# US 8,277,678 B2 · Polymer-bonded magnetic materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,678 B2
- Document ID: US8277678B2
- Status: Granted
- Kind: B2
- Application number: 12/039,592
- Filed: 2008-02-28
- Published: 2009-09-03
- Granted: 2012-10-02
- Earliest claimed: 2008-02-28
- Assignees: The Hong Kong Polytechnic University
- Inventors: Ka Wai Eric Cheng; Yuen Wah Wong; Wei Tai Wu; Kai Ding; Yiu Lun Ho; Tsz Kong Cheung; Chi Keong Cheong
- Web page: https://patentgrep.com/patent/US8277678B2

## CPC

- H01F 1/344: {Ferrites, e.g. having a cubic spinel structure (X2+O)(Y23+O3), e.g. magnetite Fe3O4}
- H01F 1/37: in a bonding agent
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A magnetic composition for power conversion includes a thermoplastic polymer and magnetic powders. The composition has a tensile strength of greater than 20 N/mm2.

## Claims

### Claim 1

A method of making a magnetic composition for power conversion, comprising:
a step of preparing magnetic powders from Fe2O3, NiO and ZnO;
a step of mixing dried PMMA pellets with Stearic acid (C18H36O2) in a high-speed blender to form polymer powders with appropriate size; and
a step of mixing said magnetic powders and said polymer powders in a high-speed blender to afford a magnetic composition for power conversion.

### Claim 2 (depends on 1)

The method of claim 1, wherein said step of preparing magnetic powders comprises
mixing Fe2O3, NiO and ZnO into a mixture in a high-speed blender;
sintering said mixture in a high-temperature calcination furnace;
cooling said mixture to room temperature prior to crushing said mixture; and
crushing said mixture in a high-speed blender into magnetic powders.

### Claim 3 (depends on 2)

The method of claim 2, wherein said furnace is heated at a rate of 8° C./min to 1300° C. and maintained at this temperature for 950 minutes.

### Claim 4 (depends on 1)

The method of claim 1, further comprising drying said PMMA pellets in an oven at about 60° C. for about 6 hours prior to mixing with said magnetic powders.

### Claim 5 (depends on 1)

The method of claim 1, further comprising drying said magnetic powders in an oven at about 60° C. for about 4 hours after crushing said mixture.

### Claim 6 (depends on 5)

The method of claim 5, further comprising mixing said dried magnetic powders with Titanium (IV) Isopropoxide (C12H28O4Ti) in a high-speed blender.

### Claim 7 (depends on 6)

The method of claim 6, wherein the mass ratio of C12H28O4Ti to said dried magnetic powders is about 15 weight percent.

### Claim 8 (depends on 6)

The method of claim 6, wherein the mass ratio of C18H36O2 to said dried PMMA is about 2 weight percent.

### Claim 9 (depends on 1)

A method for increasing magnetic permeability of a magnetic composition made according to the method of claim 1, comprising applying an external field to aid the alignment of a material dipole to increase magnetic permeability.

### Claim 10 (depends on 9)

The method of claim 9, wherein said external field is applied in the same direction of a flux direction in a magnetic core.