# US 8,277,686 B2 · Sialon phosphor particles and production method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,686 B2
- Document ID: US8277686B2
- Status: Granted
- Kind: B2
- Application number: 11/793,965
- Filed: 2005-12-22
- Published: 2008-12-18
- Granted: 2012-10-02
- Earliest claimed: 2004-12-27
- Assignees: Ube Industries, Ltd.
- Inventors: Shin-ichi Sakata; Takeshi Yamao; Tetsuo Yamada
- Web page: https://patentgrep.com/patent/US8277686B2

## CPC

- C09K 11/0883: {Arsenides; Nitrides; Phosphides}
- C04B 35/597: based on silicon oxynitride, {e.g. SIALONS}
- C04B 35/6262: {of calcined, sintered clinker or ceramics}
- C09K 11/77348: {Silicon Aluminium Nitrides or Silicon Aluminium Oxynitrides}
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3865: Aluminium nitrides
- C04B 2235/3873: Silicon nitrides, e.g. silicon carbonitride, silicon oxynitride
- C04B 2235/442: Carbonates
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/549: the particle size being expressed by crystallite size or primary particle size
- H10H 20/8512: {Wavelength conversion materials}
- H10W 74/00: Encapsulations, e.g. protective coatings
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

To provide sialon phosphor particles or a powder exhibiting high emission intensity in the region from ultraviolet to blue and not requiring a strong pulverization operation for pulverizing a sintered body or a large aggregated lump, and a production method thereof. Sialon phosphor particles represented by the formula: MxLnySi12−(m+n)Al(m+n)OnN16−n (wherein M is at least one metal selected from the group consisting of Li, Ca, Mg and Y, Ln is a lanthanide metal containing at least Eu, and assuming that the valence of the metal M is a and the valence of the lanthanide metal Ln is b, ax+by=m, x is 0<x, y≦2.0, 0.3≦m<4.5 and 0.5≦n<2.5), wherein in the surface analysis by X-ray photoelectron spectroscopy, the ratio between the peak area of 3d5/2 spectrum of europium and the peak area of 2p spectrum of Si is 0.5 or less.

## Claims

### Claim 1

Sialon phosphor particles represented by the formula:
MxLnySi12−(m+n)Al(m+n)OnN16−n
(wherein M is at least one metal selected from the group consisting of Li, Ca, Mg and Y, Ln is a lanthanide metal containing at least Eu, and assuming that the valence of the metal M is a and the valence of the lanthanide metal Ln is b, m=ax+by, x is 0<x, y≦2.0, 0.3≦m<4.5, 1.0≦n<2.5 and 1.0≦m/n≦2.0), wherein, in a surface analysis by X-ray photoelectron spectroscopy, a ratio between a peak area of 3d5/2 spectrum of Eu and a peak area of 2p spectrum of Si, obtained by acid-treating said sialon phosphor particles in which said ratio exceeds 0.5, is 0.5 or less.

### Claim 2 (depends on 1)

A sialon phosphor powder comprising the sialon phosphor particles claimed in claim 1, wherein said phosphor particles are aggregate particles and average particle diameter obtained by a laser diffraction/scattering particle size distribution measuring method is from 5 to 100 microns.

### Claim 3 (depends on 1)

The sialon phosphor particles as claimed in claim 1, wherein 1.25≦n<2.5.

### Claim 4 (depends on 2)

The sialon phosphor particles as claimed in claim 2, wherein 1.25≦n<2.5.

### Claim 5 (depends on 1)

The sialon phosphor particles as claimed in claim 1, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si, obtained by acid-treating the sialon phosphor particles in which said ratio is from 2.32 to 2.68, is 0.5 or less.

### Claim 6 (depends on 2)

The sialon phosphor particles as claimed in claim 2, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si, obtained by acid-treating the sialon phosphor particles in which said ratio is from 2.32 to 2.68, is 0.5 or less.

### Claim 7 (depends on 3)

The sialon phosphor particles as claimed in claim 3, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si, obtained by acid-treating the sialon phosphor particles in which said ratio is from 2.32 to 2.68, is 0.5 or less.

### Claim 8 (depends on 4)

The sialon phosphor particles as claimed in claim 4, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si, obtained by acid-treating the sialon phosphor particles in which said ratio is from 2.32 to 2.68, is 0.5 or less.

### Claim 9 (depends on 1)

The sialon phosphor particles as claimed in claim 1, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si is 0.4 or less.

### Claim 10 (depends on 2)

The sialon phosphor particles as claimed in claim 2, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si is 0.4 or less.

### Claim 11 (depends on 3)

The sialon phosphor particles as claimed in claim 3, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si is 0.4 or less.

### Claim 12 (depends on 4)

The sialon phosphor particles as claimed in claim 4, wherein the ratio between the peak area of 3d5/2 spectrum of Eu and the peak area of 2p spectrum of Si is 0.4 or less.

### Claim 13 (depends on 1)

A method for producing the sialon phosphor particles claimed in claim 1, comprising:
mixing (a) silicon nitride, (b) a substance which becomes an aluminum source and contains AlN, (c) an oxide of the metal M (wherein M is at least one metal selected from the group consisting of Li, Ca, Mg and Y) or a precursor substance which becomes an oxide upon thermal decomposition, and (d) an oxide of lanthanide metal Ln containing at least Eu, or a precursor substance which becomes an oxide upon thermal decomposition,
firing resulting mixed particles at 1,400 to 2,000° C. in a nitrogen-containing inert gas atmosphere, and
acid-treating obtained sialon particles with an acid solution selected from sulfuric acid, hydrochloric acid and nitric acid and having a concentration of 0.1 to 7 normal, thereby removing the glass layer on the surface.

### Claim 14 (depends on 13)

The method as claimed in claim 13, wherein concentration of the acid solution is from 1 to 3 normal.

### Claim 15 (depends on 13)

The method as claimed in claim 13, wherein the mixed powder is fired at 1,400 to 1,800° C. in a nitrogen gas atmosphere under 1 atm.

### Claim 16 (depends on 14)

The method as claimed in claim 14, wherein the mixed powder is fired at 1,400 to 1,800° C. in a nitrogen gas atmosphere under 1 atm.

### Claim 17 (depends on 1)

A light-emitting device comprising:
a blue light-emitting element capable of emitting blue light having a peak at a wavelength of 430 to 475 nm, and
a phosphor layer containing the sialon phosphor particles claimed in claim 1 and capable of absorbing a part of the blue light and converting it into yellow light having a wavelength of 520 to 600 nm,
wherein white light can be emitted by the mixing of the blue light and the yellow light.

### Claim 18 (depends on 2)

A light-emitting device comprising:
a blue light-emitting element capable of emitting blue light having a peak at a wavelength of 430 to 475 nm, and
a phosphor layer containing the sialon phosphor particles claimed in claim 2 and capable of absorbing a part of the blue light and converting it into yellow light having a wavelength of 520 to 600 nm,
wherein white light can be emitted by the mixing of the blue light and the yellow light.

### Claim 19 (depends on 3)

A light-emitting device comprising:
a blue light-emitting element capable of emitting blue light having a peak at a wavelength of 430 to 475 nm, and
a phosphor layer containing the sialon phosphor particles claimed in claim 3 and capable of absorbing a part of the blue light and converting it into yellow light having a wavelength of 520 to 600 nm,
wherein white light can be emitted by the mixing of the blue light and the yellow light.

### Claim 20 (depends on 1)

A light-emitting device comprising:
a violet light-emitting element capable of emitting violet light having a peak at a wavelength of 390 to 430 nm, and
a phosphor layer containing the sialon phosphor particles claimed in claim 1 and capable of absorbing a part of said violet light and converting it into yellow light having a wavelength of 520 to 600 nm,
wherein white light can be emitted by mixing said violet light and said yellow light.