# US 8,277,679 B2 · Composite magnetic material and magnetic element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,679 B2
- Document ID: US8277679B2
- Status: Granted
- Kind: B2
- Application number: 13/024,675
- Filed: 2011-02-10
- Published: 2011-07-14
- Granted: 2012-10-02
- Earliest claimed: 2009-04-02
- Assignees: Sumida Corporation
- Inventors: Akihiko Nakamura; Keisuke Watanabe
- Web page: https://patentgrep.com/patent/US8277679B2

## CPC

- H01F 1/14766: {Fe-Si based alloys}
- B22F 1/062: Fibrous particles
- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- C22C 9/00: Alloys based on copper
- C22C 33/0257: {characterised by the range of the alloying elements}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/38: with more than 1.5% by weight of manganese
- H01F 1/26: by macromolecular organic substances
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The object of the present invention is to provide a composite magnetic material having well-balanced magnetic properties and chemical properties, and a magnetic element using thereof. Concretely, the present provides the composite magnetic material comprising a binder and a magnetic powder contains followings: Mn not less than 0.25 wt % and not larger than 3 wt %, Si not less than 1 wt % and not larger than 7 wt %, Cr not less than 2 wt % and not larger than 8 wt %, and the rest of Fe and inevitable impurities with respect to the total weight of a magnetic powder material, and a ratio of powder particles having the major/minor axis is not less than 2 is not larger than 5% of the total powder particles.

## Claims

### Claim 1

A composite magnetic material comprising:
a magnetic powder comprising Mn not less than 1.1 wt % and not larger than 3 wt %, Si not less than 4 wt % and not larger than 7 wt %, Cr not less than 4 wt % and not larger than 8 wt %, Fe and inevitable impurities as balance with respect to the total weight of a magnetic powder material; and a binder;
wherein the fraction of the total powder particles of the magnetic powder having a major/minor axis ratio of equal to or greater than 2 is equal to or less than 1%.

### Claim 2 (depends on 1)

The composite magnetic material according to claim 1, wherein the insulation resistivity is equal to or greater than 150 MΩcm.

### Claim 3 (depends on 1)

The composite magnetic material according to claim 1, wherein the dielectric breakdown electric field is equal to or greater than 1.6 kV/cm.

### Claim 4 (depends on 1)

The composite magnetic material according to claim 1, wherein the core loss at a magnetic flux density of 50 mT and an effective frequency of 500 kHz is equal to or less than 5 w/cm3.

### Claim 5 (depends on 1)

The composite magnetic material according to claim 1, wherein the content of the binder is in the range of 2.5 to 4.5 wt % of the composite magnetic material.

### Claim 6 (depends on 1, 2, 3, 4, 5)

A magnetic element formed of the composite magnetic material according to any one of claims 1 to 5.

### Claim 7 (depends on 6)

The magnetic element according to claim 6, wherein an area of corrosion in the magnetic element having been maintained in the atmosphere of a temperature of 105° C. and a humidity of 100% for 8 hours is equal to or less than 5% of the surface area of the magnetic material.