# US 8,277,677 B2 · Mechanical strength and thermoelectric performance in metal chalcogenide MQ (M=Ge,Sn,Pb and Q=S, Se, Te) based compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 8,277,677 B2
- Document ID: US8277677B2
- Status: Granted
- Kind: B2
- Application number: 12/487,893
- Filed: 2009-06-19
- Published: 2010-02-04
- Granted: 2012-10-02
- Earliest claimed: 2008-06-23
- Assignees: Northwestern University
- Inventors: Mercouri G. Kanatzidis; Joseph R. Sootsman
- Web page: https://patentgrep.com/patent/US8277677B2

## CPC

- C01G 17/00: Compounds of germanium
- C01B 19/007: {Tellurides or selenides of metals (C01B19/002 takes precedence)}
- H10N 10/852: comprising tellurium, selenium or sulfur
- C01P 2002/52: containing elements as dopants
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/03: obtained by SEM
- C01P 2006/32: Thermal properties
- C01P 2006/40: Electric properties
- Y02P 20/129: Energy recovery, e.g. by cogeneration, H2recovery or pressure recovery turbines
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Thermoelectric eutectic and off-eutectic compositions comprising a minor phase in a thermoelectric matrix phase are provided. These compositions include eutectic and near eutectic compositions where the matrix phase is a chalcogenide (S, Se, Te) of Ge, Sn, or Pb or an appropriate alloy of these compounds and at least one of Ge, Ge1−xSix, Si, ZnTe, and Co are precipitated as the minor phase within the matrix. Methods of making and using the compositions are also provided. The thermoelectric and mechanical properties of the compositions make them well-suited for use in thermoelectric applications. Controlled doping of eutectic compositions and hypereutectic compositions can yield large power factors. By optimizing both the thermal conductivities and power factors of the present compositions, ZT values greater than 1 can be obtained at 700K.

## Claims

### Claim 1

A composition comprising:
(a) a matrix comprising a compound having the formula MQ, wherein M is Ge, Sn, Pb or a combination thereof and Q is S, Se, Te or a combination thereof;
(b) a minor phase comprising an alloy of Ge and Si ZnTe, Co or a combination thereof; and
(c) a dopant;
wherein the minor phase is dispersed in the matrix.

### Claim 2 (depends on 1)

The composition of claim 1 having a ZT of at least 1 at 700 K.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the composition comprises a eutectic mixture of the matrix and the minor phase.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the matrix comprises PbTe and the minor phase comprises an alloy of Ge and Si.

### Claim 5 (depends on 4)

The composition of claim 4, wherein the alloy of Ge and Si is present in an amount of about 2 to about 30 mol. %, based on the total amount of the matrix and minor phase.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the minor phase comprises Ge(1−x)Six and x has a value in the range from 0.15 to 0.25.

### Claim 7 (depends on 6)

The composition of claim 6 having a ZT at least 1 at 700 K.

### Claim 8 (depends on 1)

The composition of claim 1 having a Vickers hardness of at least 0.4 GPa.

### Claim 9 (depends on 1)

The composition of claim 1, wherein the minor phase comprises an alloy of Ge and Si.

### Claim 10 (depends on 1)

The composition of claim 1, wherein the minor phase comprises ZnTe.

### Claim 11 (depends on 1)

The composition of claim 1, wherein the minor phase comprises Co.

### Claim 12

A composition comprising:
(a) a matrix comprising a compound having the formula MQ, wherein M is Ge, Sn, Pb or a combination thereof and Q is S, Se, Te or a combination thereof;
(b) a minor phase comprising Ge(1−x)Six, ZnTe, Co or a combination thereof; and
(c) a dopant;
wherein the minor phase is dispersed in the matrix and x has a value from 0 to 1, and further
wherein the composition comprises a hypereutectic mixture of the matrix and the minor phase.

### Claim 13

A composition comprising:
(a) a matrix comprising a compound having the formula MQ, wherein M is Ge, Sn, Pb or a combination thereof and Q is S, Se, Te or a combination thereof;
(b) a minor phase comprising Ge(1−x)Six, ZnTe, Co or a combination thereof; and
(c) a dopant;
wherein the minor phase is dispersed in the matrix and x has a value from 0 to 1, and further wherein the dopant is PbI2.

### Claim 14 (depends on 13)

The composition of claim 13, wherein x =0, the composition comprising a eutectic mixture of the PbTe and the Ge and having a ZT of at least 0.6 at 675 K.

### Claim 15 (depends on 13)

The composition of claim 13, wherein x =1, the composition comprising a hypereutectic mixture of the PbTe and the Si and having a ZT of at least 0.8 as 675 K.

### Claim 16

A composition comprising:
(a) a matrix comprising a compound having the formula MQ, wherein M is Ge, Sn, Pb or a combination thereof and Q is S, Se, Te or a combination thereof; and
(b) a minor phase comprising Ge(i-x)Six;
wherein the Ge(1−x)Six is dispersed in the matrix and x has a value in the range from 0.05 to 0.95.

### Claim 17 (depends on 16)

The composition of claim 16, wherein the matrix comprises PbTe and the Ge(1−x)Six is present in an amount of about 2 to about 30 mol. %, based on the total amount of the matrix and minor phase.

### Claim 18 (depends on 16)

The composition of claim 16 having a Vickers hardness of at least 0.4 GPa.

### Claim 19

A method of making a composition, the method comprising combining a compound having the formula MQ, wherein M is Ge, Sn, Pb or a combination thereof and Q is S, Se, Te or a combination thereof, with Ge(1−x)Six, ZnTe, Co or a combination thereof, and a dopant under vacuum and heating the combination at a temperature and for a time sufficient to form a composition comprising a minor phase of Ge(1−x)Six, ZnTe, Co or a combination thereof dispersed in a matrix of the compound having the formula MQ, wherein x has a value from 0 to 1.

### Claim 20 (depends on 19)

The method of claim 19, wherein the composition comprises a eutectic mixture of the matrix and the minor phase.

### Claim 21 (depends on 19)

The method of claim 19, wherein the composition comprises a hypereutectic mixture of the matrix and the minor phase.

### Claim 22 (depends on 19)

The method of claim 19, wherein the matrix comprises PbTe, the minor phase comprises Ge(1−x)Six, and the Ge(1−x)Six is present in an amount of about 2 to about 30 mol. %, based on the total amount of the matrix and minor phase.

### Claim 23

A method for power generation comprising placing a composition in thermal contact with a heat source whereby the composition generates electricity and powering an electrical device with the electricity, the composition comprising:
(a) a matrix comprising a compound having the formula MQ, wherein M is Ge, Sn, Pb or a combination thereof and Q is S, Se, Te or a combination thereof;
(b) a minor phase comprising Ge(1−x)Six, ZnTe, Co or a combination thereof; and
(c) a dopant;
wherein the minor phase is dispersed in the matrix and x has a value from 0 to 1.