) a C2 to C25 straight-chain, or branched hydrocarbon radical substituted with at least one of the following Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH;
(b″) a C5 to C30 cycloaliphatic hydrocarbon radical substituted with at least one of the following Cl, Br, F, I, NH, OH, NH2, NHCH3 or SH
(c″) a hydroxyl;
(d″) an amine;
(e″) a thiol;
(xv) a polyether of the type —O—(—R7—O—)n—R8 or block or random type —O—(—R7—O—)n—(—R7—O—)m—R8, wherein at least one of the following is true:
(a′″) R7 is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms;
(b′″) R7′ is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms; and
(c′″) wherein n is from 1 to 40; and
(d′″) R8 is hydrogen, or a C5 to C30 straight-chain or branched hydrocarbon radical, or a C5 to C30 cycloaliphatic hydrocarbon radical, or a C6 to C30 aromatic hydrocarbon radical, or a C7 to C40 alkylaryl radical; and
(xvi) a polyether of the type —O—(—R7—O—)n—C(O)—R8 or block or random type —O—(—R7—O—)n—(—R7′—O—)m—C(O)—R8, wherein at least one of the following is true:
(a″″) R7 is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms;
(b″″) R7′ is a linear or branched hydrocarbon radical having from 2 to 4 carbon atoms; and
(c″″) wherein n is from 1 to 40; and
(d″″) R8 is hydrogen, or a C5 to C30 straight-chain or branched hydrocarbon radical, or a C5 to C30 cycloaliphatic hydrocarbon radical, or a C6 to C30 aromatic hydrocarbon radical, or a C7 to C40 alkylaryl radical; and
(B) at least one anion selected from the group consisting essentially of F—; Cl—, Br—; I—; NO3—; N(CN)2—; BF4—; ClO4—; PF6—; RSO3—; RCOO—; where R is an alkyl group, substituted alkyl group, or phenyl group; (CF3)2 PF4—; (CF3)3 PF3—; (CF3)4 PF2—; (CF3)5 PF—; (CF3)6P—; (CF2SO3—)2; (CF2CF2SO3—)2; (CF3SO2—)2N—; CF3CF2(CF3)2CO—; (CF3SO2—)2CH—; (SF5)3C—; (CF3SO2)3C—; [O(CF3)2C2(CF3)2O]2PO—; (CF3(CF2)7 SO3—; and mixtures thereof.

### Claim 14 (depends on 12)

The electrode material of claim 12, wherein the electrode material is in positioned on and is physical contact with a current collector and wherein the electrode material comprises: from about 0.5 wt % to about 95 wt % of the activated carbon particles; from about 0.5 wt % to about 95 wt % of the entangled carbon nanotube network; from about 0.5 wt % to about 40 wt % of the polymeric binder, from and optionally a plurality of carbon black particles, wherein the electrode material further comprises from about 0 to about 30 wt % carbon black, wherein the electrode material has a mass ratio of the ionic liquid to the polymeric binder form about 0.01:1 to about 1:0.01.

### Claim 15

An electrode material for an electrochemical energy storage device, comprising:
a plurality of activated carbon particles substantially intermixed and dispersed within an with an entangled carbon nanotubes network, wherein the at least most of the carbon nanotubes comprising the entangled carbon nanotube network are in contact with at least two or more active carbon particles and wherein the electrode material has one or both of a surface resistance from about 2 to about 12 ohms/cm and a specific surface area of from about 500 to about 2,000 m2/g.

### Claim 16 (depends on 15)

The electrode material of claim 15, wherein the entangled carbon nanotube network further comprise one of single walled carbon nanotubes, multi-walled carbon nanotubes, and mixtures thereof and wherein the carbon nanotubes comprising the entangled carbon nanotube network have a length ranging from about 10 to about 1,000 μm and wherein the carbon nanotubes have an electrical conductivity of at most about 200 S/cm.

### Claim 17 (depends on 15)

The electrode material of claim 15, wherein the activated carbon particles have a specific surface area of at least about 500 m2/g and wherein the electrode material is substantially free of any added carbon black.

### Claim 18 (depends on 15)

The electrode material of claim 15, wherein the electrode material is positioned on a current collector, wherein the current collector and electrode material are in physical contact and wherein the electrode material comprises: from about 0.5 wt % to about 95 wt % activated carbon and from about 0.5 wt % to about 95 wt % of the entangled cabon nanotube network; and further comprising from about 0 wt % to about 30.0 wt % carbon black and from about 0.5 wt % to about 40 wt % polymer binder.